Oglodkov M.S., Duyunova V.A., Nochovnaya N.A., Ivanov V.I., Avilochev L.Yu. Features of the technology manufacturing of deformed blanks from intermetallic alloys VIT1 for parts of the gas turbine engine // Proceedings of VIAM. 2021. No. 12 (106). Ст. 01. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2021-0-12-3-13.

Features of the technology manufacturing of deformed blanks from intermetallic alloys VIT1 for parts of the gas turbine engine

Oglodkov M.S., Duyunova V.A., Nochovnaya N.A., Ivanov V.I., Avilochev L.Yu.
Abstract

Intermetallic alloy based on a Ti2AlNb compound are the most promising high-temperature materials for gas turbine engines operating up to a temperature of 700 degrees Celsius. In this paper, the technology of hot pressure treatment of a cast billet on a plate with a thickness of 25 mcm is studied. The technology included three comprehensive forging of the ingot billet, forging by drawing the intermediate billet and its subsequent rolling to the final size. The influence of heat treatment on the macro and microstructure of plates is studied. The chosen scheme of hot deformation and the mode of heat treatment provides an increased level of mechanical properties in the plates.

Keywords
intermetallic alloy, pressure treatment, heat treatment, structure, mechanical properties.
Reference list
  1. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  2. Kablov E.N. VIAM: New generation materials for PD-14. Krylya Rodiny, 2019, no. 7-8, pp. 54–58.
  3. Kablov E.N., Bondarenko Yu.A., Kolodyazhny M.Yu., Surova V.A., Narsky A.R. Prospects for the creation of high-temperature heat-resistant alloys based on refractory matrices and natural composites. Voprosy materialovedeniya, 2020, no. 4 (104), pp. 64–78.
  4. Antipov V.V. Prospects for development of aluminium, magnesium and titanium alloys for aerospace engineering. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 186–194. DOI: 10.18577/2107-9140-2017-0-S-186-194.
  5. Nochovnaya N.A., Ivanov V.I. Prospects for the use of heat-resistant materials based on titanium aluminides. Int. conf. "Ti-2006 in the CIS". Verkhnyaya Salda, 2006, pp. 39–43.
  6. Night H.A., Bazyleva O.A., Kablov D.E., Panin P.V. Intermetallic alloys based on titanium and nickel. Ed. E.N. Kablov. Moscow: VIAM, 2018, 318 p.
  7. Leyens C., Hausmann J., Kumfert J. Continuous Fiber Reinforced Titanium Matrix Composites Fabrication, Properties and Applcation. Titanium and Titanium Alloys. Fundamental and Application. Ed. C. Leyens, M. Peters. Weinheim: Wiley-VCH Verlag GnbH & Co. KGaA 2003, pp. 305–331.
  8. Dey S. R., Roy S., Suwas S. et al. Annealing response of the intermetallic alloy T – 22Al – 25Nb. Journal of Intermetallics, 2010, vol. 18, no. 6, pp. 1122–1131.
  9. Ma X., Zeng W., Xu B. et al. Characterization of the hot deformation behavior of a Ti – 22Al – 25Nb alloy using processing maps based on the Murry criterion. Journal of Intermetallics, 2012, vol. 20, no. 1, pp. 1–7.
  10. Nochovnaya N., Alexeev E., Izotova A., Ivanov V. Oportunities of increase of mechanical properties of the deformed semifinished products from Ti – Al – Nb system alloys. Proceeding of the 12th Wold Conference on "Ti-2011". Beijing: Science Press, 2011, vol. 2, pp. 1383–1386.
  11. Wang W., Zeng W., Chen X. et al. Microstructural control and mechanical properties from isothermal forging and heat treatment of Ti – 22Al – 25Nb (at.%) Orthorhombic alloy. Journal of Intermetallics, 2015, vol. 56, pp. 79–86.
  12. Shang J.L., Guo H.-Z., Liang H.-Q. Hot deformation behavior and process parameter optimization of Ti – 22Al – 25 Nb using processing map. Journal Rare Metals, 2016, vol. 35, no. 1, pp. 118–126.
  13. Alekseev Е.B., Nochovnaya N.A., Novak A.V., Panin P.V. Wrought intermetallic titanium ortho alloy doped with yttrium Part 1. Research on ingot microstructure and rheological curves plotting. Trudy VIAM, 2018, no. 6 (66), paper no. 02. Available at: http://www.viam-works.ru (accessed: January 14, 2021). DOI: 10.18577/2307-6046-2018-0-6-12-21.
  14. Alexeev Е.B., Nochovnaya N.A., Novak A.V., Panin P.V. Wrought intermetallic titanium ortho alloy doped with yttrium. Part 2. Research on heat treatment effect on rolled slab microstructure and mechanical properties. Trudy VIAM, 2018, no. 12 (72), paper no. 04. Available at: http://www.viam-works.ru (accessed: January 14, 2021). DOI: 10.18577/2307-6046-2018-0-12-37-45.
  15. Novak A.V., Alekseev E.B., Ivanov V.I., Dzunovich D.A. The study of the quenching parameters influence on structure and hardness of orthorhombic titanium aluminide alloy VТI-4. Trudy VIAM, 2018, no. 2, paper no. 05. Available at: http://www.viam-works.ru (accessed: August 09, 2021). DOI: 10.18577/2307-6046-2018-0-2-5-5.