Babashov V.G., Maximov V.G., Basargin O.V. Technique of determination of high-speed sensitivity of tension deformation at creep // Proceedings of VIAM. 2020. No. 2 (86). Ст. 12. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2020-0-2-109-115.
Technique of determination of high-speed sensitivity of tension deformation at creep
Abstract
In order to study characteristics of material under conditions of creep and superplasticity, a technique is proposed for determining an index of speed sensitivity of steady creep stress. Method is based on analysis of relaxation curves, i.e. dependence of reaction forces of tested samples on time in process of stress relaxation due to creep developing in them. The example shows the use of this technique to determine creep of mullite-based ceramic composite samples.
Keywords
deformation, creep, ceramics, stress relaxation, superplasticity, mullite.
Reference list
- Kablov E.N. Russia needs new generation materials. Redkiye zemli, 2014, no. 3, pp. 8–13.
- Kablov E.N. At the crossroads of science, education and industry. Ekspert, 2015, no. 15 (941), pp. 49–53.
- Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
- Grashchenkov D.V. Strategy of development of non-metallic materials, metal composite materials and heat-shielding. Aviacionnye materialy i tehnologii, 2017, No. S, pp. 264–271. DOI: 10.18577/2071-9140-2017-0-S-264-271.
- Varrik N.M., Ivahnenko Yu.A., Maksimov V.G. Oxide-oxide composites for gas-turbine engines (review). Trudy VIAM, 2014, no. 8, paper no. 03. Available at: http://www.viam-works.ru (accessed: May 30, 2019). DOI: 10.18577/2307-6046-2014-0-8-3-3.
- Basargin O.V., Kolyshev S.G., Shhetanov B.V., Shheglova T.M. Some features of high-temperature bend tests of Nb-based CM specimens. Trudy VIAM, 2015, no. 5, paper no. 11. Available at: http://www.viam-works.ru (accessed: May 30, 2019). DOI: 10.18577/2307-6046-2015-0-5-11-11.
- Grashchenkov D.V., Babashov V.G., Maksimov V.G., Basargin O.V., Kolyshev S.G. Stress relaxation in mullite – ZrO2 ceramics at high temperatures. Steklo i keramika, 2016, no. 6, pp. 12–14.
- Grashchenkov D.V., Lomovskoy V.A., Basargin O.V., Balinova Yu.A., Babashov V.G., Maksimov V.G., Kolyshev S.G. Investigation of dissipative processes by methods of static and dynamic mechanical relaxation in polydispersed ceramics based on mullite hardened with zirconium dioxide. Vestnik RFFI, 2015, no. 1 (85), pp. 47–53.
- Maksimov V.G., Basargin O.V., Shheglova T.M., Nikitina V.Yu. About superplasticity manifestation in unequigranular ceramics mullit-zirconium oxide with size of crystals more than 10 microns. Trudy VIAM, 2013, no. 6, paper no. 04. Available at: http://www.viam-works.ru (accessed: April 30, 2019).
- A method of obtaining a powder of ceramic composite material: pat. 2292320 Rus. Federation, no. 2005125772/03; filed 15.08.05; publ. 27.01.07.
- A method of obtaining a ceramic product: pat. 2486159 Rus. Federation, no. 2011125560/03; filed 22.06.11; publ. 27.12.12.
- Chumachenko E.N., Smirnov O.M., Tsepin M.A. Superplasticity: materials, theory, technology. 2nd ed. Moscow: Librocom, 2009, 320 p.
- Malkin A.Ya., Isaev A.I. Rheology. Concepts, methods, applications. Moscow: Profession, 2007, p. 60.
- Marine I.M., Simonov A.V. Ballistic support for the development and flights of the Fregat interorbital space tug. Vestnik NPO im. S.A. Lavochkina, 2014. no. 1 (22), pp. 10–15.
- Kirenkov V.V., Mikitenko V.G., Sirosh A.N. Determination of actual values of specific impulse of marching engines of upper stages of DM as a typical inverse problem. Kosmicheskaya tekhnika i tekhnologii, 2018, no. 1 (20), pp. 75–81.