Sagomonova V.A., Dolgopolov S.S., Tselikin V.V., Sorokin A.E. Investigation of the effect of an integrated vibration-absorbing layer on the properties of composite three-layer soundproofing sandwich panels // Proceedings of VIAM. 2020. No. 9 (91). Ст. 10. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2020-0-9-87-95.
Investigation of the effect of an integrated vibration-absorbing layer on the properties of composite three-layer soundproofing sandwich panels
Abstract
Presents the results of a study of the influence of the presence of an integrated vibration absorbing layer on the physical and vibration damping properties of the experimental samples of composite heat- and soundproofing panels of various compositions and structures. The factors affecting the level of properties of the manufactured experimental samples of composite heat- and soundproofing panels are established. The influence of the composition and structure of experimental samples of composite heat- and soundproofing panel on its characteristics is analyzed.
Keywords
sandwich panel, polymer composite material, sheathing, fiberglass, prepreg, honeycomb, core, fiberglass reinforced plastic, integrated vibration-absorbing layer, mechanical loss coefficient
Reference list
- Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
- Kablov E.N. The key problem is materials. Tendentsii i oriyentiry innovatsionnogo razvitiya Rossii. Moscow: VIAM, 2015, pp. 458–464.
- Kablov E.N. At the crossroads of science, education and industry. Ekspert, 2015, no. 15 (941), pp.49–53.
- Raskutin A.E. Russian polymer composite materials of new generation, their exploitation and implementation in advanced developed constructions. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 349–367. DOI: 10.18577/2071-9140-2017-0-S-349-367.
- Raskutin A.E. Development strategy of polymer composite materials. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 344–348. DOI: 10.18577/2071-9140-2017-0-S-344-348.
- Grashchenkov D.V. Strategy of development of non-metallic materials, metal composite materials and heat-shielding. Aviacionnye materialy i tehnologii, 2017, No. S, pp. 264–271. DOI: 10.18577/2071-9140-2017-0-S-264-271.
- Young M.V., Reshetnikova E.V., Zakharov V.A. Constructive and technological features of the manufacture of interior panels for passenger aircraft. Vestnik Voronezhskogo gosudarstvennogo tekhnicheskogo universiteta, 2011, no. 11-2, pp. 48–50.
- Minakov V.T., Postnov V.I., Shvets N.I., Zastrogina O.B., Petukhov V.I., Makrushin K.V. Features of the manufacture of three-layer honeycomb panels with a hot-curing polymer filler. Aviacionnye materialy i tehnologii, 2009, no. 3, pp. 6–9.
- Kavun N.S., Abramov P.A., Yudin A.A., Barbotko S.L. Investigation of the properties of three-layer panels based on a modified binder FPR-520G. Aviacionnye materialy i tehnologii, 2009, no. 3, pp.19–23.
- Barannikov A.A., Veshkin E.A., Postnov V.I., Strelnikov S.V. On the issue of production of floor panels from PCM for aircraft (review article). Izvestiya Samarskogo nauchnogo tsentra RAN, 2017, vol. 19, no. 4 (2), pp.198–212.
- Testoedov N.A., Nagovitsin V.N., Permyakov M.Yu. Application of three-layer honeycomb structures in space vehicles. Vestnik Sibirskogo gosudarstvennogo aerokosmicheskogo universiteta im. akademika M.F. Reshetneva, 2016, vol. 17, no.1, pp. 200–211.
- Sagomonova V.A., Sytyi Yu.V., Kislyakova V.I., Dolgopolov S.S. Investigation of the damping properties of vibration-absorbing materials based on thermoplastic elastomers. Aviacionnye materialy i tehnologii, 2014, no. S3, pp. 5–10. DOI: 10.18577 / 2071-9140-2014-0-s3-5-10.
- Kablov E.N., Sagomonova V.A., Sorokin A.E., Tselikin V.V., Gulyaev A.I. Investigation of the structure and properties of a polymer composite material with an integrated vibration-absorbing layer. Vse materialy. Entsiklopedicheskiy spravochnik, 2020, no. 3, pp. 2–9.
- Polymer composite material with an integrated vibration-absorbing layer: pat. 2687938 Rus. Federation; filed 07.11.18; publ. 16.05.19.
- Fiber-reinforced composite material and molding thereof: pat. 2016210027A JP; filed 30.04.15; publ. 15.12.16.
- Sandwich panel: pat. 2006002869A JP; filed 18.06.04; publ. 05.01.06.
- Kishi H., Kuwata M., Matsuda S., Asami T., Murakami A. Damping properties of thermoplastic-elastomer interleaved carbon fiber-reinforced epoxy composites. Composites Science and Technology, 2004, vol. 64, no. 16, pp. 2517–2523.
- Vibration-damping fiber-reinforced composite material: pat. 2009078422A JP; ffiled 26.09.07; publ. 16.04.09.
- Fotsing E.R., Sola M., Ross A., Ruiz E. Dynamic characterization of viscoelastic materials used in composite structures. Journal of Composite Materials, 2013, vol. 48, no. 30, pp. 3815–3825.
- Soundproofing trim panel for helicopter type rotorcraft, has core that is melamine self-extinguishing foam in which inserts are arranged, and skins provided with carbon cloth layers respectively: pat. 2939406B1 FR; filed 05.12.08; publ. 12.07.13.
- Structural composite material with improved acoustic and vibrational damping properties: pat. 20100170746A1 US; filed 06.01.10; publ. 08.07.10.
- Multilayer and composition gradient structures with improved damping properties: pat. 20120164907 US; filed 09.12.11; publ. 28.06.12.
- Composite article including viscoelastic layer with barrier layer: pat. 2010151186 US; filed 15.12.09; publ. 17.06.10.