Laptev A.B., Pavlov M.R., Novikov A.A., Slavin A.V. Current trends in the development of testing materials for resistance to climatic factors (review). Part 2. Main trends // Proceedings of VIAM. 2021. No. 2 (96). Ст. 11. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2021-0-2-99-108.

Current trends in the development of testing materials for resistance to climatic factors (review)

Part 2. Main trends
Laptev A.B., Pavlov M.R., Novikov A.A., Slavin A.V.
Abstract

In the second part of the review, based on the analysis of the world experience in conducting climate tests, the main development trends related to new applications of materials, their compatibility, modeling of loading cycles, acceleration of climate tests, the impact of climate gradients, taking into account the level of climate factors in a particular area with a minimum resolution, climate change, new methods for assessing the climatic resistance of materials and biolo-gical impact factors are identified. The relevance of complex tests of materials for climatic and biological resistance with the use of methods for predicting their properties is shown.

Keywords
climate tests, polymer composite materials, aviation materials, determination of service life, accelerated climate tests, gradient of climatic factors.
Reference list
  1. Chatterjee B., Bhowmik S. Evolution of material selection in commercial aviation industry – a review. Sustainable Engineering Products and Manufacturing Technologies, 2019, pp. 199–219. DOI: 10.1016/B978-0-12-816564-5.00009-8.
  2. Kablov E.N., Startsev O.V., Medvedev I.M. Corrosion of the marine atmosphere. Part 2. New approaches to assessing the corrosiveness of coastal atmospheres. Korroziya: materialy, zashchita, 2016, no. 1, pp. 1-15.
  3. Petrunin M.A., Maksaeva L.B., Yurasova T.A. et al. The effect of self-organizing vinyl siloxane nanolayers on the corrosion behavior of aluminum in neutral chloride-containing solution. Protection of Metals and Physical Chemistry of Surfaces, 2014, vol. 50, no. 6, pp. 784–791.
  4. Erofeev V.T., Salnikova A.I., Kablov E.N., Startsev O.V., Varchenko E.A. Investigation of the durability of bituminous composites in conditions of variable humidity, ultraviolet radiation and sea water. Fundamentalnye issledovaniya, 2014, no. 12, pp. 2549–2556.
  5. Sehra A.K., Whitlow W.W. Propulsion and power for 21st century aviation. Progress in Aerospace Sciences, 2004, vol. 40, is. 4–5, pp. 199–235. DOI: 10.1016/j.paerosci.2004.06.003.
  6. Singha D., Ravi K., Amritap M. et al. Mechanical Characterization of C–Ph Composites Treated with Aviation Grade Fluids. Procedia Structural Integrity, 2020, vol. 25, pp. 159–171. DOI: 10.1016/j.prostr.2020.04.019.
  7. Mirzaa J., Duranda B., Bhuttab A.R., Tahirb M.M. Preferred test methods to select suitable surface repair materials in severe climates. Construction and Building Materials, 2014, vol. 50, pp. 692–698. DOI: 10.1016/j.conbuildmat.2013.10.006.
  8. Jenkins M.G., Lara-Curzio E., Gonczy S.T. Mechanical, Thermal and Environmental Testing and Performance of Ceramic Composites and Components. Philadelphia, 2000, 53 р.
  9. Sitziaab F., Lisciab C., Mirãoab J. Accelerate ageing on building stone materials by simulating daily, seasonal thermo-hygrometric conditions and solar radiation of CSA Mediterranean climate. Construction and Building Materials, part A, 2021, vol. 266. DOI: 10.1016/j.conbuildmat.2020.121009.
  10. Laptev A.B., Barbotko S.L., Nikolaev E.V., Skirta A.A. Statistical processing of the results of climatic tests of fiberglass. Plasticheskiye massy, 2016, no. 3–4, pp. 58–64.
  11. Chena S., Youa Z., Sharifia N.P., Yaoba H., Gongac F. Material selections in asphalt pavement for wet-freeze climate zones: a review. Construction and Building Materials, 2019, vol. 201, pp. 510–525. DOI: 10.1016/j.conbuildmat.2018.11.276.
  12. Sharifia N.P., Chena S., Youa Z., Damb T.V., Gilbertsona C. A review on the best practices in concrete pavement design and materials in wet-freeze climates similar to Michigan. Journal of Traffic and Transportation Engineering (English Edition), 2019, vol. 6, is. 3, pp. 245–255. DOI: 10.1016/j.jtte.2018.12.003.
  13. Laptev A.B., Nikolayev E.V., Kolpachkov E.D. Thermodynamic characteristics of aging of polymeric composite materials under conditions of real exploitation. Aviaсionnye materialy i tehnologii, 2018, no. 3, pp. 80–88. DOI: 10.18577/2071-9140-2018-0-3-80-88.
  14. Lutsenko A.N., Course M.G., Laptev A.B. Justification of the timing of full-scale climatic tests of metallic materials in the atmosphere of the Black Sea coast. Analytical review. Voprosy materialovedeniya, 2016, no. 3 (87), pp. 126–137.
  15. Koopmans S., Heusinkveld B.G., Steeneveld G.J. A standardized Physical Equivalent Temperature urban heat map at 1-m spatial resolution to facilitate climate stress tests in the Netherlands. Construction and Building Materials, 2020, vol. 213, pp. 115–132. DOI: 10.1016/j.buildenv.2020.106984.
  16. Averina A.E., Laptev A.B., Nesterov A.S., Sarvaeva G.A., Nikolaev E.V. Application of quantum-chemical calculations to evaluate the aging processes of polyethylene terephthalate under the influence of climate. Aviaсionnye materialy i tehnologii, 2020, no. 3 (60), pp. 47–56. DOI: 10.18577/2071-9140-2020-0-3-47-56.
  17. Verbista K.M.J., Maureira-Cortésb H., Rojasb P., Vicuñac S. A stress test for climate change impacts on water security: A CRIDA case study. Climate Risk Management, 2020, vol. 10, art. 100222. DOI: 10.1016/j.crm.2020.100222.
  18. Nikolaev E.V., Pavlov M.R., Laptev A.B., Ponomarenko S.A. To the problem of determining the moisture sorbed in polymeric composite materials. Trudy VIAM, 2017, no. 8 (56), paper no. 07. Available at: http://www.viam-works.ru (accessed: November 19, 2020). DOI: 10.18577/2307-6046-2017-0-8-7-7.
  19. Laptev A.B., Bugay D.E., Alexandrov A.A., Larionov V.I. Environmental and biological factors affecting complex technical systems. Bezopasnost v tekhnosfere, 2017, vol. 6, no. 4, pp. 21–30.
  20. Wolkoff P., Nielsen A. A new approach for indoor climate labeling of building materials – emission testing, modeling, and comfort evaluation. Atmospheric Environment, 1996, vol. 30, is. 15, pp. 2679–2689. DOI: 10.1016/1352-2310(95)00323-1.
  21. ASTM D2176-16. Standard Test Method for Folding Endurance of Paper and Plastics Film by the M.I.T. Tester: Active Standard (Latest Version). Last Updated November 1, 2016. Available at: https://www.astm.org/Standards/D2176.htm (accessed: November 19, 2020).
  22. ASTM D5870-16. Standard Practice for Calculating Property Retention Index of Plastics: Active Standard (Latest Version). Last Updated April 1, 2016. Available at: https://www.astm.org/Standards/D5870.htm (accessed: November 19, 2020).
  23. ASTM D3012-19. Standard Test Method for Thermal-Oxidative Stability of Polypropylene Using a Specimen Rotator Within an Oven: Active Standard (Latest Version). Last Updated May 9, 2019. Available at: https://www.astm.org/Standards/D3012.htm (accessed: November 19, 2020).
  24. Tourova T., Sokolova D., Nazina T., Grouzdev D., Kurshev E., Laptev A. Biodiversity of microorganisms colonizing the surface of polystyrene simples exposed to different aqueous environments. Sustainability, 2020, vol. 12, no. 9, art. 3624. DOI: 10.3390/su12093624.
  25. Laptev A.B., Nikolaev E.V., Kurshev E.V., Goryashnik Yu.S. Features of biodegradation of thermoplastics based on polyesters in different climatic zones. Trudy VIAM, 2019, no. 7 (79), paper no. 10. Available at: http://www.viam-works.ru (accessed: November 19, 2020). DOI: 10.18577/2307-6046-2019-0-7-84-91.
  26. Kogan A.M., Nikolayev E.V., Golubev A.V., Laptev A.B., Movenko D.A. Stages of biofouling and corrosion of steel in the Black sea water. Trudy VIAM, 2019, no. 6 (78), paper no. 09. Available at: http://viam-works.ru (accessed: November 19, 2020). DOI: 10.18577/2307-6046-2019-0-6-84-94.
  27. ASTM D6954-18. Standard Guide for Exposing and Testing Plastics that Degrade in the Environment by a Combination of Oxidation and Biodegradation: Active Standard (Latest Version). Last Updated March 13, 2018. Available at: https://www.astm.org/Standards/D6954.htm (accessed: November 19, 2020).
  28. ASTM D6400-19. Standard Specification for Labeling of Plastics Designed to be Aerobically Composted in Municipal or Industrial Facilities: Active Standard (Latest Version). Last Updated June 4, 2019. Available at: https://www.astm.org/Standards/D6400.htm (accessed: November 19, 2020).
  29. ASTM D7991-15. Standard Test Method for Determining Aerobic Biodegradation of Plastics Buried in Sandy Marine Sediment under Controlled Laboratory Conditions: Active Standard (Latest Version). Last Updated September 1, 2015. Available at: https://www.astm.org/Standards/D7991.htm (accessed: November 19, 2020).
  30. STP533. Disposal of Plastics with Minimum Environmental Impact. Available at: https://www.astm.org/DIGITAL_LIBRARY/STP/SOURCE_PAGES/STP533_foreword.pdf (accessed: November 19, 2020).
  31. ASTM F2759-19. Standard Guide for Assessment of the Ultra-High Molecular Weight Polyethylene (UHMWPE) Used in Orthopedic and Spinal Devices: Active Standard (Latest Version). Last Updated February 6, 2020. Available at: https://www.astm.org/Standards/F2759.htm (accessed: November 19, 2020).
  32. ASTM D5338-15. Standard Test Method for Determining Aerobic Biodegradation of Plastic Materials Under Controlled Composting Conditions, Incorporating Thermophilic Temperatures: Active Standard (Latest Version). Last Updated June 1, 2015. Available at: https://www.astm.org/Standards/D5338.htm (accessed: November 19, 2020).
  33. ASTM E2317-04. Standard Guide for Conducting Renewal Microplate-Based Life-Cycle Toxicity Tests with a Marine Meiobenthic Copepod: Active Standard (Latest Version). Last Updated December 1, 2012. Available at: https://www.astm.org/Standards/E2317.htm (accessed: November 19, 2020).
  34. ASTM E1562-00. Standard Guide for Conducting Acute, Chronic, and Life-Cycle Aquatic Toxicity Tests with Polychaetous Annelids: Active Standard (Latest Version). Last Updated March 1, 2013. Available at: https://www.astm.org/Standards/E1562.htm (accessed: November 19, 2020).
  35. ASTM D7475-20. Standard Test Method for Determining the Aerobic Degradation and Anaerobic Biodegradation of Plastic Materials under Accelerated Bioreactor Landfill Conditions: Active Standard (Latest Version). Last Updated March 6, 2020. Available at: https://www.astm.org/Standards/D7475.htm (accessed: November 19, 2020).