Venediktova M.A., Petrova A.P., Barbotko S.L., Bryk Ya. А. Application of new environmentally friendly organophosphorus flame retardants in the composition of heat-protective putty // Proceedings of VIAM. 2020. No. 9 (91). Ст. 04. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2020-0-9-35-43.

Application of new environmentally friendly organophosphorus flame retardants in the composition of heat-protective putty

Venediktova M.A., Petrova A.P., Barbotko S.L., Bryk Ya. А.
Abstract

In work the assessment of possibility of replacement of Fospoliol-II as a part of heat-protective putty on new environmentally friendly organophosphorus flame retardants of domestic production for the purpose of decrease in toxicity and environmental pollution when manufacturing and processing has been carried out. The comparative assessment of ecological safety of flame retardants, and also mechanical, thermophysical characteristics of heat-protective putty with Fospoliolom-II and new fire-retarding agents is carried out.

Keywords
polymer composite materials, flame retardants, organophosphorus compound, putty.
Reference list
  1. Schmidt D.L. Ablation. Structural properties of plastics (physicochemical bases of application). Moscow: Khimiya, 1967, pp. 401–456.
  2. Mikhailin Yu.A. Special polymer composite materials. Saint Petersburg: Nauchnye osnovy i tekhnologii, 2008, 660 p.
  3. Pankratov B.M. Descent vehicles. Moscow: Mashinostroenie, 1984, 232 p.
  4. Avduevsky V.S., Galitseysky B.M., Glebov G.L. et al. Fundamentals of heat transfer in aviation and rocket technology. Moscow: Mashinostroenie, 1975, 624 p.
  5. Kablov E.N. Materials and chemical technologies for aircraft engineering. Herald of the Russian Academy of Sciences, 2012, vol. 82, no. 3, pp. 158-167.
  6. Kablov E.N. Chemistry in Aviation Materials Science. Russian Chemical Journal. 2010, vol. LIV, no. 1, pp. 3–4.
  7. Grashchenkov D.V. Strategy of development of non-metallic materials, metal composite materials and heat-shielding. Aviacionnye materialy i tehnologii, 2017, No. S, pp. 264–271. DOI: 10.18577/2071-9140-2017-0-S-264-271.
  8. Zweifel H., Maer RD, Schiller M. Additives to polymers: a reference book. SSaint Petersburg: Professiya, 2010, 1144 p.
  9. Tkachuk A.I., Afanasyeva E.A. Reactive type flame retardants for epoxy resins. Part 2. Trudy VIAM, 2020, no. 4-5 (88), paper no. 02. Available at: http://www.viam-works.ru (accessed: July 1, 2020). DOI: 10.18577/2307-6046-2020-0-45-13-21.
  10. Chizhova M.A., Khairullin R.Z. Toxicity of combustion products of polymeric materials with the introduction of fire retardants into their composition. Vestnik Kazanskogo tekhnologicheskogo universiteta, 2014, vol. 17, no. 9, pp. 144–145.
  11. Mikhailin Yu.A. Heat-resistant polymers and polymer materials. Saint Petersburg: Professiya, 2006, 624 p.
  12. Torre L., Kenny J.M., Maffezzoli A.M. Degradation behavior of a composite material for thermal protection systems. Part I. Experimental characterization. Journal of Material Science, 2010, vol. 33, no. 12, pp. 3137–3143.
  13. Barbotko S.L., Volny O.S., Kirienko O.A., Shurkova E.N. Assessment of the fire safety of polymer materials for aviation purposes: analysis of the state, test methods, development prospects, methodological features. Moscow: VIAM, 2018, 424 p.
  14. Lukina A.I., Parakhin I.V. Thermo-protection properties of hetero-chain properties. Trudy VIAM, 2016, no. 11 (47), paper no. 04. Available at: http://www.viam-works.ru (accessed: July 1, 2020). DOI: 10.18577/2307-6046-2016-0-11-4-4.
  15. Chanda M., Roy S.K. Industrial polymer, specialty polymers, and their applications. CRC Press Taylor & Francis Group, 2009, 432 p.
  16. Gren M. Flame Retardant Chemicals: Technologies and Global Markets. BCC Research, 2015, 164 p.
  17. Polymer Green Flame Retardant. Ed. C.D. Papaspyrides, P. Kiliaris. Elsevier, 2014, 943 p.
  18. Serkova EA, Zastrogina O. B., Barbotko S. L. Study of the possibility of use of new environmentally friendly organophosphorus flame retardants in the composition of binders for interior fire safety materials. Trudy VIAM, 2019, no. 2 (74), paper no. 03. Available at: http://www.viam-works.ru (accessed: July 1, 2020). DOI: 10.18577/2307-6046-2019-0-2-24-34.
  19. Mukhametov R.R., Petrova A.P. Thermosetting binders for polymer composites (review). Aviacionnye materialy i tehnologii, 2019, no. 3 (56), pp. 48–58. DOI: 10.18577/2071-9140-2019-0-3-48-58.
  20. Mashlyakovsky L.N., LykovA.D., Repkin V.Yu. Organic coatings of low flammability: textbook. Leningrad: Chemistry, 1989, 184 p.
  21. Venediktova M.A., Petrova A.P., Bryk Ya.A., Krasnov L.L. Investigation of the possibility of using new environmentally friendly fire retardants in the composition of a polymer heat-protective putty. Abstracts of the All-Russian. scientific and technical conf. «Thermoplastic materials and functional coatings». Moscow, 2019, pp. 55–68.
  22. Organization for the Prohibition of Chemical Weapons. Chemical Weapons Convention. Available at: http://www.opcw.org/ru (date of access: 01.07.2020).
  23. Koitov S.A., Melnikov V.N. Analysis of the thermophysical properties of polymers in order to select the optimal composite material for the heat-shielding coating of an aircraft. Vestnik YUUrGU, 2012, no. 12, pp. 194–198.
  24. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  25. Barbotko S.L. Development of the fire safety test methods for aviation materials. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 516–526. DOI: 10.18577/2071-9140-2017-0-S-516-526.
  26. Aviation Regulation 25. Standards of airworthiness of transport category aircraft. Moscow: Aviaizdat, 2009, 274 p.