Lebedeva Yu.E., Shchegoleva N.E., Voronov V.A., Solntsev St.S. Al2O3 and ZrO2 ceramic materials obtained by sol-gel method // Proceedings of VIAM. 2021. No. 4 (98). Ст. 05. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2021-0-4-61-73.
Al2O3 and ZrO2 ceramic materials obtained by sol-gel method
Abstract
The rheological properties, processes of structure and phase formation of the Al2O3–ZrO2 system compositions obtained by the sol-gel method have been investigated. The temperature range of crystallization of the compositions is 900–1100 °C. With an increase in the concentration of zirconium dioxide in the system, the temperature of the transition from the tetragonal to the monoclinic phase decreases. The effect of the ratio of the components in the initial solutions and the temperature regime of heat treatment of gels on the physicochemical properties of nanopowders and sintered materials has been studied. Ceramic materials of eutectic composition give the highest density and lower values of porosity and water absorption.
Keywords
aluminum oxide, zirconium oxide, ceramic materials, nano powders, sintering, sol-gel method.
Reference list
- Kablov E.N. New generation materials - the basis of innovation, technological leadership and national security of Russia. Intellekt i tekhnologii, 2016, no. 2 (14), pp. 16–21.
- Balkevich V.L. Technical ceramics. Moscow: Stroyizdat, 1984, 256 p.
- Kablov E.N. Trends and guidelines for innovative development in Russia: collection of articles. inform. mater. 3rd ed., Rev. and add. M .: VIAM, 2015.720 p.
- Evdokimov S.A., Shchegoleva N.E., Sorokin O.Yu. Ceramic materials aviation engineering (review). Trudy VIAM, 2018, no. 12 (72), paper no. 06. Available at: http://www.viam-works.ru (accessed: October 05, 2020). DOI: 10.18577/2307-6046-2018-0-12-54-61.
- Grashchenkov D.V. Strategy of development of non-metallic materials, metal composite materials and heat-shielding. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 264–271. DOI: 10.18577/2071-9140-2017-0-S-264-271.
- Buchilin N.V., Lyulyukina G.Yu. Characteristics of sintering of highly porous alumina-based ceramic materials. Aviacionnye materialy i tehnologii, 2016, no. 4 (45), pp. 40–46. DOI: 10.18577/2071-9140-2016-0-4-40-46.
- Kablov E.N., Grashchenkov D.V., Shchegoleva N.E. et al. Radiotransparent glass ceramics based on strontium aluminosilicate glass. Ogneupory i tekhnicheskaya keramika, 2016, no. 6, pp. 31–38.
- Lebedeva Yu.E., Popovich N.V., Orlova L.A., Chaynikova A.S., Grachshencov D.V. Investigation of rheological properties at sol-gel synthesis of materials in Y2O3–SiO2 system. Aviacionnye materialy i tehnologii, 2014, no. S6, pp. 67–72. DOI: 10.18577/2071-9140-2014-0-s6-67-72.
- Chainikova A.S., Kovaleva V.S., Zabelin D.A., Belyachenkov I.O. Processes of gel-, phase formation and sintering during the preparation of a sol-gel by the method of aluminosilicate glass ceramics modified with refractory oxides of hafnium and zirconium. Steklo i keramika, 2019, no. 6. pp. 5–12.
- Simonenko N.P., Simonenko E.P., Sevastyanov V.G., Kuznetsov N.T. Production of 8% Y2O3 – 92% ZrO2 (8YSZ) Thin Films by Sol-Gel Technology. Russian Journal of Inorganic Chemistry, 2015, vol. 60, no. 7. pp. 795–803.
- Simonenko N.P., Simonenko E.P., Sevastyanov V.G., Kuznetsov N.T. Preparation of Nanostructured Thin Films of Yttrium Iron Garnet (Y3Fe5O12) by Sol-Gel Technology. Russian Journal of Inorganic Chemistry, 2016, vol. 61, no. 7, pp. 805–810.
- Simonenko N.P., Nikolaev V.A., Simonenko E.P. et al. Influence of the Composition of [Ti(OC4H9)4 – x(O2C5H7)x] Complexes and Hydrolysis Conditions on the Synthesis of Titania by Sol-Gel Technology. Russian Journal of Inorganic Chemistry, 2016, vol. 61, no. 8, pp. 929–939.
- Simonenko E.P., Simonenko N.P., Kopitsa G.P. et al. How Xerogel Carbonization Conditions Affect the Reactivity of Highly Disperse SiO2–C Composites in the Sol-Gel Synthesis of Nanocrystalline Silicon Carbide. Russian Journal of Inorganic Chemistry, 2016, vol. 61, no. 11, pp. 1347–1360.
- Simonenko E.P., Derbenev A.V., Simonenko N.P. et al. Gel Formation during Sol-Gel Synthesis of Silicon Dioxide. Russian Journal of Inorganic Chemistry. 2015, vol. 60, no. 12, pp. 1444–1451.
- Simonenko N.P., Nikolaev V.A., Simonenko E.P. et al. Preparation of Nanostructured Titania Thin Films by Sol-Gel Technology. Russian Journal of Inorganic Chemistry, 2016, vol. 61, no. 12. P. 1505-1511.
- Simonenko E.P., Simonenko N.P., Sevastianov V.G., Grashchenkov D.V., Kuznetsov N.T., Kablov E.N. Functionally gradient composite material SiC / (ZrO2–HfO2–Y2O3) obtained using the sol-gel method. Kompozity i nanostruktury, 2011, no. 4, pp. 52–64.
- Makarov N.A. Composite material in the aluminum oxide – zirconium dioxide system. Steklo i keramika, 2007, no. 4, pp. 12–15.
- Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
- Guzeev V.V., Khorobraya E.G. Thermal method of obtaining microfibers of zirconium dioxide. Steklo i keramika, 2002, no. 10. P. 18–21.
- Karakchiev L.G., Lyakhov N.Z. Heat treatment of zirconium dioxide gel. Neorganicheskie materialy, 1998, vol. 34, no. 5, pp. 575–579.
- Konstantinova T.E., Danilenko I.A., Tokiy V.V., Glazunova V.A. Obtaining zirconium dioxide nanopowders. From innovation to innovation. Nauka i innovatsii, 2005, vol. 1, no. 3, pp. 76–87.
- McHale J. M., Auroux A., Perrotta A. J., Navrotsky A. Suface Energies and Thermodynamic Phase Stability in Nanocrystalline Aluminas. Journal Sceince, 1997, vol. 277, no. 5327, pp. 788–791.
- Kikkawa S., Kijima A., Hirota K., Yamaguchi O. Soft solution preparation methods in a ZrO2–Al2O3 binary system. Journal of Solid State Ionics, 2002, vol. 151, pp. 359–364.
- Klimova T., Rojas M., Castillo P. et al. Characterization of Al2O3–ZrO2 mixed oxide catalytic supports prepared by the sol-gel method. Journal Microporous and Mesoporous Materials, 1998, vol. 20, is. 4-6, pp. 293–306.
- Belyakov A.V., Pershikov S.A., Sukhozhak A.N. Chemisorption and catalytic reduction in the sintering temperature of ceramics. Glass and ceramics. 1996, no. 6, pp. 16–18.