Gorlov D.S., Zaklyakova O.V., Aleksandrov D.A., Budinovskiy S.A. Improving of fretting resistance intermetallic Ti2AlNb alloy // Proceedings of VIAM. 2021. No. 2 (96). Ст. 07. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2021-0-2-62-70.

Improving of fretting resistance intermetallic Ti2AlNb alloy

Gorlov D.S., Zaklyakova O.V., Aleksandrov D.A., Budinovskiy S.A.
Abstract

The results of research on improving the fretting resistance of a titanium alloy made of orthorhombic titanium aluminide Ti2AlNb by forming a coating consisting of a barrier and an outer layer on the surface using an industrial vacuum-arc installation MAP-3 are presented. The dependences of the total wear and the coefficient of friction of samples made of Ti2AlNb alloy with and without coating in combination with a counterbody made of high-strength welded dispersed-hardening alloy during fretting damage tests at room (20 °C) and elevated (700 °C) temperatures are established. The kinetics of oxygen saturation of the surface of samples made of Ti2AlNb alloy with and without coating at the operating temperature of the alloy based on 200 h is shown. The phase and elemental compositions of the fretting-resistant coating after high-temperature exposure are investigated.

Keywords
orthorhombic titanium aluminide Ti2AlNb, dispersion-hardening alloy, ion-plasma coating, fretting resistance, fretting damage, heat resistance, phase composition, element composition.
Reference list
  1. Smyslov A.M., Selivanov K.S. Development and research of technological methods for increasing the fretting resistance of rotor blades made of titanium alloys. Vestnik UGATU, ser.: Mashinostroyenie, 2007, vol. 9, no. 1 (19), pp. 77–83.
  2. Lesnevsky L.N. Fretting corrosion of coatings of the «solid lubricant» type in extreme operating conditions. Vestnik nauchno-tekhnicheskogo razvitiya, 2009, no. 2 (18), pp. 31–35.
  3. Selivanov K.S., Galiakbarov R.F. Increasing the fretting resistance of machine parts by complex vacuum plasma treatment. Aviatsionno-kosmicheskaya tekhnika i tekhnologiya, 2011, no. 7 (84), pp. 29–32.
  4. Gorlov D.S., Skripak V.I., Muboyadzhyan S.A., Egorova L.P. The research of fretting-wear slip and ion-plasma coatings. Trudy VIAM, 2017, no. 3, paper no. 07. Available at: http://www.viam-works.ru (accessed: November 26, 2020). DOI: 10.18577/2307-6046-2017-0-3-7-7.
  5. Kablov E.N., Ospennikova O.G., Bazyleva O.A. Materials for highly heat-loaded parts of gas turbine engines. Vestnik MGTU im. N.E. Baumana, ser.: Mashinostroyenie, 2011, no. SP2, pp. 13-19.
  6. Kablov E.N. Cast blades of gas turbine engines: alloys, technologies, coatings. 2nd ed. Moscow: Nauka, 2006, 632 p.
  7. Putyrskij S.V., Arislanov A.A., Artemenko N.I., Yakovlev A.L. Different methods of wear resistance increase of titanium alloys and comparative analysis of their efficiency for VT23M titanium alloy. Aviacionnye materialy i tehnologii, 2018, no. 1, pp. 19–24. DOI: 10.18577/2071-9240-2018-0-1-19-24.
  8. Sibileva S.V., Kozlova L.S. Review of technologies of applying coatings to titanium alloys by plasma electrolytic oxidation. Aviacionnye materialy i tehnologii, 2016, no. S2, pp. 3–10. DOI: 10.18577/2071-9140-2016-0-S2-3-10.
  9. Kablov E.N., Muboyadzhyan S.A., Budinovskiy S.A., Pomelov Ya.A. Ion-plasma protective coatings for blades of gas turbine engines. Konversiya v mashinostroyenii, 1999, no. 2, pp. 42–47.
  10. Muboyadzhyan S.A., Budinovskij S.A. Ion-plasma technology: prospective processes, coatings, equipment. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 39–54. DOI: 10.18577/2071-9140-2017-0-S-39-54.
  11. Kablov E.N., Nochovnaya N.A., Panin P.V., Alekseev E.B., Novak A.V. Investigation of the structure and properties of heat-resistant alloys based on titanium aluminides with microadditions of gadolinium. Materialovedenie, 2017, no. 3, pp. 3–10.
  12. Antipov V.V. Prospects for development of aluminium, magnesium and titanium alloys for aerospace engineering. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 186–194. DOI: 10.18577/2107-9140-2017-0-S-186-194.
  13. Novak A.V., Alekseev E.B., Ivanov V.I., Dzunovich D.A. The study of the quenching parameters influence on structure and hardness of orthorhombic titanium aluminide alloy VТI-4. Trudy VIAM, 2018, no. 2, paper no. 05. Available at: http://www.viam-works.ru (accessed: November 26, 2020). DOI: 10.18577/2307-6046-2018-0-2-5-5.
  14. Kurzina I.A., Popova N.A., Nikonenko E.L., Kalashnikov M.P., Savkin K.P., Sharkeev Yu.P., Kozlov E.V. Formation of nanosized intermetallic phases under conditions of implantation of titanium targets by aluminum ions. Izvestiya RAN, ser.: Fizicheskaya, 2012, vol. 76, no. 1, pp. 74–78.
  15. Alexandrov D.A., Muboyadzhyan S.A., Gayamov A.M., Gorlov D.S. Studies of heat resistance and kinetics of elemental composition of VT41 titanium alloy with heat-resistant coatings. Aviacionnye materialy i tehnologii, 2014, no. S5, pp. 61–66. DOI: 10.18577/2071-9140-2014-0-s5-61-66.
  16. Gorlov D.S., Aleksandrov D.A., Zaklyakova O.V., Azarovskiy E.N. Investigation of the possibility of protection of intermetallic titanium alloy against fretting wear by ion-plasma coating. Trudy VIAM, 2018, no. 4 (64), paper no. 06. Available at: http://www.viam-works.ru (accessed: November 26, 2020). DOI: 10.18577/2307-6046-2018-0-4-51-58.
  17. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.