Prokhorchuk E.A., Leonov A.A., Vlasova K.A., Trapeznikov A.V., Nikitin V.I., Nikitin K.V. Prospects for the use of hot isostatic pressing in cast aluminum alloys (review) // Proceedings of VIAM. 2021. No. 12 (106). Ст. 03. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2021-0-12-21-30.

Prospects for the use of hot isostatic pressing in cast aluminum alloys (review)

Prokhorchuk E.A., Leonov A.A., Vlasova K.A., Trapeznikov A.V., Nikitin V.I., Nikitin K.V.
Abstract

Provides an overview of methods for producing porous aluminum, its properties, advantages and disadvantages, and considers the use of aluminum foamed materials in the aerospace and mechanical engineering industries. It has been established that the mechanical properties of foam aluminum depend on the size and location of the pores, as well as on the method of its production; carrying out the process of modeling the deformation of samples with different pore diameters and the type of porous structure will make it possible to control the mechanical properties of a porous aluminum alloy.

Keywords
porous structure, foam aluminum, energy-absorbing material, porosity, thermal conductivity.
Reference list
  1. Kablov E.N. VIAM: materials of new generation for PD-14. Krylya Rodiny, 2019, no. 7-8, pp. 54–58.
  2. Kablov E.N., Antipov V.V., Girsh R.I, Serebrennikova N.Yu., Konovalov A.N. Designed layered materials on the basis of sheets from aluminum lithium alloys and fibreglasses in designs of flight vehicles of new generation. Vestnik mashinostroeniya, 2020, no. 12, pp. 46–52.
  3. Antipov V.V. Prospects for development of aluminium, magnesium and titanium alloys for aerospace engineering. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 186–194. DOI: 10.18577/2107-9140-2017-0-S-186-194.
  4. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  5. Antipov V.V., Klochkova Yu.Yu., Romanenko V.A. Modern aluminum and aluminum-lithium alloys. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 195–211. DOI: 10.18577/2107-9140-2017-0-S-195-211.
  6. Way of receiving frothed metal: pat. 2016113 Rus. Federation; filed 20.05.92; publ. 15.07.94.
  7. Sugimura Y., Meyer J., He Y. et al. On the mechanical performance of closed cell A1 alloys foams. Acta Materialia, 1997, vol. 45, pp. 5245–5259.
  8. Way of production of porous semi-finished products from powder aluminum alloys: pat. 2121904 Rus. Federation; filed 17.07.01; publ. 20.11.98.
  9. Калиниченко B.A., Калиниченко A.С. Способы получения вспененного алюминия, области его применения и ряд особенностей механической обработки // Литье и металлургия. 2005. № 2-1 (34). С. 164–169.
  10. Hassanli F., Paydar M.H. Improvement in energy absorption properties of aluminum foams by designing pore-density distribution. Journal of Materials Research and Technology, 2021, vol. 14, pp. 609–619.
  11. Hangai Y., Saito K., Utsunomiya T., Kuwazuru O. Fabrication and compression properties of functionally graded foam with uniform pore structures consisting of dissimilar A1050 and A6061 aluminum alloys. Materials Science and Engineering: A, 2014, vol. 613, pp. 163–170.
  12. Brothers A.H., Dunand D.C. Density-graded cellular aluminum. Advanced Engineering Materials, 2006, vol. 8 (9), pp. 805–809.
  13. Mirzaei M., Paydar M.H. Fabrication and characterization of coreeshell density-graded 316L stainless steel porous structure. Journal of Materials Engineering and Performance, 2019, no. 28 (1), pp. 221–230.
  14. Hе S.Y., Lv Y.N., Chen S.T. et al. Gradient regulation and compressive properties of density-graded aluminum foam. Materials Science and Engineering: A, 2020, vol. 772, pp. 501–511.
  15. Mahbod M., Asgari M. Elastic and plastic characterization of a new developed additively manufactured functionally graded porous lattice structure: analytical and numerical models. International Journal of Mechanical Sciences, 2019, vol. 155, pp. 248–266.
  16. Gupta N. A functionally graded syntactic foam material for high energy absorption under compression. Materials Letters, 2007, vol. 61, pp. 979–982.
  17. Singh G., Pandey P.M. Uniform and graded copper open cell ordered foams fabricated by rapid manufacturing: surface morphology, mechanical properties and energy absorption capacity. Materials Science and Engineering: A, 2019, vol. 761, pp. 192–205.
  18. Jeon I., Katou K., Sonoda T. et al. Cell wall mechanical properties of closed-cell Al foam. Mechanics of Materials, 2009, vol. 41, pp. 60–73.
  19. Leushin I.O., Grachev A.N., Nazarov V.N., Gorokhov P.A. Foamed aluminum – perspective material for production of cast products of responsible assignment. Teoriya i tekhnologiya metallurgicheskogo proizvodstva, 2020, no. 4 (35), pp. 35–38.
  20. Butarovich D.O., Smirnov A.A., Ryabov D.M. Foamed aluminum as power absorbing material and its mechanical properties. Mashinostroenie, 2011, no 7, pp. 53–58.
  21. Kraev I.D., Sorokin A.E., Nyrtsov A.V., Shipin N.O., Krayeva A.A., Titkova Yu.M. Foams designed to ensure the absorption of acoustic waves over a wide range of frequencies. Trudy VIAM, 2018, no. 1 (61), paper no. 10. Available at: http://www.viam-works.ru (accessed: August 09, 2021). DOI: 10.18577/2307-6046-2018-0-1-10-10.
  22. Zhelezina G.F., Kolobkov A.S., Kulagina G.S., Kan A.Ch. Damping properties of hybrid layered metal-polymer materials based on aluminum, titanium alloys and organoplastics layers. Trudy VIAM, 2021, no. 2 (96), paper no. 02. Available at: http://www.viam-works.ru (accessed: August 8, 2021). DOI: 10.18577/2307-6046-2021-0-2-10-19.
  23. Stoyakina E.A., Kurbatkina E.I., Simonov V.N., Kosolapov D.V., Gololobov A.V. Mechanical properties of aluminium-matrix composite materials reinforсed with SiC particles, depending on the matrix alloy (review). Trudy VIAM, 2018, no. 2, paper no. 08. Available at: http://www.viam-works.ru (accessed: August 8, 2021). DOI: 10.18577 / 2307-6046-2018-0-2-8-8.
  24. Weber A. Light weighting Is Top Priority for Automotive Industry. Available at: https://www.assemblymag.com/articles/94341-lightweighting-is-top-priorityfor-automotive-industry (accessed: August 16, 2021).
  25. Claar T.D., Vu C.J., Hall L. et al. Ultra-lightweight Aluminum Foam Materials for Automotive Applications. SAE Technical Papers, 2000, vol. 36 (6), pp. 11–18.
  26. Banhart J. Manufacturing Routes for Metallic Foams. Journal of the Minerals, Metals, 2000, vol. 52 (12), pp. 22–27.
  27. Fuganti A., Lorenzi L., Hanssen A.G., Langseth M. Aluminium foam for automotive applications. Advanced Engineering Materials, 2000, vol. 2 (4), pp. 200–204.
  28. Mohammed R.H., Mesalhy O., Elsayed M.L. et al. Performance of desiccant heat exchangers with aluminum foam coated or packed with silica gel. Available at: https://www.sciencedirect.com/science/article/abs/pii/S1359431119339286 (accessed: August 16, 2021).