Sidorina A.I., Safronov A.M., Kutsevich K.E., Klimenko O.N. Carbon fabrics for aircraft products // Proceedings of VIAM. 2020. No. 12 (94). Ст. 05. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2020-0-12-47-58.

Carbon fabrics for aircraft products

Sidorina A.I., Safronov A.M., Kutsevich K.E., Klimenko O.N.
Abstract

Current information about the nomenclature of woven reinforcing fillers for composite materials (CM) with a polymer matrix produced at production facilities of FSUE «VIAM», located on the basis of the Voskresensk experimental and technological center for special materials is presented. The main properties of manufactured carbon and hybrid fabrics, promising areas of their application, as well as the main properties of commercially produced and experimental composites based on polymer matrices and woven fillers of FSUE «VIAM» are presented. The directions of further expansion of the range of manufactured woven reinforcing fillers for CM with a polymer matrix are marked.

Keywords
carbon fibers, carbon fabrics, hybrid fabrics, reinforcing fillers, molten binders, adhesive binders, polymer matrices, polymer composite material, prepreg, carbon plastic.
Reference list
  1. Non-crimp fabric composites: Manufacturing, properties and applications. Ed. S.V. Lomov. Cambridge: Woodhead Publishing, 2011, 544 p.
  2. Meola C., Boccardi S., Carlomagno G. Infrared Thermography in the Evaluation of Aerospace Composite Materials. Cambridge: Woodhead Publishing, 2017, 180 p.
  3. Kurnosov A.O., Vavilova M.I., Melnikov D.A. Manufacturing technologies of glass fillers and study of effects of finishing material on physical and mechanical properties of fiberglass plastics. Aviacionnye materialy i tehnologii, 2018, no. 1 (50), pp. 64–70. DOI: 10.18577/2071-9140-2018-0-1-64-70.
  4. Slavin A.V., Startsev O.V. Properties of aircraft glass- and carbonfibers reinforced plastics at the early stage of natural weathering. Trudy VIAM, 2019, No. 8 (80), paper no. 08. Available at: http://www.viam-works.ru (accessed: October 15, 2020). DOI: 10.18577/2307-6046-2018-0-9-71-82.
  5. Timoshkov P.N. Equipment and materials for the technology of automated calculations prepregs. Aviacionnye materialy i tehnologii, 2016, no. 2, pp. 35–39. DOI: 10.18577/2071-9140-2016-0-2-35-39.
  6. Hexcel. Available at: http://www.hexcel.com (accessed: October 15, 2020).
  7. Porcher industries. Available at: http://www.porcher-ind.com (accessed: October 15, 2020).
  8. SGL Carbon. Available at: https://www.sglcarbon.com (accessed: October 15, 2020).
  9. Kablov E.N. New generation materials and digital technologies for their processing. Vestnik Rossiyskoy akademii nauk, 2020, vol. 90, no. 4, pp. 331–334.
  10. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  11. Sidorina A.I. Mechanical properties of polymer composite materials based on Russian high-strength carbon fillers and new generation polymer matrices. Khimicheskiye volokna, 2018, no. 2, pp. 16–19.
  12. Gunyayeva A.G., Sidorina A.I., Kurnosov A.O., Klimenko O.N. Polymeric composite materials of new generation on the basis of binder VSE-1212 and the filling agents alternative to ones of Porcher Ind. and Toho Tenax. Aviacionnye materialy i tehnologii, 2018, no. 3 (52), pp. 18–26. DOI: 10.18577/2071-9140-2018-0-3-18-26.
  13. Sidorina A.I., Safronov A.M. Development of carbon fabrics with high surface density manufacturing technologies. Trudy VIAM, 2020, no. 6–7 (89), paper no. 08. Available at: http://www.viam-works.ru (accessed: October 15, 2020). DOI: 10.18577/2307-6046-2020-0-67-72-80.
  14. Zhidkova O.G., Kashtanov P.P., Tumanin A.N. Features of the design of composite shaping equipment for the manufacture of high-precision dimensionally stable reflector composite antennas of integral design. Konstruktsii iz kompozitsionnykh materialov, 2019, no. 1, pp. 36–44.
  15. Kablov E.N., Gunyaev G.M., Ilchenko S.I. et al. Structural carbon-fiber reinforced plastics with increased conductivity. Aviacionnye materialy i tehnologii, 2004, no. 2, pp. 25–36.