Alekseev A.V., Yakimovitch P.V., Kvachonok I.K. Determination of impurities in nickel by ICP-MS // Proceedings of VIAM. 2020. No. 2 (86). Ст. 11. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2020-0-2-101-108.

Determination of impurities in nickel by ICP-MS

Alekseev A.V., Yakimovitch P.V., Kvachonok I.K.
Abstract

The content of impurities of 20 elements (P, Ti, V, Mn, Fe, Co, Cu, Zn, Ga, As, Se, Mo, Ag, Cd, Sn, Sb, Te, Tl, Pb, Bi) in nickel samples by inductively coupled plasma mass spectrometry (ICP-MS). The technique of sample dissolution and its preparation for analysis is given. Spectral interference was eliminated using the equations of mathematical correction, the use of a reaction-collision cell, and also by selecting the plasma power. The correctness of the results is confirmed by analysis of a certified standard sample of nickel alloy. The range of determined concentrations: 0,00002–0,0101% of the mass.

Keywords
inductively coupled plasma mass spectrometry (ICP-MS), nickel alloys, determination of harmful impurities, nickel analysis, microwave sample preparation.
Reference list
  1. Kablov E.N. The strategic directions of development of materials and technologies of their processing for the period to 2030. Aviacionnye materialy i tehnologii, 2012, no. S, pp. 7–17.
  2. Petrushin N.V., Ospennikova O.G., Svetlov I.L. Single-crystal Ni-based superalloys for turbine blades of advanced gas turbine engines. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 72−103. DOI: 10.18577/2071-9140-2017-0-S-72-103.
  3. Kablov E.N., Bondarenko Yu.A., Echin A.B. Development of technology of cast superalloys directional solidification with variable controlled temperature gradient. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 24–38. DOI: 10.18577/2071-9140-2017-0-S-24-38.
  4. Kablov E.N., Bondarenko Yu.A., Echin A.B. Development of technology of cast superalloys directional solidification with variable controlled temperature gradient. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 24–38. DOI: 10.18577/2071-9140-2017-0-S-24-38.
  5. Bazyleva O.A., Ospennikova O.G., Arginbaeva E.G., Letnikova E.Yu., Shestakov A.V. Development trends of nickel-based intermetallic alloys. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 104–115. DOI: 10.18577/2071-9140-2017-0-S-104-115.
  6. Kablov E.N., Chabina E.B., Morozov G.A., Muravskaya N.P. Conformity assessment of new materials using high-level CO and MI. Kompetentnost, 2017, no. 2, pp. 40–46.
  7. State Standard 6689.13–92. Nickel, nickel and copper-nickel alloys. Methods for the determination of arsenic. Moscow: Publishing house of standards, 1992, pp. 1–4.
  8. State Standard 6689.17–92. Nickel, nickel and copper-nickel alloys. Methods for the determination of bismuth. Moscow: Publishing house of standards, 1992, pp. 1–4.
  9. State Standard 13047.16–2002. Nickel. Cobalt. Methods for the determination of cadmium. Moscow: Publishing house of standards, 2002, pp. 1–3.
  10. State Standard 6012–98. Nickel. Methods of chemical atomic emission spectral analysis. Moscow: Publishing house of standards, 1999, pp. 1–4.
  11. ASTM E2594-09. Standard Test Method for Analysis of Nickel Alloys by Inductively Coupled Plasma Atomic Emission Spectrometry (Performance-Based Method). USA, 2014, pp. 1–9.
  12. Hu J., Wang H. Determination of Trace Elements in Super Alloy by ICP-MS. Mikrochimica Acta, 2001, vol. 137, pp. 149–155.
  13. ASTM E2823-17. Standard Test Method for Analysis of Nickel Alloys by Inductively Coupled Plasma Mass Spectrometry (Performance-Based). USA, 2017, pp. 1–8.
  14. Pupyshev A.A., Epova E.N. Spectral interference of polyatomic ions in inductively coupled plasma mass spectrometry. Analitika i kontrol, 2001, vol. 5, no. 4, pp. 335–369.
  15. Leikin A.Yu., Karandashev V.K., Lisovsky S.V., Volkov I.A. The use of a reaction-collision cell to determine impurity elements in rare-earth metals by the ICP-MS method. Zavodskaya laboratoriya. Diagnostika materialov, 2014. vol. 80, no. 5, pp. 6–9.
  16. Stolyankov Yu.V., Ishodzhanova I.V., Antyufeeva N.V. On the question of carbon fiber reinforced plastics (CFRP) test specimen flaws. Trudy VIAM, 2014, no. 10, paper no. 10. Available at: http://viam-works.ru (accessed: October 21, 2019). DOI: 10.18577/2307-6046-2014-0-2-6-6.
  17. Karandashev V.K., Zhernokleeva K.V., Karpov Yu.A. The use of doubly charged ions in the determination of some rare-earth elements in neodymium, samarium, europium and their compounds by inductively coupled plasma mass spectrometry. Zavodskaya laboratoriya. Diagnostika materialov, 2012, vol. 78, no. 12, pp. 5–10.