Kolobkov A.S. Influence of non-woven thermoplastic materials on the strength of layered polymer composite materials (review) // Proceedings of VIAM. 2020. No. 9 (91). Ст. 05. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2020-0-9-44-51.
Influence of non-woven thermoplastic materials on the strength of layered polymer composite materials (review)
Abstract
Рrovides an overview of the work carried out to find ways to increase the interlayer effects in polymer composite materials and in particular shock loads. Discusses the use of nanofibersveils in the manufacture of laminated CFRP and the change in strength characteristics of the obtained materials, depending on different surface density nanofiber veils and their chemical composition. There is a General tendency to increase the interlayer strength in carbon fiber when using nanofiber veils with a slight decrease in the elastic modulus.
Keywords
polymer composite materials, carbon fiber plastics, nanofiber veils, impact strength, mechanical property, nanofiber.
Reference list
- Kablov E.N., Semenova L.V., Petrova G.N., Larionov S.A., Perfilova D.N. Polymer composite materials on a thermoplastic matrix. News of higher educational institutions. Ser .: Chemistry and Chemical Technology. 2016, vol. 59, no. 10, pp. 61–71.
- Kablov E.N., Chursova L.V., Babin A.N., Mukhametov R.R., Panina N.N. Developments of FSUE "VIAM" in the field of melt binders for polymer composite materials. Polymer materials and technologies, 2016, vol. 2, no. 2, pp. 37–42.
- Gunyayeva A.G., Sidorina A.I., Kurnosov A.O., Klimenko O.N. Polymeric composite materials of new generation on the basis of binder VSE-1212 and the filling agents alternative to ones of Porcher Ind. and Toho Tenax. Aviacionnye materialy i tehnologii, 2018, no. 3 (52), pp. 18–26. DOI: 10.18577/2071-9140-2018-0-3-18-26.
- Shenming C., Yan L., Hong-Yuan L., Yiu-Wing M. Effect of electrospun polysulfone/cellulose nanocrystals interleaves on the interlaminar fracture toughness of carbon fiber/epoxy composites. Composite Science and Technology, 2019, vol. 181, pp. 1–8. DOI: 10.1016/j.compscitech.2019.05.030.
- Krylov V.D., Yakovlev N.O., Kurganova Yu.A., Lashov O.A. Mezhsloyevy crack firmness of constructional polymeric composite materials. Aviacionnye materialy i tehnologii, 2016, no. 1 (40), pp. 79–85. DOI: 10.18577/2071-9140-2016-0-1-79-85.
- Platonov A.A. Polymer composite materials on a base of stitched preforms with high impact resistance. Aviacionnye materialy i tehnologii, 2014, No. 4, pp. 43–47. DOI: 10.18577/2071-9140-2014-0-4-43-47.
- Ni X., Furtado C., Kalfon C.E., Zhou Y., Valdes G.A., Hank T.J. et al. Static and fatigue interlaminar shear reinforcement in aligned carbon nanotube-reinforced hierarchical advanced composites. Composites. Part A, 2019, vol. 120, pp. 106–115. DOI: 10.1016/j.compositesa.2019.02.023.
- Kondrashov S.V., Shashkeev K.A., Petrova G.N., Mekalina I.V. Constructional polymer composites with functional properties. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 405–419. DOI: 10.18577/2071-9140-2017-0-S-405-419.
- Zhang J.S., Wang Y.T., Wang X.S., Ding G.W., Pan Y.Q., Xie H.F. et al. Effects of aminofunctionalized carbon nanotubes on the properties of amine-terminated butadieneacrylonitrile rubber-toughened epoxy resins. Applied Polymer Science, 2014, vol. 131, pp. 1–7. DOI: 10.1002/app.40472.
- Chikhi N., Fellahi S., Bakar M. Modification of epoxy resin using reactive liquid (ATBN) rubber. European Polymer Journal, 2002, vol. 38 (2), pp. 251–264. DOI: 10.1016/S0014-3057(01)00194-X.
- Shuai Z., Zhengguo C., Roger T., Chao C., Zeyu S., Lei X. et al. Highly improving the mechanical and thermal properties of epoxy resin via blending with polyetherketone cardo. Composite Communications, 2019, vol. 13, pp. 80–84. DOI: 10.1016/j.coco.2019.03.003.
- Jing Z., Xuming X. Influence of addition of silica particles on reaction-induced phase separation and properties of epoxy/PEI blends. Composite. Part B, 2011, vol. 42, pp. 2163–2169. DOI: 10.1016/j.compositesb.2011.05.013.
- Weizhen L., Zonglian X., Ao L., Yang L., Baoyu W., Wenjun G. Effect of SiO2 nanoparticles on the reaction induced phase separation in dynamically asymmetric epoxy/PEI blends. Research Advances, 2015, vol. 5, pp. 8471–8478. DOI: 10.1039/C4RA12261E.
- Gangineni P.K., Yandrapu S., Ghosh S.K., Anand A., Prusty R.K., Ray B.C. Mechanical behavior of graphene decorated carbon fiber reinforced polymer composites: an assessment of the influence of functional groups. Composite. Part A, 2019, vol. 122, pp. 36–44. DOI: 10.1016/j.compositesa.2019.04.017.
- Ou Y., González C., Vilatela J.J. Interlaminar toughening in structural carbon fiber/epoxy composites interleaved with carbon nanotube veils. Composite. Part A, 2019, vol. 124, pp. 1–11. DOI: 10.1016/j.compositesa.2019.105477.
- Ning H., Li Y., Li J., Hu N., Liu Y., Wu L. et al. Toughening effect of CB-epoxy interleaf on the interlaminar mechanical properties of CFRP laminates. Composite. Part A, 2015, vol. 68. P. 226–234. DOI: 10.1016/j.compositesa.2014.09.030.
- Ning H., Li J., Hu N., Yan C., Liu Y., Wu L. et al. Interlaminar mechanical properties of carbon fiber reinforced plastic laminates modified with graphene oxide interleaf. Carbon, 2015, vol. 91, pp. 224–233. DOI: 10.1016/j.carbon.2015.04.054.
- Qian X., Kravchenko O.G., Pedrazzoli D., Manas-Zloczower I. Effect of polycarbonate film surface morphology and oxygen plasma treatment on mode I and II fracture toughness of interleaved composite laminates. Composite. Part A, 2018, vol. 105, pp. 138–149. DOI: 10.1016/j.compositesa.2017.11.016.
- Quan D., Flynn S., Artuso M., Murphy N., Rouge C., Ivankovic A. Interlaminar fracture toughness of CFRPs interleaved with stainless steel fibres. Composite Structurer, 2019, vol. 210, pp. 49–56. DOI: 10.1016/j.compstruct.2018.11.016.
- Kuwata M., Hogg P.J. Interlaminar toughness of interleaved CFRP using non-woven veils: Part 1. Mode-I testing. Composite. Part A, 2011, vol. 42, pp. 1551–1559. DOI: 10.1016/j.compositesa.2011.07.016.
- Beylergil B., Tanoglu M., Aktas E. Mode-I fracture toughness of carbon fiber/epoxy composites interleaved by aramid nonwoven veils. Steel Composite Structure, 2019, vol. 31, pp. 113–123.
- Kumar V., Ramakrishna S., Yoong J.L., Neisiany R., Surendran S., Balaganesan G. Electrospun nanofiber interleaving in fiber reinforced composites-Recent trends. Mater Des Process Communication, 2019, vol. 1 (1), pp. 24–32. DOI: 10.1002/mdp2.24.
- Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
- Wong D.W.Y., Lin L., McGrail P.T., Peijs T., Hogg P.J. Improved fracture toughness of carbon fibre/epoxy composite laminates using dissolvable thermoplastic fibers. Composite. Part A, 2010, vol. 41, pp. 759–767. DOI: 10.1016/j.compositesa.2010.02.008.
- Tsotsis T.K. Interlayer toughening of composite materials. Polymer Composites, 2009, vol. 30, pp. 70–86. DOI: 10.1002/pc.20535.
- Wong D.W.Y., Zhang H., Bilotti E., Peijs T. Interlaminar toughening of woven fabric carbon/epoxy composite laminates using hybrid aramid/phenoxy interleaves. Composite. Part A, 2017, vol. 101, pp. 151–159. DOI: 10.1016/j.compositesa.2017.06.001.
- Li G., Li P., Zhang C., Yu Y., Liu H., Zhang S. et al. Inhomogeneous toughening of carbon fiber/epoxy composite using electrospun polysulfone nanofibrous membranes by in situ phase separation. Composite Science and Technology, 2008, vol. 68, pp. 987–994. DOI: 10.1016/j.compscitech.2007.07.010.
- Peng L., Dawei L., Bo Z., Xiaolong J., Lili W., Li G. Synchronous effects of multiscale reinforced and toughened CF/EP composites by MWNTs-EP/PSF hybrid nanofibers with preferred orientation. Composite, Part A. 2015, vol. 68, pp. 72–80. DOI: 10.1016/j.compositesa.2014.09.010.
- Chao C., Chenyu Z., Jinli Z., Minqiang J., Zeyu S., Shuai Z. et al. Improving the interlaminar toughness of the carbon fiber/epoxy composites via interleaved with polyethersulfone porous films. Composite Science and Technology, 2019, vol. 183, pp. 1–12. DOI: 10.1016/j.compscitech.2019.107827.
- Beylergil B., Tanoglu M., Aktas E. Enhancement of interlaminar fracture toughness of carbon fiber epoxy composites using polyamide-6,6 electrospun nanofibers. Applied Polymer Science, 2017, vol. 134 (35), pp. 1–12. DOI: 10.1002/app.45244.
- Beylergil B., Tanoglu M., Aktas E. Effect of polyamide-6,6 (PA 66) nonwoven veils on the mechanical performance of carbon fiber/epoxy composites. Composite Structure, 2018, vol. 194. P. 21–35. DOI: 10.1016/j.compstruct.2018.03.097.
- Ramirez V.A., Hogg P.J., Sampson W.W. The influence of the nonwoven veil architectures on interlaminar fracture toughness of interleaved composites. Composite Science and Technology, 2015, vol. 110, pp. 103–110. DOI: 10.1016/j.compscitech.2015.01.016.
- Beckermann G.W., Pickering K.L. Mode I and Mode II interlaminar fracture toughness of composite laminates interleaved with electrospun nanofibre veils. Composite. Part A, 2015, vol. 72. P. 11–21. DOI: 10.1016/j.compositesa.2015.01.028.
- Beckermann G.W. Nanofiber interleaving veils for improving the performance of composite laminates. Reinforced Plastic, 2017, vol. 61, pp. 289–293. DOI: 10.1016/j.repl.2017.03.006.
- Daelemans L., van der Heijden S., Baere I.D., Rahier H., Paepegem W.V., Clerck K.D. Nanofibre bridging as a toughening mechanism in carbon/epoxy composite laminates interleaved with electrospun polyamide nanofibrous veils. Composite Science and Technology, 2015, vol. 117, pp. 244–256. DOI: 10.1016/j.compscitech.2015.06.021.
- Chao C., Zhengguo C., Zhuang H. Simultaneously improving mode I and mode II fracture toughness of the carbon fiber/epoxy composite laminates via interleaved with uniformly aligned PES fiber webs. Composites. Part A, 2020, vol. 129, pp. 1–11. DOI: 10.1016/j.compositesa.2019.105696.