Kablov E.N., Valueva M.I., Zelenina I.V., Khmelnitskiy V.V., Aleksashin V.M. Carbon plastics based on benzoxazine oligomers – perspective materials // Proceedings of VIAM. 2020. No. 1 (85). Ст. 07. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2020-0-1-68-77.

Carbon plastics based on benzoxazine oligomers – perspective materials

Kablov E.N., Valueva M.I., Zelenina I.V., Khmelnitskiy V.V., Aleksashin V.M.
Abstract

Presents the results of studies of prepregs and carbon plastics, in the manufacture of which oligomeric benzoxazines with different ratios of mono and diamines in the system were used as binders: this class of polymer resins combines the best properties of epoxy and phenol formaldehyde resins. The reaction activity of prepregs was studied, including after long-term storage, and the properties of carbon plastics. An increase in the amount of diamine allows one to increase the glass transition temperature from 151 to 220 °C, which leads to an increase in the heat resistance of the material. CFRPs based on oligomeric benzoxazines have a sufficiently high level of strength properties and retain at least 80% of their mechanical properties at elevated test temperatures; have low water and moisture absorption and are resistant to moisture.

Keywords
benzoxazines, benzoxazine oligomers, prepregs, carbon composites.
Reference list
  1. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  2. Kablov E.N. What to make the future of? Materials of a new generation, technologies for their creation and processing - the basis of innovation. Krylya Rodiny, 2016, no. 5, pp. 8–18.
  3. Kablov E.N., Startsev O.V., Krotov A.S., Kirillov V.N. Climatic aging of composite materials for aviation purposes. III. Significant factors of aging. Deformatsiya i razrusheniye materialov, 2011, no. 1, pp. 34–40.
  4. Kablov E.N., Chursova L.V., Babin A.N., Mukhametov R.R., Panina N.N. Developments of FSUE VIAM in the field of melt binders for polymer composite materials. Polimernyye materialy i tekhnologii, 2016, vol. 2, no. 2, pp. 37–42.
  5. Grashchenkov D.V. Strategy of development of non-metallic materials, metal composite materials and heat-shielding. Aviacionnye materialy i tehnologii, 2017, No. S, pp. 264–271. DOI: 10.18577/2071-9140-2017-0-S-264-271.
  6. Raskutin A.E. Development strategy of polymer composite materials. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 344–348. DOI: 10.18577/2071-9140-2017-0-S-344-348.
  7. Khmelnitsky V.V., Shimkin A.A. Polymeric benzoxazines – a new type of high temperature polymer resins (review). Trudy VIAM, 2019, no. 2 (74), paper no. 05. Available at: http://viam-works.ru (accessed: October 20, 2019). DOI: 10.18577/2307-6046-2019-0-2-43-57.
  8. Ghosh N., Kiskan B., Yagci Y. Polybenzoxazines – new high performance thermosetting resins: synthesis and properties. Progress in Polymer Science, 2007, vol. 32, pp. 1344–1391.
  9. Yagci Y., Kiskan B., Gosh N. Recent advancement on polybenzoxazines – A newly developed high performance thermoset. Journal Polymer Science. Part A: Polymer Chemistry, 2009, vol. 47, pp. 5565–5576.
  10. Kiskan B., Ghosh N., Yagci Y. Polybenzoxazine-based composites as high-performance materials. Polymer International, 2011, vol. 60, pp. 167–177.
  11. Ishida H., Froimowicz P. Advanced and Emerging Polybenzoxazine Science and Technology. Netherlands: Elsevier, 2017. 1126 p.
  12. Melnikov D.A., Khaskov M.A., Guseva M.A., Antyufeeva N.V. To the question of the development of pressing mode for laminated PCMs based on prepregs. Trudy VIAM, 2018, no. 2, paper no. 09. Available at: http://www.viam-works.ru (accessed: October, 2019). DOI: 10.18577/2307-6046-2018-0-2-9-9.
  13. Antyufeeva N.V., Aleksashin V.M. The use of thermal analysis methods to determine the indicators of technological and operational properties of materials. Vse materialy. Entsiklopedicheskiy spravochnik, 2017. No1. S. 55–64.
  14. Aleksashin V.M., Zelenina I.V., Khmelnitsky V.V., Shimkin A.A. Thermoanalytical study of the influence of a carbon filler on the reactivity of oligomers with benzoxazine rings in the main chain. Vse materialy. Entsiklopedicheskiy spravochnik, 2020, no. 3 (publishing).
  15. Kablov E.N., Startsev V.O. Systematical analysis of the climatics influence on mechanical properties of the polymer composite materials based on domestic and foreign sources (review). Aviacionnye materialy i tehnologii, 2018, no. 2 (51), pp. 47–58. DOI: 10.18577/2071-9140-2018-0-2-47-58.
  16. Valevin E.O., Shvedkova A.K., Bukharov S.V. The role of heat and humidity tests in the development of new polymer composite materials. Zavodskaya laboratoriya. Diagnostika materialov, 2016, vol. 82, no. 2, pp. 28–32.
  17. Nikolaev E.V., Kirillov V.N., Skirta A.A., Grashhenkov D.V. Study of moisture transport rules and development of a standard on measurement of the diffusion coefficient and moisture content limit to evaluate mechanical properties of carbon fiber reinforced plastics. Aviacionnye materialy i tehnologii, 2013, no. 3, pp. 44–48.
  18. Valevin E.O., Bukharov S.V., Kirillov V.N., Melekhina M.I., Marakhovsky P.S. The study of moisture resistance of structural fiberglass in laboratory heat and humidity tests. Plasticheskiye massy, 2014, no. 1–2, pp. 26-30.
  19. Rimdusit S., Leingvachiranon C., Tiptipakorn S., Jubsilp C. Thermomechanical characteristics of benzoxazine-urethane copolymers and their carbon fiber-reinforced composites. Journal of Applied Polymer Science, 2009, vol. 113, pp. 3823–3830.