Barannikov A.A., Postnov V.I., Veshkin E.A, Starostina I.V. Link between the energy characteristics of the surface of fiberglass of the VPS-53К brand and the strength of the adhesive joint based on it // Proceedings of VIAM. 2020. No. 10 (92). Ст. 05. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2020-0-10-40-50.

Link between the energy characteristics of the surface of fiberglass of the VPS-53К brand and the strength of the adhesive joint based on it

Barannikov A.A., Postnov V.I., Veshkin E.A, Starostina I.V.
Abstract

Based on the study of the wetting phenomenon and the theory of adhesion, the surface of fiberglass of the VPS-53K brand was studied before and after its treatment with atmospheric pressure plasma, which is one of the advanced methods of surface preparation for various adhesion processes. Two methods for determining the free energy of a surface are considered – the OUN's, Wendt's, Rabel's, and Kjelbla's method and the extended Fowkes method. The values of the free energy of the surface and its components are obtained using two methods under consideration. The connection between the energy characteristics of the surface of fiberglass of the VPS-53 K brand and the strength of the adhesive joint based on it is established.

Keywords
adhesion, contact angle, free surface energy, work of adhesion, fiberglass, resistance to delamination.
Reference list
  1. Kablov E.N. New generation materials – the basis for innovation, technological leadership and national security of Russia. Intellekt & Tekhnologii, 2016, no. 2, pp. 41–46.
  2. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  3. Podzhivotov N.Yu., Kablov E.N., Antipov V.V., Erasov V.S. et al. Layered metallopolymer materials in aircraft structural elements. Perspektivnyye materialy, 2016, no. 10, pp. 5–19.
  4. Grashchenkov D.V. Strategy of development of non-metallic materials, metal composite materials and heat-shielding. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 264–271. DOI: 10.18577/2071-9140-2017-0-S-264-271.
  5. Kablov E.N. Chemistry in Aviation Materials Science. Rossiyskiy khimicheskiy zhurnal, 2010, vol. LIV, no. 1, pp. 3–4.
  6. Barannikov A.A., Postnov V.I., Veshkin E.A., Strelnikov S.V. On the role of fiberglass surface preparation for gluing. Klei. Germetiki. Tekhnologii, 2019, no. 6, pp. 19–27.
  7. Bogdanova Yu.G. Adhesion and its role in ensuring the strength of polymer composites. Moscow: MSU named after M.V. Lomonosov, 2010, 68 p.
  8. Kraus E. Increasing the strength of adhesive joints of polymer materials by laser and plasma surface treatment: thesis, Cand. Sc. (Tech.). Kazan: KNRTU, 2017, 184 p.
  9. Danchenko Yu.M. Regulation of free surface energy of epoxy polymeric materials using mineral fillers. Polimernyye materialy i tekhnologii, 2017, vol. 3, no. 2, pp. 56–63.
  10. Langer M., Otto D. Methods of investigation of surface characteristics of polymers after plasma treatment. Comparative analysis. Analiz i kontrol: tekhnologii, pribory, resheniya, 2018, no. 2 (39), pp. 2–7.
  11. Williams T.S., Yu H., Hicks R.F. Atmospheric pressure plasma activation of polymers and composites for adhesive bonding: a Critical Review. Reviews of Adhesion and Adhesives, 2013, vol. 1, no. 1, p. 46–87. DOI: 10.7569/RAA.2013.097302.
  12. Serrano J.S. Surface modifications of composite materials by atmospheric pressure plasma treatment: PhD thesis. Madrid: Universidad Rey Juan Carlos, 2011, 302 p. Available at: https://eciencia.urjc.es/bitstream/10115/11379/1/Thesis_June%202011%20JSS-SLU-AUF_v5.pdf (accessed: May 15, 2020).
  13. Gleich H. Zusammenhang zwischen Oberflächenenergie und Adhäsionsvermögen von Polymer werkstoffen am Beispiel von PP und PBT und deren Beeinflussung durch die Niederdruck-Plasmatechnologie: dis. Universtät Duisburg-Essen, 2004.103 p. Available at: https://duepublico2.uni-due.de/servlets/MCRFileNodeServlet/duepublico_derivate_00005593/gleichdiss.pdf (accessed: May 15, 2020).
  14. Rodríguez B.N. Pre-Treatment for adhesive bonding of aerospace composite components: PhM thesis. London: Brunel University, 2016, 133 p. Available at: https://bura.brunel.ac.uk/bitstream/2438/14669/1/FulltextThesis.pdf (accessed: May 15, 2020).
  15. Al-Maliki H.L.R. Adhesive and tribological behavior of cold atmospheric-treated polymer surfaces: PhD Dissertation. Gödöllő: Szent István University, 2018, 115 p. Available at: https://szie.hu/sites/default/files/hayder_lateef_dissertation.pdf (accessed: May 15, 2020).
  16. Lisco F., Shaw A., Wright A. et al. Atmospheric-pressure plasma surface activation for solution processed photovoltaic devices. Solar Energy, 2017, vol. 146, pp. 287–297.
  17. Kostova K.G., Nishimea T.M.C., Castroa A.H.R. et al. Surface modification of polymeric materials by cold atmosphericplasma jet. Applied Surface Science, 2014, vol. 314, p. 367–375.
  18. Akiyama H., Hasegawa K., Sekigawa T., Yamazaki N. Atmospheric pressure plasma treatment for composites bonding. Mitsubishi Heavy Industries Technical Review, 2018, vol. 55, no. 2, pp. 1–5.
  19. Lucchetta G. Experimental analysis of atmospheric plasma treatment and resin optimization for adhesive bonding of carbon fiber/epoxy composites. Available a: http://tesi.cab.unipd.it/48832/1/Tesi_ANTONELLO_Julien.pdf (accessed: May 15, 2020).
  20. Barannikov A.A., Veshkin E.A., Postnov V.I., Semenichev V.V. Structural studies of adhesive joints of VPS-53K fiberglass sheets treated with atmospheric pressure plasma. Klei. Germetiki. Tekhnologii, 2020, no. 3, pp. 27–33. DOI: 10.31044/1813-7008-2020-0-3-27-33.
  21. Postnov V.I., Pletin I.I., Veshkin E.A., I. V. Starostina, S. V. Strelnikov. Technological features of the production of thin-sheet skins of helicopter blades from structural fiberglass VPS-53K. Izvestiya Samarskogo nauchnogo tsentra RAN, 2016, vol. 18, no.4 (3), pp. 186–188.
  22. Dementeva L.A., Serezhenkov A.A., Lukina N.F., Kucevich K.E. Adhesive prepregs and layered materials on their basis. Aviacionnye materialy i tehnologii, 2013, no. 2, pp. 19–21.
  23. Lukina N.F., Dementeva L.A., Petrova A.P., Anihovskaya L.I. Gluing materials in the design of blades of helicopters. Trudy VIAM, 2016, no. 7, paper no. 07. Available at: http://www.viam-works.ru (accessed: May 15, 2020). DOI: 10.18577/2307-6046-2016-0-7-7-7.
  24. Petrova A.P., Lukina N.F., Melnikov D.A., Besednov K.L., Pavlyuk B.F. Research of properties of cured adhesive binders. Trudy VIAM, 2017, no. 10 (58), paper no. 06. Available at: http//www.viam-works.ru (accessed: June 15, 2020). DOI: 10.18577/2307-6046-2017-0-10-6-6.
  25. Operating manual OCA 15EC: Version 1.0; English; Valid as of firmware version 10.27, and SCA software version 4.4.1 Build 1046. Data Physics Instruments GmbH. Available at: https://vdocuments.site/manual-sca20-u.html (accessed: May 05, 2020).
  26. Thomsen F. Practical Contact Angle Measurement (5). Custom – made models: from contact angle to surface free energy: KRUSS Technical Note TN315e, pp. 1–6. Available at: https://warwick.ac.uk/fac/cross_fac/sciencecity/programmes/internal/themes/am2/booking/dropshapeanalyser/practical_contact_angle_measurement_5.pdf (accessed: June 05, 2020).