Tkachuk A.I., Terekhov I.V., Afanaseva E.A. Reactive type flame retardants for epoxy resins. Part 1 // Proceedings of VIAM. 2020. No. 3 (87). Ст. 04. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2020-0-3-41-48.

Reactive type flame retardants for epoxy resins

Part 1
Tkachuk A.I., Terekhov I.V., Afanaseva E.A.
Abstract

The first part of the paper considers the combustion mechanism of polymer materials and the widely used traditional and new promising halogenated and organophosphorus reactive type flame retardants for epoxy resins, which contribute to reducing the combustibility of polymer materials for various purposes without significantly reducing their heat resistance and mechanical properties are given. In particular, a wide range of compounds based on phosphates and derivatives of 9,10-dihydro-9-oxa-10-phosphaphenanthrene-10-oxide are described. The effects of these additives and their mechanism of action are shown.

Keywords
epoxy resins, modification, flame retardants, resistance to burning, functional groups, organophosphorus compounds.
Reference list
  1. Kablov E.N. Chemistry in Aviation Materials Science. Rossiyskiy khimicheskiy zhurnal, 2010, vol. LIV, no. 1, pp. 3–4.
  2. Kablov E.N. Aviation materials science: results and prospects. Vestnik Rossiyskoy akademii nauk, 2002, vol. . 72. No. 1. S. 3–12.
  3. Donetskiy K.I., Karavayev R.Yu., Tsybin A.I., Veshkin E.A., Mikhaldykin E.S. Constructional fiberglass plastic for manufacturing of enclosing sheeting elements. Aviacionnyye materialy i tehnologii, 2017, no. 3 (48), pp. 56–64. DOI: 10.18577/2071-9140-2017-0-3-56-64.
  4. Ivanov N.V., Gurevich Ya.M., Khaskov M.A., Akmeev A.R. Mode studying curing binding VSE-34 and its influences on mechanical properties. Aviacionnyye materialy i tehnologii, 2017, no. 2 (47), pp. 50–55. DOI: 10.18577 / 2071-9140-2017-0-2-50-55.
  5. Aseeva R.M., Zaik G.E. Reduced flammability of polymeric materials. Moscow: Znaniye, 1981, 64 p.
  6. Barbotko S.L. Determination of fire hazard characteristics of glues and self-adhesive materials. Klei. Germetiki. Tekhnologii, 2019, no. 4, pp. 23–29.
  7. Barbotko S. L., Volny O. S., Veshkin E. A., Goncharov V. A. Assessment of fire resistance of materials and structural elements for aircraft. Aviatsionnaya promyshlennost, 2018, no. 2, pp. 63–67.
  8. Lu S.Y., Hamerton I. Recent developments in the chemistry of halogen-free flame retardant polymers. Progress in Polymer Science, 2002, no. 27, pp. 1661–1712.
  9. Terekhov I.V. Functional oligomeric aryloxycyclotriphosphazenes and polymer compositions based on them: thesis, Cand. Sc. (Chem.). Moscow: RKhTU, 2014, 124 s.
  10. Barbotko S.L., Volny O.S., Kirienko O.A., Shurkova E.N. Analysis of the main areas of research carried out by foreign organizations involved in the fire safety of aviation equipment and aerospace materials (review). Problemy bezopasnosti poletov, 2018, no. 2, pp. 3–35.
  11. Terekhov I.V., Shlenskiy V.A., Kurshev E.V., Lonskiy S.L., Dyatlov V.A. Researches of factors affecting the formation of epoxy-containing microcapsules for the self-healing compositions. Aviacionnye materialy i tehnologii, 2018, no. 3 (52), pp. 27–34. DOI: 10.18577/2071-9140-2018-0-3-27-34.
  12. Kablov E.N. Materials and chemical technologies for aircraft engineering. Herald of the Russian Academy of Sciences, 2012, vol. 82, no. 3, p. 158–167.
  13. Petrova A.P., Lukina N.F., Isaev A.Yu. Epoxy adhesives and their use. Klei. Germetiki. Tekhnologii, 2019, no. 10, pp. 37–42.
  14. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  15. Horrocks A.R., Price D. Fire retardant materials. Abington: Woodhead Publishing Limited, 2001, 429 p.
  16. Sheinbaum M., Sheinbaum L., Weizman O. et al. Toughening and enhancing mechanical and thermal properties of adhesives and glass-fiber reinforced epoxy composites by brominated epoxy. Composites. Part B: Engineering, 2019, Vol. 165, P. 604–612.
  17. Batizat D.V., Anikhovskaya L.I., Barbotko S.L., Sakharov A.M., Yarosh A.A. Non-combustible adhesive compositions based on brominated epoxy resins for the manufacture of film adhesives and adhesive prepregs for structural purposes. Klei. Germetiki. Tekhnologii, 2016, no. 2, pp. 9–14.
  18. BarontiniF., Cozzani V., Petarca L. Calorimetric and Kinetic Analysis of the Diglycidyl Ether of the Bisphenol A/Tetrabromobisphenol A Reaction for the Production of Linear Brominated Epoxy Resins. Industrial & Engineering Chemistry Research, 2000, vol. 39, p. 855–863.
  19. Wikoff D., Thompson C., Perry C. et al. Development of toxicity values and exposure estimates for tetrabromobisphenol A: application in a margin of exposure assessment. Journal of Applied Toxicology, 2015, vol. 35 (11), pp. 1292–1308.
  20. Colnot T., Kacew S., Dekant W. Mammalian toxicology and human exposures to the flame retardant 2,2′,6,6′-tetrabromo-4,4′-isopropylidenediphenol (TBBPA): implications for risk assessment. Archives of Toxicology, 2014, vol. 88, pp. 553–573.
  21. Mixture of epoxy resin, epoxide group-containing P compound, P-modified epoxy resin and polyamine: pat. US6201074; filed 10.09.97; publ. 13.03.01.
  22. Flame retardant casting resins as moulding compounds: pat. EP0412425; filed 01.08.90; publ. 11.13.96.
  23. Levchik S.V., Wang C.-S. P-based flame retardants in halogen-free laminates. On Board Technology, 2007, vol. 4, p. 18–20.
  24. Flame retardant epoxy resin composition: pat. US6353080; filed 25.06.98; publ. 05.03.02.
  25. Kornilov K.N. Oligomeric derivatives of dihydric phenols and phosphorus-containing acids: Recent studies. Phosphorus, Sulfur, and Silicon and the Related Elements, 2017, vol. 192, pp. 896–904.
  26. Derouet D., Morvan F,.Brosse J.C. Chemical modification of epoxy resins by dialkyl (or aryl) phosphate: evaluation of fire behavior and thermal stability. Journal of Applied Polymer Science, 1996, vol. 62 (11), pp. 1855–1868.
  27. Jian R., Ai Y., Xia L. et al. Single component phosphamide-based intumescent flame retardant with potential reactivity towards low flammability and smoke epoxy resins. Journal of Hazardous Materials, 2019, vol. 371, pp. 529–539.
  28. Jin S., Qian L., Qiu Y. et al. High-efficiency flame retardant behavior of bi-DOPO compound with hydroxyl group on epoxy resin. Polymer Degradation and Stability, 2019, vol. 166, pp. 344–352.
  29. Yan W., Wang K., Huang W. et al. Synergistic effects of phenethyl-bridged DOPO derivative with Al(OH)3 on flame retardancy for epoxy resins. Polymer-Plastics Technology and Materials. 2019. Available at: http://www.tandfonline.com/doi/full/10.1080/25740881.2019.1695269 (accessed: February 03, 2020). DOI: 10.1080/25740881.2019.1695269.
  30. Ciesielski M., Schäfer A., Döring M. Novel efficient DOPO based flame retardants for PWB relevant epoxy resins with high glass transition temperatures. Polymers for Advanced Technologies, 2008, vol. 19, no. 6, p. 507–515.
  31. Epoxy resin rendered flame retardant by reaction with 9,10-dihydro-9-oxa-10-phosphaphenanthrene-10-oxide: pat. US6291627; filed 10.11.99; publ. 18.09.01.
  32. Wang C.S., Shien J.Y. Phosphorus containing epoxy resin for an electronic application. Journal of Applied Polymer Science, 1999, vol. 73, p. 353–361.
  33. Rakotomalala M., Wagner,S., Döring M. Recent Developments in Halogen Free Flame Retardants for Epoxy Resins for Electrical and Electronic Applications. Materials, 2010, vol. 3, pp. 4300–4327.
  34. Wang C.S., Shieh J.Y. Synthesis and properties of epoxy resins containing 2-(6-oxid-6H-dibenz [c,e] [1,2] oxaphosphorin-6-yl)1,4-benzenediol. Polymer, 1998, vol. 39 (23), pp. 5819–5826.
  35. Cho C.S., Fu S.C., Chen L.W., Wu T.R. Aryl phosphinate anhydride curing for flame retardant epoxy networks. Polymer International, 1998, vol. 47 (20), pp. 203–209.
  36. Seibold S., Schäfer A., Lohstroh W. et al. Phosphorus-containing terephthaldialdehyde adducts – structure determination and their application as flame retardants in epoxy resins. Journal of Applied Polymer Science, 2008, vol. 108 (1), pp. 264–271.
  37. Wang C.S., Lin C.H. Properties and curing kinetics of diglycidyl ether of bisphenol A cured with a phosphorus-containing diamine. Journal of Applied Polymer Science, 1999, vol. 74 (7), pp. 1635–1645.
  38. Xu Y., Chen L., Rao W. et al. Latent curing epoxy system with excellent thermal stability, flame retardance and dielectric property. Chemical Engineering Journal, 2018, vol. 347, p. 223–232.