Benarieb I., Romanenko V.A., Klochkova Y.Y., Ovchinnikov V.V., Sbitneva S.V. Application of high-tech aluminum alloy V-1341 of Al–Mg–Si system for pipelines of aircraft products // Proceedings of VIAM. 2020. No. 11 (93). Ст. 03. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2020-0-11-21-30.

Application of high-tech aluminum alloy V-1341 of Al–Mg–Si system for pipelines of aircraft products

Benarieb I., Romanenko V.A., Klochkova Y.Y., Ovchinnikov V.V., Sbitneva S.V.
Abstract

In this paper a task in developing of industrial production of cold-worked thin-walled tubes from high-tech aluminum alloy V-1341 of Al–Mg–Si system was accomplished. Tubes are purposed for application in hydraulic and air conditioning systems of aircraft products. Results of investigation of the structure and mechanical properties of tubes during their technological process and heat treatment are presented. Forming of tubes was performed and construction elements of pipelines were produced, which are identical to pipelines of commercial airplanes.

Keywords
alloy V-1341, Al–Mg–Si system, calcium, cold-worked thin-walled tubes, heat treatment, microstructure, mechanical properties, forming, weldability.
Reference list
  1. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  2. Kablov E.N. Trends and guidelines for innovative development of Russia: Collection of information materials. Moscow: VIAM, 2015, 720 p.
  3. Kablov E.N. Aviation materials science in the XXI century. Prospects and tasks. Vse materialy. Entsiklopedicheskiy spravochnik, 2007, no. 1, pp. 23–47.
  4. Antipov V.V. Prospects for development of aluminium, magnesium and titanium alloys for aerospace engineering. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 186–194. DOI: 10.18577/2071-9140-2017-0-S-186-194.
  5. Antipov V.V., Klochkova Yu.Yu., Romanenko V.A. Modern aluminum and aluminum-lithium alloys. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 195–211. DOI: 10.18577/2071-9140-2017-0-S-195-211.
  6. Benarieb I., Ber L.B., Antipov K.V., Sbitneva S.V. Trends in development of wrought alloys of Al–Mg–Si–(Cu) system. Part 1 (review). Aviacionnye materialy i tehnologii, 2019, no. 3 (56), pp. 14–22. DOI: 10.18577/2071-9140-2019-0-3-14-22.
  7. Kolykhalov D.G., Maryin B.N., Sysoev O.E. Structural and technological analysis of liquid-bone-gas systems of aircraft. Uchenyye zapiski Komsomolskogo-na-Amure gosudarstvennogo tekhnicheskogo universiteta, 2016, vol. 1, no. 3, pp. 4–10.
  8. Kolykhalov D.G., Sysoev O.E., Ivanov I.N. Assessment of the manufacturability of pipeline systems of aircraft at the early stages of design. Trudy MAI, 2016, no. 90, pp. 1–22.
  9. Feoktistov S.I., Maryin B.N., Maryin S.B., Kolykhalov D.G. Theory and practice of manufacturing elements of pipelines for aircraft: textbook. Komsomolsk-on-Amur: KnAGTU, 2013, 88 p.
  10. Maksimenkov V.I., Fedoseev V.I., Shevchenko O.I. Investigation of the technology of manufacturing pipeline systems of medium-range aircraft. Vestnik Voronezhskogo gosudar-stvennogo tekhnicheskogo universiteta, 2011, no. 11-12, pp. 76–79.
  11. Maryin B.N., Kim V.A., Sysoev O.E. et al. Analysis of defects in operating hydro-gas systems of pipelines. Uchenyye zapiski Komsomolskogo-na-Amure gosudarstvennogo tekhnicheskogo universiteta, 2017, vol. 1, no. 1, pp. 79–89.
  12. Maryin B.N., Maryin S.B., Shport R.V. Production of assembly blanks for pipelines. Uchenyye zapiski Komsomolskogo-na-Amure gosudarstvennogo tekhnicheskogo universiteta, 2014, vol. 1, no. 3, pp. 60–63.
  13. Gureeva M.A., Grushko O.E. Aluminum alloys in welded structures of modern vehicles. Mashinostroyeniye i inzhenernoye obrazovanie, 2009, no. 3, pp. 27–41.
  14. Kuznetsov E.A., Sysoev O.E., Kolykhalov D.G. Forecasting the limiting states of high-pressure pipelines of hydro-gas systems at the stage of commissioning. Trudy MAI, 2016, no. 88, pp. 1–17.
  15. Aluminum. Metallurgy, processing and application of aluminum alloys. Eds. A.T. Tumanova, F.I. Kvasova, I.N. Friedlander. Moscow: Metallurgiya, 1972, p. 349.
  16. Altman M.B., Arbuzov Yu.P., Babichev B.I. et al. Aluminum alloys. Application of aluminum-mini-alloys: a reference book. Moscow: Metallurgiya, 1985, pp. 269–275.
  17. Fridlyander I.N., Grushko O.E., Bersenev V.V., Shmeleva L.M., Ivanova L.A. Influence of the type of structure on the properties of cold-rolled sheets from aluminum alloys. Tekhnologiya legkikh splavov, 2002, no. 4, pp. 47–52.
  18. Klochkov G.G., Grushko O.E., Popov V.I., Ovchinnikov V.V., Shamray V.F. Structure, technological properties and weldability of B-1341 (Al–Mg–Si) sheets. Aviacionnye materialy i tehnologii, 2011, no. 1, pp. 3–8.
  19. Mouritz A.P. Aluminum alloys for aircraft structures. Introduction to aerospace materials, Woodhead Publishing Ltd, 2012, pp. 188–216.
  20. Klochkov G.G., Ovchinnikov V.V., Klochkova Yu.Yu., Romanenko V.A. Structure and properties of sheets from workable aluminium alloy V-1341 of Al–Mg–Si system. Trudy VIAM, 2017, no. 12 (60), paper no. 03. Available at: http://www.viam-works.ru (accessed: February 15, 2020). DOI: 10.18577/2307-6046-2017-0-12-3-3.
  21. Klochkov G.G., Klochkova Yu.Yu., Romanenko V.A. Influence of deformation temperature on structure and properties of extruded products of Al–Mg–Si alloy V-1341. Trudy VIAM, 2016, no. 9 (45), paper no. 01. Available at: http://www.viam-works.ru (accessed: February 15, 2020). DOI: 10.18577/2307-6046-2016-0-9-1-1.
  22. Archakova ZN, Balakhontsev G.A., Basova I.G. et al. Structure and properties of semi-finished products from aluminum alloys: a reference book. Moscow: Metallurgiya, 1984, 408 p.
  23. Gureeva M.A., Grushko O.E. Influence of calcium alloying additives on the structure and phase composition of alloy ingots of the Al–Mg–Si system. Zagotovitelnye proizvodstva v mashinostroenii, 2014, no. 8, pp. 36–40.
  24. Kablov E.N., Lukina E.A., Sbitneva S.V., Khokhlatova L.B., Zaitsev D.V. Formation of meta-stable phases during the decomposition of a solid solution in the process of artificial aging of Al-alloys. Tekhnologiya legkikh splavov, 2016, no. 3, pp. 7–17.