Rassokhina L.I., Bityutskaya O.N., Gamazina M.V., Kochetkov A.S. Features of the manufacturing technology of highly refractory ceramic molds for castings from γ-TiAl alloys // Proceedings of VIAM. 2020. No. 2 (86). Ст. 04. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2020-0-2-31-40.

Features of the manufacturing technology of highly refractory ceramic molds for castings from γ-TiAl alloys

Rassokhina L.I., Bityutskaya O.N., Gamazina M.V., Kochetkov A.S.
Abstract

The results of research on new modern materials for the manufacture of highly refractory ceramic molds for the production of castings from γ-TiAl alloys are presented. Technological, physical and chemical properties of yttrium oxide binder Sol (Y2O3) and aluminum oxide binder Sol (Al2O3) were tested.

Based on the results of studies of the main properties of yttrium oxide Sol, it was decided to stop further work with the binder as unpromising in terms of determining the possibility of its use for the manufacture of ceramic molds for the manufacture of castings from γ-TiAl alloys at the Leicomelt 5 furnace.

According to the study of the basic properties of water the binder Sol of aluminum oxide were obtained satisfactory results on the strength of the ceramic layer, it sintering during high-temperature firing, therefore it was decided to continue work on the study of the properties of a Sol of aluminum oxide to further develop the technology for the manufacture of ceramic molds for casting of γ-TiAl alloys on the Leicomelt 5 furnace.

Keywords
the binder sol of yttrium oxide, the binder sol of aluminium oxide, water-based binders, highly resistant ceramic molds, titanium intermetallics.
Reference list
  1. Nochovnaya N.A., Bazyleva O.A., Kablov D.E., Panin P.V. Intermetallic alloys based on titanium and nickel. Moscow: VIAM, 2018, 308 p.
  2. Belov V.D., Pavlinich S.P., Fadeev A.V. Intermetallic Ti–Al – tomorrow's material for the Russian engine industry. Liteyshchik Rossii, 2013, no. 11, pp. 12–14.
  3. Kablov E.N., Lukin V.I. Intermetallides based on titanium and nickel for products of new technology. Avtomaticheskaya svarka, 2008, no. 11, pp. 76–82.
  4. Putyrskiy S.V., Yakovlev A.L., Nochovnaya N.A., Krokhina V.A. Research of different heat treatment modes influence on properties of semi-finished products and welded joints from titanium alloy ВТ22М. Aviacionnye materialy i tehnologii, 2019, no. 1 (54), pp. 3–10. DOI: 10.18577/2071-9140-2019-0-1-3-10.
  5. Ilyin A.A., Kolachev B.A., Polkin I.S. Titanium alloys. Composition, structure, properties: reference book. Moscow: VILS; MATI, 2009, 520 p.
  6. Nochovnaya N.A., Panin P.V., Kochetkov A.S., Bokov K.A. Modern heat-resistant alloys based on gamma-aluminide titanium. Metallovedeniye i termicheskaya obrabotka metallov, 2014, no. 7 (709), pp. 23–27.
  7. Kablov E.N., Nochovnaya N.A., Panin P.V., Alekseev E.B., Novak A.V. Study of the structure and properties of heat-resistant alloys based on titanium aluminides with gadolinium microadditives. Materialovedeniye, 2017, no. 3, pp. 3–10.
  8. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  9. Imaev V.M., Imaev R.M., Oleneva T.I. The current state of research and development prospects for intermetallic γ-TiAl alloys technologies. Pisma o materialakh, 2011. T. 1, pp. 25–31.
  10. Andreev A.L., Anoshkin N.F., Bochvar G.A. and others. Titanium alloys. Melting and casting of titanium alloys. Moscow: Metallurgiya, 1994, 368 s.
  11. Kablov D.E., Panin P.V., Shiryaev A.A., Nochovnaya N.A. The use of ADL VAR L200 vacuum-arc furnace for ingots fabrication of high-temperature titanium aluminides base alloys. Aviacionnye materialy i tehnologii, 2014, no. 2, pp. 27–33. DOI: 10.18577/2071-9140-2014-0-2-27-33.
  12. Nochovnaya N.A., Panin P.V., Kochetkov A.S. Problems of obtaining chemically and structurally uniform ingots from heat-resistant alloys based on titanium gamma-aluminide. Tr. konf. «Problemy proizvodstva slitkov i polufabrikatov iz slozhnolegirovannykh i intermetallidnykh titanovykh splavov». Moscow: VIAM, 2015, paper no. 03. 1 CD.
  13. Cast blades of gas turbine engines: alloys, technology, coatings / gen. ed. E.N. Kablov. 2nd ed. Moscow: Nauka, 2006, 632 p.
  14. Kulakov B.A., Dubrovin V.K., Karpinsky A.V., Chesnokov A.A. Technological features of producing castings from titanium alloys. Liteyshchik Rossii, 2014, no. 1, pp. 18–20.
  15. Putyrskij S.V., Arislanov A.A., Artemenko N.I., Yakovlev A.L. Different methods of wear resistance increase of titanium alloys and comparative analysis of their efficiency for VT23M titanium alloy. Aviacionnye materialy i tehnologii, 2018, no. 1, pp. 19–24. DOI: 10.18577/2071-9240-2018-0-1-19-24.
  16. Bratukhin A.G., Bibikov E.L., Glazunov S.G. et al. Production of shaped castings from titanium alloys. Moscow: VILS, 1998, 292 p.
  17. Kulakov B.A., Dubrovin V.K., Pavlinich S.P., Goichenberg Yu.N., Karpinsky A.V. Castings from intermetallic titanium alloys. Liteynoye proizvodstvo, 2012, no. 7, pp. 6–9.