Kablov E.N., Lukinа E.A., Zavodov A.V., Efimochkin I.Yu. The formation of structure in ultrafine WC–Co carbide material in the presence of inhibitory additives // Proceedings of VIAM. 2020. No. 4-5 (88). Ст. 10. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2020-0-45-89-99.

The formation of structure in ultrafine WC–Co carbide material in the presence of inhibitory additives

Kablov E.N., Lukinа E.A., Zavodov A.V., Efimochkin I.Yu.
Abstract

Samples of 6 milling cutters from different producers made of WC–Co carbide material were studied. Correlation dependences of hardness and coercive force on the size of grain WC and specific interfacial surface are constructed based on the carried out researches. It is shown that the value of the coercive force can indirectly estimate the grain size WC. The results of the mapping and distribution profiles of the inhibitors over the volume of Co-bundles reveal the nature of this distribution: V is concentrated mainly at the borders of tungsten carbide, while the Cr is uniformly distributed over the volume of Co binder.

Keywords
cemented carbide, tungsten carbide, WC–Co, inhibitor, coercive force, Co-binder, hardness.
Reference list
  1. Kablov E.N. The key problem is materials. Tendentsii i oriyentiry innovatsionnogo razvitiya Rossii. Moscow: VIAM, 2015, pp. 458–464.
  2. Kablov E.N. Materials are the basis of any business. Delovaya slava Rossii, 2013, no. 2, pp. 4–9.
  3. Kablov E.N. At the crossroads of science, education and industry. Ekspert, 2015, no. 15 (941), pp. 49–53.
  4. Reva V.P., Onishchenko D.V., Petrov V.V. et al. Formation of VK8 hard alloy using tungsten carbide powder synthesized by mechanochemical technology. Novyye ogneupory, 2013, no. 7, pp. 39–43.
  5. Chuvildiev V.N., Moskvicheva A.V., Boldin M.S. et al. Electropulse plasma sintering of nanostructured tungsten carbide and hard alloys based on it. Fizika tverdogo tela, 2013, no. 2, pp. 115–119.
  6. reinforcing properties of ion-plasma coatings using plasma assisted deposition. Trudy VIAM, 2015, no. 7, paper no. 07. Available at: http://www.viam-works.ru (accessed: October 29, 2019). DOI: 10.18577/2307-6046-2015-0-7-7-7.
  7. Matveev P.V., Budinovsky S.A. Influence of vacuum annealing on structure of ion-plasma coatings made with double aluminizing technology. Trudy VIAM, 2016, no. 3 (39), paper no. 08. Available at: http://www.viam-works.ru (accessed: October 29, 2019). DOI: 10.18577/2307-6046-2016-0-3-8-8.
  8. Gorlov D.S., Skripak V.I., Muboyadzhyan S.A., Egorova L.P. The research of fretting-wear slip and ion-plasma coatings. Trudy VIAM, 2017, no. 3, paper no. 07. Available at: http://www.viam-works.ru (accessed: October 29, 2019). DOI: 10.18577/2307-6046-2017-0-3-7-7.
  9. Gorlov D.S., Shhepilov A.V. Influence of surface roughness and abrasive wear on the damping capacity of the composition «alloy–coating». Trudy VIAM, 2017, no. 5, paper no. 11. Available at: http://www.viam-works.ru (accessed: October 29, 2019). DOI: 10.18577/2307-6046-2017-0-5-11-11.
  10. Garcia J., Collado V.G., Blomqvist A., Kaplan B. Cemented carbide microstructures: a review. International Journal of Refractory Metals and Hard Materials, 2019, vol. 80, pp. 40–68.
  11. Exner H.E. Physical and chemical nature of cemented carbides. International Metals Reviews, 1979, vol. 24, pp. 149–173.
  12. Takahashi T., Freise E.J. Determination of the slip system in single crystals of tungsten monocarbide. The Pilosophical Magazine: A Journal of Theoretical Experimental and Applied Physics, 1965, vol. 12, pp. 1–8.
  13. Bondarenko V.P., Gnatenko I.A. Prospects for controlling the process of forming a carbide skeleton in sintered alloys of the WC – Co system. Porodorazrushayushchiy i metalloobrabatyvayushchiy instrument – tekhnika i tekhnologiya yego izgotovleniya i primeneniya, 2011, no. 14, pp. 423–441.
  14. Vicens J., Benjdir M., Nouet G. et al. Cobalt intergranular segregation in WC–Co composites. Journal of Materials Science, 1994, vol. 29, no. 4, pp. 987–994.
  15. Christensen M., Wahnström G., Allibert C., Lay S. Quantitative analysis of WC grain shape in sintered WC–Co cemented carbides. Physical Review Letters, 2005, vol. 94, pp. 66105.
  16. Ortner H., Kolaska H., Ettmayer P. The history of the technological progress of hardmetal. International Journal of Refractory Metals and Hard Materials, 2014, no. 44, pp. 148–159.
  17. State diagrams of double metal systems: a reference book: in 3 vols. / Ed. N.P. Lyakishev. Moscow: Mashinostroyeniye, 1996, vol. 1, 992 p.
  18. Yousfi A. Microstructure development of WC–Co based cemented carbides during creep testing: thesis, PhD. Göteborg, 2016, 43 p.
  19. Egam E., Kusaka T., Machida M., Kobayashi K. Ultra submicron hardmetals for miniature drills. Metal Powder Report, 1989, vol. 44, no. 12, pp. 822–826.
  20. Yamamotoa T., Ikuharaa Y., Sakumab T. High resolution transmission electron microscopy study in VC-doped WC–Co compound. Science and Technology of Advanced Materials, 2000, vol. 1, pp. 97–104.