Veshkin E.A, Semenychev V.V., Postnov V.I., Krasheninnikova E.V. Research of the geometric section for sclerometric furnish sections obtained on the cured binding EDT-69N at different load levels for inductor // Proceedings of VIAM. 2020. No. 3 (87). Ст. 08. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2020-0-3-74-81.

Research of the geometric section for sclerometric furnish sections obtained on the cured binding EDT-69N at different load levels for inductor

Veshkin E.A, Semenychev V.V., Postnov V.I., Krasheninnikova E.V.
Abstract

EDT-69H binder samples cured under various temperature and time conditions were scratched using a laboratory sclerometer over a wide range of indenter loads. The obtained sclerometric grooves were measured andgraphs were plotted for changes in the width and depth of the grooves depending on the load on the samples of composites, cured at different conditions. The geometric shape of the cross-section of the grooves was studied on the transverse sections of plastic samples, the depth of the grooves on the microsections was specified and the microhardness values in the region of deformation of the material from the action of the indenter of the sclerometer were estimated. It has been established that the microhardness value and sclerometric characteristics are very sensitive parameters to the technological modes of curing the binder. The change in the roughness of the front surface of samples with different curing modes was studied and it was shown that an increase in the microhardness of the surface of the sample leads to a decrease in its roughness.

Keywords
composite material, binder EDT-69N, curing modes, sclerometry, microhardness, roughness, microscopic studies.
Reference list
  1. Raskutin A.E. Development strategy of polymer composite materials. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 344–348. DOI: 10.18577/2071-9140-2017-0-S-344-348.
  2. Kablov E.N. Russia in the market of intellectual resources. Ekspert, 2015, no. 28 (951), pp. 48–51.
  3. Grashchenkov D.V. Strategy of development of non-metallic materials, metal composite materials and heat-shielding. Aviacionnye materialy i tehnologii, 2017, No. S, pp. 264–271. DOI: 10.18577/2071-9140-2017-0-S-264-271.
  4. Raskutin A.E. Russian polymer composite materials of new generation, their exploitation and implementation in advanced developed constructions. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 349–367. DOI: 10.18577/2071-9140-2017-0-S-349-367.
  5. Kablov E.N. Composites: today and tomorrow. Metally Evrazii, 2015, no. 1, pp. 36–39.
  6. Mostovoi A.S., Ledenev A.N. Modification of epoxy polymers with nanodispersed silicon. Fizika i khimiya obrabotki materialov, 2017, no. 4, pp. 61–66.
  7. Aristov V.M., Aristova E.P. The effect of structural heterogeneity on the physical properties of partially crystalline polymers. Plasticheskiye massy, 2016, no. 3–4, pp. 15–18. DOI: 10.35164/0554-2901-2016-3-4-15-18.
  8. Platonov A.A., Kogan D.I., Dushin M.I. The manufacture of three-dimensional PCM by the method of impregnation with a film binder. Plasticheskiye massy, 2013, no. 6, pp. 56–61.
  9. Lavrov N.A., Kiyomov Sh.N., Kryzhanovsky V.K. Properties of unfilled epoxy polymers. Plasticheskiye massy, 2019, no. 1–2, pp. 37–39.
  10. Wulf B.K., Romadin K.P. Aviation materials science. Moscow: Mashinostroyeniye, 1967, 391 p.
  11. Tager A.A. Physical chemistry of polymers. Moscow: Nauchnyy mir, 2007, 128 p.
  12. Veshkin E.A., Postnov V.I., Semenychev V.V. Microhardness assessment of samples based on a BST-1210 binder cured in various modes as a testing method. Materialovedeniye, 2018, no. 6, pp. 3–6.
  13. GOST 9450–76. Microhardness measurement by indentation of diamond tips. Moscow: Izd-vo standartov, 1993, 35 p.
  14. Kuritsyna A.D. Application of the microhardness method to determine some properties of polymeric materials. Metody ispytaniya na mikrotverdost. Moscow: Nauka, 1965, pp. 255–260.
  15. Veshkin E.A., Postnov V.I., Semenychev V.V., Krasheninnikova E.V. Anisotropic properties of cured binders. Klei. Germetiki. Tekhnologii, 2018, no. 8, pp. 20–24. DOI: 10.31044/1684-579KH-2018-0-8-20-24.
  16. Veshkin E.A., Postnov V.I., Semenychev V.V., Barannikov A.A. Anisotropy of properties in the high section of fiberglass samples molded by press and autoclave methods. Kompozity i nanostruktury, 2019, vol. 11, no. 2 (42), pp. 51–58.
  17. Gadalov V.N., Bredikhina O.A., Kamyshnikov Yu.P., Skripkina Yu.V., Shkodkin V.I., Kvashnin B.N. Using the sclerometry method for evaluating metals and alloys with electrophysical coatings. Novye materialy i tekhnologii v mashinostroyenii. Bryansk: BGITA, 2006, is. 6, pp. 10–15.
  18. Belous V.A., Lunev V.M., Pavlov V.S., Turchina A.K. Quantitative determination of the adhesion strength of thin metal films to glass. Voprosy atomnoy nauki i tekhniki, 2006, no. 4, pp. 221–223.
  19. Useinov A.S., Kravchuk K.S., Maslenikov I.I. Indentation. Measurement of hardness and crack resistance of coatings. Nanoindustriya, 2013, no. 7 (45), pp. 48–57.
  20. Lvova N.A., Kravchuk K.S., Shirokov I.A. Scratch image processing algorithms in the sclerometry method. Fizika tverdogo tela, 2013, vol. 55, no. 8, pp. 1570–1577.
  21. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.