Knyazev A. E., Vostrikov A.V. Sieving of powders additive and powder manufacturings (review) // Proceedings of VIAM. 2020. No. 11 (93). Ст. 02. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2020-0-11-11-20.

Sieving of powders additive and powder manufacturings (review)

Knyazev A. E., Vostrikov A.V.
Abstract

Considers the features of powders obtained by various methods, their technological properties in relation to additive and granular manufacturing. The sequence of operations upon receipt of metal powder compositions is presented. The factors affecting the process of vibration sieving of metal powders and granules are described. The features and advantages of vibratory sieving on horizontally arranged circular sieves using ultrasonic cleaning to obtain specified trajectories of motion are shown. Criteria for evaluating the sieving efficiency are given and explanations are given for determining the particle size distribution of powders and granules.

Keywords
powder, granule, vibration sieving, metal-powder composition, additive manufacturing, granular manufacturing, fraction, ultrasonic, technological properties, gas atomization, PREP, sieve.
Reference list
  1. Kablov E.N. VIAM: new generation materials for PD-14. Krylya Rodiny, 2019, no. 7-8, pp. 54–58.
  2. Kablov E.N. Present and future of additive technologies. Metally Evrazii, 2017, no. 1, pp. 2–6.
  3. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  4. Alishin M.I., Knyazev A.E. Production of metal-powder high-purity titanium alloy compositions by induction gas atomization for application in additive manufacturing. Trudy VIAM, 2017, no. 11 (59), paper no. 05. Available at: http://www.viam-works.ru (accessed: June 09, 2020). DOI: 10.18577/2307-6046-2017-0-11-5-5.
  5. Kablov E.N. Powders get rid of unnecessary things. Ekspert, 2014, no. 49 (926), pp. 46–51.
  6. Kablov E.N. Additive technologies – the dominant of the national technological initiative. Intellekt i tekhnologii, 2015, no. 2 (11), pp. 52–55.
  7. Petrov I.M. Main trends of the Russian market of metal powders for additive technologies. Additivnyye tekhnologii, 2019, no. 1, pp. 24–26.
  8. Kudrolli A. Size separation in vibrated granular matter. Reports оn Progress in Physics, 2004, vol. 67, pp. 209–247. DOI: 10.1088/0034-4885/67/3/R01.
  9. Khodkin V.I. Research of processes and creation of technology for pulse-mechanical and vacuum-heat treatment of granules of heat-resistant nickel alloys in the production of blanks for engine building: thesis, Dr. Sc. (Tech.). Moscow: VILS, 1982, 410 p.
  10. Knyazev A.E., Nerush S.V., Alishin M.I., Kuko I.S. Researches of the technological properties of metal-powder compositions of VT6 and VT20 titanium alloys obtained by induction melting and gas atomization. Trudy VIAM, 2017, no. 11 (59), paper no. 06. Available at: http://www.viam-works.ru (accessed: June 09, 2020). DOI: 10.18577/2307-6046-2017-0-11-6-6.
  11. Garibov G.S., Koshelev V.Ya. Influence of the density of filling granules of high-temperature nickel alloys on the shape change of capsules during hot isostatic pressing. Tekhnologiya legkikh splavov, 2013, no. 1, pp. 27–33.
  12. Girshov V.L., Kotov S.A., Tsemenko V.N. Modern technologies in powder metallurgy: textbook. allowance. Saint Petersburg: Publishing house of Polytechnic. University, 2010, pp. 200–214.
  13. Romanov A.I. Study of the regularities of the process of classification by size of fine-dispersed granules of heat-resistant nickel alloys: thesis, Cand. Sc. (Tech.). Moscow: MATI, 2009, 141 p.
  14. Strelov K.K., Mamykin P.S. Refractory technology. Moscow: Metallurgiya, 1978, 376 p.
  15. Koshelev V.Ya., Koshelev V.I. Investigation of the process of obtaining and physicomechanical processing of powders. Tekhnologiya legkikh splavov, 1995, no. 6, pp. 50–53.
  16. Romanov A.I., Kasatkin V.V. Influence of the frontal resistance force on the movement of fine-dispersed granules in a gas environment. New materials and technologies in aviation and rocket-space technology. Korolev: Mashpribor, 2005, pp. 21–25.
  17. Koshelev V.Ya., Golubeva E.A., Durmanova G.Ya. Sieving of granules of heat-resistant nickel alloys on vibrating screens. Metallurgiya granul. Moscow: VILS, 1993, is. 6, pp. 239–246.
  18. Nazarov K.S., Fet Sh. Analysis of modern design solutions that increase the efficiency of vibration classification of difficult-to-use materials. Gornyi informatsionno-analiticheskiy byulleten, 2009, vol. 16, no. 12, pp. 383–393.
  19. Kadel R. Wirtschaftliche Klassierung von siebschwierigem Gut mit ClipClean. Aufbereitungstechnik, 2003, no. 7, pp. 11–16.
  20. Meinel A. Zu den Grundlagen der Klassierung siebschwieriger Materialien. Aufbereitungstechnik, 1999, no. 7, pp. 313–325.
  21. Meinel A. Zur Fein-, Mittel- und Grobkornklassierung auf Wurfsiebmaschinen. Aufbereitungstechnik, 1998, no. 7, pp. 317–326.
  22. Khodkin V.I., Kasatkin V.V., Petrov S.G. Method for evaluating the efficiency of granules sieving. Metallurgiya granul, Moscow: VILS, 1989, is. 5. pp. 208–212.
  23. A method of controlling a sieving machine: pat. 2486968 Rus. Federation; filed 13.02.12; publ. 10.07.13.
  24. Denisov D.G. Separation of polydisperse materials on screens. Vestnik Ivanovskogo gosudarstvennogo energeticheskogo universiteta, 2006, no. 4, pp. 24–27.
  25. Vostrikov A.V., Sukhov D.I. The production of powders by PREP method for addictive manufacturing – current situation and development prospects. Trudy VIAM, 2016, no. 8 (44), paper no. 03. Available at: http://www.viam-works.ru (accessed: June 09, 2020). DOI: 10.18577/2307-6046-2016-0-8-3-3.