Dvoretskov R.M., Slavin A.V., Karachevtsev F.N., Zagvozdkina T.N. Comparisons of the nickel alloys VZH172 and VZHL21 reference materials kits using the AES ICP method // Proceedings of VIAM. 2021. No. 11 (105). Ст. 12. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2021-0-11-120-132.

Comparisons of the nickel alloys VZH172 and VZHL21 reference materials kits using the AES ICP method

Dvoretskov R.M., Slavin A.V., Karachevtsev F.N., Zagvozdkina T.N.
Abstract

The procedure for comparing the kits of reference materials of nickel alloys VZh172 and VZhL21 is considered. Using the method of atomic emission spectrometry with inductively coupled plasma for analytical lines of elements Al, Co, Cr, Mo, Ti, W, Zr, Fe, Mn, calibration characteristics were constructed using by two kits of reference materials VZh172 and VZhL21. According to statistical criteria an assessment is made of the possibility of joint use of the kits when constructing general calibration characteristics using the method of atomic emission spectrometry with inductively coupled plasma for the simultaneous determination of elements Al, Co, Cr, Mo, Nb, Ta, Ti, W, Zr, Fe, Mn in nickel alloys.

Keywords
heat-resistant nickel alloys, atomic emission spectrometry, inductively coupled plasma, reference materials, comparison of reference materials, calibration, chemical analysis.
Reference list
  1. Karpov Yu.A., Baranovskaya VB Analytical control is an integral part of materials diagnostics. Zavodskaya laboratoriya. Diagnostika materialov, 2017, vol. 83, no. 1, pp. 5–12.
  2. Karpov Yu.A., Baranovskaya VB Problems of standardization of methods of chemical analysis in metallurgy. Zavodskaya laboratoriya. Diagnostika materialov, 2019, vol. 85, no. 1–2, pp. 5-14.
  3. Kablov E.N. Quality control of materials is a guarantee of the safety of aircraft operation. Aviacionnye materialy i tehnologii, 2001, no. 1, pp. 3–8.
  4. Kablov E.N., Chabina E.B., Morozov G.A., Muravskaya N.P. Conformity assessment of new materials using high-level CRM and MI. Kompetentnost, 2017, no. 2 (143), pp. 40–46.
  5. Lomberg B.S., Ovsepjan S.V., Bakradze M.M., Letnikov M.N., Mazalov I.S. The application of new wrought nickel alloys for advanced gas turbine engines. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 116–129. DOI: 10.18577/2071-9140-2017-0-S-116-129.
  6. Kosmin A.A., Budinovskiy S.A., Muboyadzhyan S.A. Heat and corrosion resistant coating for working turbine blades from promising high-temperature alloy VZhL21. Aviacionnye materialy i tehnologii, 2017, no. 1 (46), pp. 17–24. DOI: 10.18577/2071-9140-2017-0-1-17-24.
  7. Gundobin V.I., Titov V.I., Orlov G.V., Pchelkin A.I. Development of monolithic standard samples of the composition of cast heat-resistant nickel alloys of the Ni – Cr – Al – Co – Mo – Nb – W – Ti – V system for spectral analysis. Liteyshchik Rossii, 2014, no. 7, pp. 21–24.
  8. Karpov Yu.A., Baranovskaya VB The role and possibilities of analytical control in metallurgy. Tsvetnye metally, 2016, no. 8 (884). S. 63–67. DOI: 10.17580/tsm.2016.08.09.
  9. Chernikova I.I., Kostrikina T.V., Tyumneva K.V., Ermolaeva T.N. Application of standard samples of blast-furnace, steelmaking, converter slags and welding fused fluxes in the development of methods for analyzing slag-forming mixtures by atomic emission spectrometry with inductively coupled plasma. Standartnye obraztsy, 2017, no. 3-4, pp. 29–40. DOI: 10.20915/2077-1177-2017-13-3-4-29-40.
  10. Nalobin D.P., Osintseva E.V. Methods for comparing standard samples of the composition of substances and materials. Standartnye obraztsy, 2006, no. 1 (3), pp. 36–44.
  11. Stepanovskikh V.V., Guzeev L.I. Comparison of domestic and foreign reference materials on the SA-2000 device. Analitika i kontrol, 2000, vol. 4, no. 3, pp. 293–297.
  12. Saprygin A.V., Golik V.M., Makarov A.A., Dzhavaev B.G., Kudryavtsev V.N. Comparison of standard samples of isotopic composition of uranium produced by NBL (USA) and UEKhK. Standartnye obraztsy, 2007, no. 2, pp. 39–48.
  13. Gundobin N.V., Titov V.I., Pchelkin A.I. Standard samples of the composition of high-temperature nickel alloys of the Ni – Al – Co – Mo – Nb – Ta – Cr – W – Re system for spectral analysis. Zavodskaya laboratoriya. Diagnostika materialov, 2015, vol. 81, no. 2, pp. 71–74.
  14. Orlov G.V., Titov V.I. X-ray fluorescence and optical-emission methods of analysis of aviation alloys. Metallurgiya mashinostroeniya, 2018, no. 3, pp. 31–33.
  15. Karachevtsev F.N., Letov A.F., Protsenko O.M., Yakimova M.S. Development and application of certified reference materials of airborne advanced alloys. Trudy VIAM, 2016, no. 10, paper no. 8. Available at: http://www.viam-works.ru (accessed: July 14, 2021). DOI: 10.18577/2307-6046-2016-0-10-8-8.
  16. Karpov Yu.A., Gimelfarb F.A., Savostin A.P., Salnikov V.D. Analytical control of metallurgical production. Moscow: Metallurgy, 1995, 400 p.
  17. Otto M. Modern methods of analytical chemistry: in 2 vol. Moscow: Tekhnosfera, 2003, vol. I, 416 p.
  18. RMG 56-2002. GSE. Sets of reference materials for the composition of substances and materials. Intercomparison methodology. Moscow: Publishing house of standards, 2004.10 p.
  19. MI 3257-2009. GSE. Standard samples of materials (substances). Intercomparison technique. Eekaterinburg: UNIIM, 2009, 36 p.
  20. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  21. Kablov E.N. Aviation materials science in the XXI century. Prospects and tasks. Aviation materials. Selected works of VIAM 1932–2002. Moscow: MISIS-VIAM, 2002, pp. 23–47.
  22. Kablov E.N. Trends and guidelines for innovative development in Russia: collection of articles. sci.-inf. materials. 3rd ed. Moscow: VIAM, 2015, 720 p.
  23. Letov A.F., Karachevtsev F.N., Zagvozdkina T.N. Development the set of methods measurements of the chemical composition of nickel-based alloys. Trudy VIAM, 2018, no. 8 (68), paper no. 09. Available at: http://www.viam-works.ru (accessed: July 15, 2021). DOI: 10.18577/2307-6046-2018-0-8-89-97.
  24. Karachevtsev F.N., Zagvozdkina T.N., Dvoretskov R.M., Zyablikova I.N. Application of model solutions in the development and implementation of AES-ICP techniques. Vse materialy. Entsiklopedicheskiy spravochnik, 2015, no. 2, pp. 10–15.
  25. Karachevtsev F.N., Alekseev A.V., Letov A.F., Dvoretskov R.M. Plasma methods of nickel alloys elemental chemical composition analysis. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 483–497. DOI: 10.18577/2071-9140-2017-0-S-483-497.
  26. Osintseva E.V. Comparisons of reference materials: experimental planning and processing of measurement results. Standartnyye obraztsy, 2016, no. 4, pp. 3–14. DOI: 10.20915/2077-1177-2016-0-4-3-14.
  27. Dörffel K. Statistics in analytical chemistry. Moscow: Mir, 1994.268 p.
  28. Garmash A.V., Sorokina N.M. Metrological foundations of analytical chemistry. Moscow: Moscow State University, 2012, 47 p.