UDC
620.193.8
DOI
10.18577/2307-6046-2021-0-12-107-116
Article PDF (Russian)
(787.81 KB)
How to cite
Krivushina A.A., Terekhov I.V., Moskvitina K.N., Malysheva S.F., Kuimov V.A. Efficiency of new fungicide compounds based on modified polysept for protection of polymer materials against biodeterioration // Proceedings of VIAM. 2021. No. 12 (106). Ст. 12. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2021-0-12-107-116.
Efficiency of new fungicide compounds based on modified polysept for protection of polymer materials against biodeterioration
Abstract
In order to protect polymer materials in particular polyurethanes and similar materials from biodeterioration by microscopic fungi, seven fungicidal compounds of the guanidine series were synthesized and their effectiveness was investigated in various concentrations. Among the tested compounds, the most effective is the first fraction of polyhexamethylene guanidine n-octylphosphonate (code B1), which completely suppresses the growth of all studied micromycetes at a minimum concentration of 0.01 % by weight. At a lower concentration of 0.001 % by weight, compound the first fraction of polyhexamethylene guanidine n-octylphosphonate inhibits the growth of most of the studied micromycetes, with the exception of the Aspergillus niger culture.
Reference list
- Lugauskas A.Yu., Levinskayte L.I., Luksaite D.I. The defeat of polymer materials by micromycetes. Plasticheskiye massy, 1991, no. 2, pp. 24–28.
- Kablov E.N., Erofeev V.T., Dergunova A.V., Deraeva E.V., Svetlov D.A. Influence of environmental factors on the processes of biodegradation of vinylester composites. Journal of Physics: Conference Series. International Conferece on Engineering Systems, 2020, vol. 1687, art. 012029. DOI: 10.1088/1742-6596/1687/1/012029.
- Kablov E.N., Startsev V.O. Climatic aging of aviation polymer composite materials. II. Development of methods for studying the early stages of aging. Russian metallurgy (Metally), 2020, vol. 2020, no. 10, pp. 1088–1094. DOI: 10.1134/S0036029520100110.
- Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
- Polyakova A.V., Krivushina A.A., Goryashnik Yu.S., Buharev G.MMicrobiological resistance tests under nature conditions in variety of climatiс zones. Trudy VIAM, 2016, no. 4, paper no. 11. Available at: http://www.viam-works.ru (accessed: August 18, 2021). DOI: 10.18577/2307-6046-2016-0-4-11-11.
- Chertishchev V.Yu., Ospennikova O.G., Boi-chuk A.S., Dikov I.A., Generalov A.S. Determination of the size and depth of defects in multilayer PCM honeycomb structures based on the mechanical impedance value. Aviaсionnye materialy i tehnologii, 2020, no. 3 (60), pp. 72–94. DOI: 10.18577/2071-9140-2020-0-3-72-94.
- Sakhno ON, Selivanov OG, Chukhlanov V.Yu. Biological stability of polymeric materials. Ed. T.A. Trifonova. Vladimir: Vladimir. state un-t them. A.G. and N.G. Stoletovs, 2014, 64 p.
- Klempner D., Sendidzharevich V. Polymer foams and foaming technology. Ed. A.M. Chebotarya. Saint Petersburg: Professiya, 2009, 600 p.
- Pekhtasheva E.L., Neverov A.N., Zaikov G.E., Stoyanov O.V., Rusanova S.N. Biodamage and protection of synthetic polymeric materials. Vestnik Kazanskogo tekhnologicheskogo universiteta, 2012., vol. 15, no. 10, pp. 166–173.
- Kraev I.D., Pykhtin A.A., Lonskii S.L., Kurshev E.V., Terekhov I.V. Effect of biocidal additives on technological parameters in the manufacture of polyurethane foams. Inorganic materials: Applied Research, 2021, vol. 12 (1), pp. 125–132.
- Krivushina A.A., Goryashnik Yu.S. Ways of protection of materials and products from microbiological damage (review). Aviacionnye materialy i tehnologii, 2017, no. 2 (47), pp. 80–86. DOI: 10.18577/2071-9140-2017-0-2-80-86.
- Vointseva I.I., Gembitsky P.A. Polyguanidines are disinfectants and multifunctional additives in composite materials. Moscow: LKSM-press, 2009, 303 p.
- Ozerov M.Yu., Karkishchenko V.N., Popov D.V. et al. Means for disinfection of objects contaminated with B. anthracis spores. Biomedicine, 2009, no. 1, pp. 28–37.
- Kablov E.N., Startsev V.O. Systematical analysis of the climatics influence on mechanical properties of the polymer composite materials based on domestic and foreign sources (review). Aviacionnye materialy i tehnologii, 2018, no. 2 (51), pp. 47–58.
- Rai M., Yadav A., Gade A. Silver nanoparticles as a new generation of antimicrobials. Biotechnology Advances. 2009, vol. 27, pp. 76–83.
- Dallas P., Sharma V.K., Zboril R. Silver polymeric nanocomposites as advanced antimicrobial agents: Classification, synthetic paths, applications, and perspectives. Advances in Colloid and Interface Science, 2011, vol. 166, pp. 119–135.
- Duran N., Duran M., de Jesus M.B. et al. Silver nanoparticles: A new view on mechanistic aspects on antimicrobial activity. Nanomedicine: Nanotechnology, Biology, and Medicine, 2016, vol. 12, pp. 789–799.
- Picca R.A., Paladini F., Sportelli M.C. et al. Combined Approach for the Development of E ffi cient and Safe Nanoantimicrobials: The Case of Nanosilver-Modi fi ed Polyurethane Foams. ACS Biomaterials Science and Engineering, 2017, vol. 3 (7), pp. 1417–1425.
- Yakovenko T.V., Bukharev G.M., Bobyreva T.V. et al. Experience in the selection of biocidal additives for modifications of polyurethane foams. Climate-2019: Modern approaches to assessing the impact of external factors on materials and complex technical systems. Gelendzhik, 2019, pp. 201–211.
- Kuimov V.A., Malysheva S.F., Belogorlova N.A. et al. Synthesis of Long-Chain n-Alkylphosphonic Acids by Phosphonylation of Alkyl Bromides with Red Phosphorus and Superbase under Micellar/Phase Transfer Catalysis. European Journal of Organic Chemistry, 2021, vol. 2021 (10), pp. 1596–1602. DOI: 10.1002/ejoc.202100067.
- Arslanova M.M., Yampolskaya T.D. Microorganisms as biodestructors of various materials. Vestnik SurGU, 2015, is. 3 (9), s. 14–22.
- Arashkova A.A., Goncharova I.A., Mitskevich A.G., Kostenevich A.A., Sharich T.V. Fungi of the genus Aspergillus in foci of mold infection in residential and public premises. Vestsi Natsyanalnay Akademii Navuk Belarusi, 2016, no. 3, pp. 13–16.
- Kurakov A.V., Gevorkyan S.A., Goginyan V.B., Ozerskaya S.M. Diversity and compositional features of microscopic fungi on synthetic polymeric materials. Prikladnaya biokhimiya i mikrobiologiya, 2008, vol. 44, no. 2, pp. 232–235.
- Sakhno O.N., Selivanov O.G., Chukhlanov V.Yu. Biostability of polymeric materials and methods of its assessment: textbook. Vladimir: Publishing house of Vladimir University, 2018, 83 p.