Rassokhina L.I., Bityutskaya O.N., Gamazina M.V., Avdeev V.V. Research of compositions of ceramic rods based on fused quartz and their manufacturing technology // Proceedings of VIAM. 2021. No. 1 (95). Ст. 04. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2021-0-1-34-42.

Research of compositions of ceramic rods based on fused quartz and their manufacturing technology

Rassokhina L.I., Bityutskaya O.N., Gamazina M.V., Avdeev V.V.
Abstract

The results of research on the selection of raw materials (ceramic charge, thermoplasticizer) and experimental compositions of the core mass for the manufacture of ceramic rods from fused quartz are presented. The optimal technological parameters were selected and the technology for manufacturing the core mass of experimental compositions was developed. The results of studies of technological parameters for the production of ceramic samples of experimental rod compositions based on fused quartz are presented. According to the results of these studies, the optimal one is selected.

Keywords
fused quartz, core mass based on fused quartz, ceramic core, wax model with a ceramic core, casting of a cooled blade.
Reference list
  1. Cast blades of gas turbine engines: alloys, technology, coatings. Ed. E.N. Kablov. Moscow: Nauka, 2006, 632 p.
  2. Kablov E.N., Folomeykin Yu.I., Demonis I.M. Highly refractory ceramic rods and molds for casting cooled blades of gas turbine engines. Int. scientific-practical. conf. «Science and technology of silicate materials – the present and the future»: collection of articles in 2 vol. St. Petersburg: Information of Education, 2003. vol. 2. pp. 49–56.
  3. Belyakov A.V., Razumnova I.V., Demonis I.M., Folomeykin Yu.I. Easily removable ceramic rods for casting GTE blades according to investment models. Steklo i keramika, 2012, no. 4. pp. 26–31.
  4. Landa M.I., Kopytov N.N. Influence of the grain size composition of the powder composition on the properties of porous corundum ceramics with increased strength. Ogneupory, 1984, no. 4. pp. 21–25.
  5. Bakunov V.S., Balkevich V.L., Vlasov A.S. et al. Ceramics from highly refractory oxides. Moscow: Metallurgiya, 1977, 304 p.
  6. Strelov K.K. Structure and properties of refractories. Moscow: Metallurgiya, 1982, 208 p.
  7. Folomeykin Yu.I. Formation of the structure of porous highly refractory ceramic material of granular structure. Steklo i keramika, 2015, no. 8. pp. 30–35.
  8. Mix for the manufacture of casting ceramic rods of hollow blades from heat-resistant alloys by investment casting: pat. 2691435 Rus. Federation; filed 23.07.18; publ. 13.06.19.
  9. Mix for the manufacture of foundry ceramic rods: pat. 2273543 Rus. Federation; filed 01.09.04; publ. 10.04.06.
  10. Kablov E.N., Ospennikova O.G., Svetlov I.L. Highly efficient cooling of GTE hot section blades. Aviacionnye materialy i tehnologii, 2017, no. 2 (47), pp. 3–14. DOI: 10.18577/2071-9140-2017-0-2-3-14.
  11. Ospennikova O.G., Rassokhina L.I., Bityutskaya O.N., Gamazina M.V. Optimization of the production technology of ceramic rods to improve the quality of cast blades of gas turbine engines. Novosti materialovedeniya. Nauka i tekhnika, 2017. no. 3, paper. no. 04. Available at: http://www.materialsnews.ru (accessed: November 30, 2020).
  12. Ospennikova O.G., Rassohina L.I., Bitjuckaja O.N., Gamazina M.V. Development of technology for production of castings by the method of direc-tional solidification of GTE blades made of alloys based on Nb–Si composite. Trudy VIAM, 2017, no. 4 (52), paper no. 01 Available at: http://www.viam-works.ru (accessed: November 30, 2020). DOI: 10.18577/2307-6046-2017-0-4-1-1.
  13. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  14. Loshchinin Yu.V., Shorstov S.Yu., Kuzmina I.G. Research of influence of technology factors on thermal conductivity of ceramic casting molds. Aviacionnye materialy i tehnologii, 2019, no. 2 (55), pp. 89–94. DOI: 10.18577 / 2071-9140-2019-0-2-89-94.
  15. Zuev A.V., Loshchinin Yu.V., Barinov D.Ya., Marakhovskij P.S. Computational and experimental investigations of thermophysical properties. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 575–595. DOI: 10.18577/2071-9140-2017-0-S-575-595.
  16. Loshchinin Yu.V., Folomeykin Yu.I., Rykova T.P. Marakhovsky P.S., Pakhomkin S.I. Thermovisual properties of ceramic materials of molds and rods for casting GTE blades from heat-resistant alloys. Materialovedenie, 2014, no. 3 (204). pp. 47–52.