Iatsyuk I.V., Dobrynin D.A., Doronin O.N., Pavlova T.V. Methods for removing heat resistant coatings (review) // Proceedings of VIAM. 2020. No. 10 (92). Ст. 10. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2020-0-10-90-96.
Methods for removing heat resistant coatings (review)
Abstract
Provides an overview of coating removal methods widely used in the aviation industry to prepare the surface of used parts for subsequent restoration and repair. The analysis of the main advantages and disadvantages methods of removing coatings is carried out. The results of the application of the promising method of electrolyte-plasma treatment are also presented.
For the first time in the domestic and foreign aviation industry, VIAM has developed a comprehensive technology for repairing spent turbine blades, including removing coatings by electrolytic-plasma surface treatment.
Keywords
removal of coatings, electrolytic plasma treatment, condensation-diffusion coating, ion-plasma coating, heat-resistant coating, turbine blade repair.
Reference list
- Kablov E.N., Muboyadzhyan S.A. Heat resisting and heat-protective coverings for turbine blades of high pressure of perspective GTE. Aviacionnye materialy i tehnologii, 2012, no. S, pp. 60–70.
- Kablov E.N., Muboyadzhyan S.A. Protective coatings for turbine blades of promising gas turbine engines. Gazoturbinnye tekhnologii, 2001, no. 2 (12), pp. 30–32.
- Popova S.V., Muboyadzhyan S.A., Budinovskiy S.A., Dobrynin D.A. The feature of electrolytic plasma etching of heat resistant coatings from parts surface of high-temperature nickel alloys. Trudy VIAM, 2016, no. 2 (38), paper no. 04. Available at: http://www.viam-works.ru (accessed: August 17, 2020). DOI: 10.18577/2307-6046-2016-0-2-4-4.
- Popova S.V., Dobrynin D.A., Muboyadzhyan S.A., Budinovskiy S.A. Removal of heat resisting condensation and diffusion coatings from the surface of GTE blades before and after the operating time. Trudy VIAM, 2017, no. 1 (49), paper no. 04. Available at: http://www.viam-works.ru (accessed: August 17, 2020). DOI: 10.18577/2307-6046-2017-0-1-4-4.
- Dobrynin D.A., Pavlova T.V., Afanasyev-Khodykin A.N., Alekseeva M.S. The use of electrolytic-plasma treatment for repair of GTE blades. Trudy VIAM, 2019, No. 8 (80), paper no. 03. Available at: http://www.viam-works.ru (accessed: August 17, 2020). DOI: 10.18577//2307-6046-2019-0-8-18-26.
- Kablov E.N., Muboyadzhyan S.A., Budinovskij S.A., Lutsenko A.N. Ion-plasma protective coatings for blades of gas turbine engines. Metally, 2007, no. 5, pp. 23–34.
- Muboyadzhyan S.A., Budinovskij S.A. Ion-plasma technology: prospective processes, coatings, equipment. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 39–54. DOI: 10.18577/2071-9140-2017-0-S-39-54.
- Muboyadzhyan S.A., Kablov E.N., Budinovskij S.A. Vacuum and plasma technology of receiving protecting covers from complex-alloyed alloys. Metallovedenie i termicheskaya obrabotka metallov, 1995, no 2, pp. 15–18.
- Method of removing a coating from a substrate: pat. US6905396B1; filed 20.11.03; publ. 14.07.05.
- Process for treating the surface of a component, made from a Ni based superalloy, to be coated: pat. US6440238B1; filed 09.08.99; publ. 27.08.02.
- Method for repairing a thermal barrier coating: pat. US6544346B1; filed 01.07.97; publ. 08.04.03.
- Method of decoating a turbine blade: pat. US6660102B2; filed 27.12.00; publ. 17.10.02.
- Process for applying a protective layer: pat. US7736704B2; filed 15.09.04; publ. 10.08.06.
- Method for selectively removing coatings from metal substrates: pat. US8021491B2; filed 07.12.06; publ. 22.10.09.
- Method for removal of surface layers of metallic coatings: pat. US6036995A; filed 31.01.97; publ. 14.03.00.
- Method for removing aluminide coating from metal substrate and turbine engine part so treated: pat. US7270764B2; filed 09.01.03; publ. 03.11.05.
- Method for cleaning metal parts: pat. US4324594A; filed 02.02.78; publ. 13.04.82.
- Chemical stripping composition and method: pat. US8859479B2; filed 26.08.11; publ. 28.02.13.
- Method of removing heat-resistant coating from parts made of heat-resistant nickel alloys: pat. 2339738C1 Rus. Federation; filed 27.03.07; publ. 27.11.08.
- Method for removing coatings from parts made of heat-resistant alloys: pat. 2200211C2 Rus. Federation; filed 07.03.01; publ. 10.03.03.
- Method for repairing turbine blades of a gas turbine engine: pat. 2367554С2 Rus. Federation; filed 08.11.07; publ. 20.09.09.
- Pogrebnyak A.D., Tyurin Yu.N., Boyko A.G., Zhadkevich M.L., Kalyshkanov M.K., Ruzimov Sh.M. Electrolytic-plasma treatment and coating of metals and alloys // Uspekhi fiziki metallov. 2005, vol. 6, no. 4, pp. 273–344.
- Method for removing coating from a metal substrate: US Pat. 2094546С1 Rus. Federation; filed 03.04.95; publ. 27.10.97.
- Kulikov I.S., Vaschenko S.V., Kamenev A.Ya. Electrolytic-plasma processing of materials. Minsk: Belarusian Science, 2010, 232 p.
- Way of control of extent of removal of covering from details from heat resisting nickel alloys: pat. 2440878С2 Rus. Federation; filed 21.04.09; publ. 27.01.12.
- Way of removal of heat resisting metallic coating: pat. 2228396С1 Rus. Federation; filed 19.09.02; publ. 10.05.04.
- Way of removal of alyuminidny covering on the basis of nickel: pat. 2211261С2 Rus. Federation; filed 12.11.01; publ. 27.08.03.