Postnov V.I., Satdinov R.A., Makrushin K.V., Ivanov M.S. Issues of constructive and technological development of flexible pipelines made of polymer composite materials for air conditioning systems // Proceedings of VIAM. 2021. No. 1 (95). Ст. 07. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2021-0-1-66-76.

Issues of constructive and technological development of flexible pipelines made of polymer composite materials for air conditioning systems

Postnov V.I., Satdinov R.A., Makrushin K.V., Ivanov M.S.
Abstract

The main issues of structural and technological development of flexible pipelines made of polymer composite materials (PCM) of air conditioning systems (ACS) of modern aviation equipment are discussed. The analysis of existing designs of flexible pipelines of ACS from PCM is carried out. The main results of research, samples of flexible pipelines from PCM and the General scheme of the technological process of manufacturing flexible pipelines are shown.

Keywords
polymer composite materials, flexible pipes, air conditioning systems, elastic sheath, spiral reinforcement, thermosetting binder.
Reference list
  1. State Standard 22607–77. Air conditioning systems for aircraft and helicopters. Terms and Definitions. Moscow: Publishing house of standards, 1977, 7 p.
  2. Tkacheva V.R., Galka G.A. Review of existing air conditioning systems. Molodoy ucheniy, 2016, no. 23 (127), pp. 91–95.
  3. Kablov E.N. What to make the future of. New generation materials, technologies for their creation and processing - the basis of innovations. Krylya Rodiny, 2016, no. 5, pp. 8–18.
  4. Kablov E.N. VIAM: Materials of a new generation for PD-14. Krylya Rodiny, 2019, no. 7-8, pp. 54–58.
  5. Satdinov R.A., Veshkin E.A., Postnov V.I., Strelnikov S.V. РСМ low-pressure air ducts in aircraft. Trudy VIAM, 2016, no. 8, paper no. 8. Available at: http://www.viam-works.ru (accessed: October 23, 2020). DOI: 10.18577/2307-6046-2016-0-8-8-8.
  6. Veshkin E.A., Satdinov R.A., Postnov V.I., Strelnikov S.V. Modern polymer materials for manufacture of elements of the air conditioning system in flying apparatus. Trudy VIAM, 2017, no. 12 (60), paper no. 06. Available at: http://www.viam-works.ru (accessed: March 23, 2020). DOI: 10.18577/2307-6046-2017-0-12-6-6.
  7. Grashchenkov D.V. Strategy of development of non-metallic materials, metal composite materials and heat-shielding. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 264–271. DOI: 10.18577/2071-9140-2017-0-S-264-271.
  8. Kablov E.N. Marketing of materials science, aircraft construction and industry: present and future. Direktor po marketingu i sbytu, 2017, no. 5-6, pp. 40–44.
  9. Kablov E.N. We should not assemble aircraft from foreign components. Intellekt i tekhnologii, 2014, no. 3 (9), pp. 28–35.
  10. Ivanov M.S., Postnov V.I., Sapego E.O., Sapego Yu.A. Thermoplastic non-flammable strand for reinforcement of flexible pipeline SKV. Vse materialy. Entsiklopedicheskiy spravochnik, 2020, no. 12, pp. 38–44.
  11. Ivanov M.S., Veshkin E.A. Thermoplastic materials in the design of a flexible pipeline of the air conditioning system of aircraft. Thermoplastic materials and functional coatings: materials of All-Rus. Scientific and Technical Conf. (Moscow, April 23, 2019) Moscow: VIAM, 2019, pp. 68–78.
  12. Ivanov M.S., Veshkin E.A., Satdinov R.A., Donskikh I.N. New domestic coated textile material for flexible air conditioning ducts of flight vehicles. Trudy VIAM, 2019, no. 4 (76), DOI: 10.18577/2307-6046-2019-0-4-57-66.
  13. Cloth film material and product based on it: pat. 2733779 Rus. Federation. no. 2019136152; filed 11.11.19; publ. 06.10.20.
  14. Grigolyuk E.I., Kulikov G.M. Multi-layer reinforced casings. Calculation of pneumatic tires. Moscow: Mashinostroenie, 1988, 91 p.
  15. Flexible hose: pat. 2015916 Rus. Federation, no. 5025406/05; filed 04.02.92; publ. 15.07.94.
  16. A method of manufacturing elastic tubular products reinforced with a spiral of stiffness: pat. 2460645 Rus. Federation, no. 2010140245/05; filed 04.10.10; opubl. 10.09.12.
  17. Orlova O.V., Fomicheva T.N., Okunchikov A.Z., Kurskiy G.R. Technology of varnishes and paints. Moscow: Chemistry, 1980, 79 p.
  18. Sorokin M.F., Shode L.G., Kochneva Z.A. Chemistry and technology of film-forming substances. Moscow: Chemistry, 1981, 160 p.
  19. Flexible pipeline made of polymer composite material: pat. 2733797 Rus. Federation, no. 2019136153; filed 11.11.19, publ. 06.10.20.
  20. Krysin V.N., Krysin M.V. Technological processes of forming, winding and gluing structures. Moscow: Mashinostroenie, 1989, 140 p.