Zakharova L.V. Solid-metal embrittlement of titanium alloy VT20 in contact with silver, zinc and cadmium // Proceedings of VIAM. 2019. No. 9 (81). Ст. 04. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2019-0-9-38-46.

Solid-metal embrittlement of titanium alloy VT20 in contact with silver, zinc and cadmium

Zakharova L.V.
Abstract

On the example of an alloy VT20 the problem of solid-metal embrittlement of titanium alloys in contact with silver, zinc and cadmium in the solid state was considered. The influence of the contact density of the surface of titanium alloy with metals, temperature and duration of tests, as well as the application of external tensile stresses were investigated. Temperature thresholds and incubation periods of cracking of VT20 alloy in contact with the studied metals were determined. Studies of fractures of titanium samples and analysis of the chemical composition of their surface after testing were carried out.

Keywords
solid-metal embrittlement, contact density, contact pressure, local plastic deformation, cracking.
Reference list
  1. Kablov E.N., Grashchenkov D.V., Isayeva N.V., Solntsev S.S., Sevastyanov V.G. Vysokotemperaturnyye konstruktsionnyye kompozitsionnyye materialy na osnove stekla i keramiki dlya perspektivnykh izdeliy aviatsionnoy tekhniki [High-temperature structural composite materials based on glass and ceramics for promising aircraft products] // Steklo i keramika. 2012. №4. S. 7–11.
  2. Kablov E.N. Kompozity: segodnya i zavtra [Composites: today and tomorrow] // Metally Evrazii. 2015. №1. S. 36–39.
  3. Podzhivotov N.Yu., Kablov E.N., Antipov V.V., Erasov V.S., Serebrennikova N.Yu., Abdullin M.R., Limonin M.V. Sloistyye metallopolimernyye materialy v elementakh konstruktsii vozdushnykh sudov [Layered metal-polymer materials in aircraft structural elements] // Perspektivnyye materialy. 2016. №10. S. 5–19.
  4. Raskutin A.E. Rossiiskie polimernye kompozitsionnye materialy novogo pokoleniia, ikh osvoenie i vnedrenie v perspektivnykh razrabatyvaemykh konstruktsiiakh [Russian polymer composite materials of new generation, their exploitation and implementation in advanced developed constructions] // Aviacionnye materialy i tehnologii. 2017. №S. S. 349–367. DOI: 10.18577/2071-9140-2017-0-S-349-367.
  5. Lomberg B.S., Ovsepjan S.V., Bakradze M.M., Letnikov M.N., Mazalov I.S. Primenenie novyh deformiruemyh nikelevyh splavov dlja perspektivnyh gazoturbinnyh dvigatelej [The application of new wrought nickel alloys for advanced gas turbine engines] // Aviacionnye materialy i tehnologii. 2017. №S. S. 116–129. DOI: 10.18577/2071-9140-2017-0-S-116-129.
  6. Gromov V.I., Voznesenskaya N.M., Pokrovskaya N.G., Tonysheva O.A. Vysokoprochnye konstrukcionnye i korrozionnostojkie stali FGUP «VIAM» dlya izdelij aviacionnoj tehniki [High-strength constructional and corrosion-resistant steels developed by VIAM for aviation engineering] // Aviacionnye materialy i tehnologii. 2017. №S. S. 159–174. DOI: 10.18577/2071-9140-2017-0-S-159-174.
  7. Antipov V.V. Perspektivy razvitiya alyuminievyh, magnievyh i titanovyh splavov dlya izdelij aviacionno-kosmicheskoj tehniki [Prospects for development of aluminium, magnesium and titanium alloys for aerospace engineering] // Aviacionnye materialy i tehnologii. 2017. №S. S. 186–194. DOI: 10.18577/2107-9140-2017-0-S-186-194.
  8. Duyunova V.A., Volkova E.F., Uridiya Z.P., Trapeznikov A.V. Dinamika razvitiya magnievyh i litejnyh alyuminievyh splavov [Dynamics of the development of magnesium and cast aluminum alloys] // Aviacionnye materialy i tehnologii. 2017. №S. S. 225–241. DOI: 10.18577/2071-9140-2017-0-S-225-241.
  9. Sibileva S.V., Karimova S.A. Obrabotka poverhnosti titanovyh splavov s celyu obespecheniya adgezionnyh svojstv [Surface treatment of titanium alloys to provide adhesion properties] // Aviacionnye materialy i tehnologii. 2013. №S2. S. 25–35.
  10. Zakharova L., Botanogov A. Podgotovka poverkhnosti titanovykh splavov VT6ch, VT20 i OT4 dlya povysheniya adgezii lakokrasochnykh pokrytiy [Surface preparation of titanium alloys VT6ch, VT20 and OT4 to increase the adhesion of coatings] // Promyshlennaya okraska. 2013. №4. S. 15–19.
  11. Zakharova L.V., Karimova S.A. Khimicheskaya obrabotka poverkhnosti titanovykh splavov dlya povysheniya ikh adgezionnoy sposobnosti k lakokrasochnym pokrytiyam [Chemical surface treatment of titanium alloys to increase their adhesion to paint coatings] // Fizika i khimiya obrabotki materialov. 2014. №2. S. 33–37.
  12. Molitor P., Barron V., Young T. Surface treatment of titanium for adhesive bonding to polymer composites: a review // International Journal of Adhesion & Adhesives. 2001. Vol. 21. P. 129−136.
  13. Venables J.D. Review: adhesion and durability of metal–polymer bonds // Journal of Materials Science. 1984. Vol. 19. P. 2431–2453.
  14. Mertens T., Gammel F.J., Kolb M. et al. Investigation of surface pre-treatments for the structural bonding of titanium // International Journal of Adhesion & Adhesives. 2012. Vol. 34. P. 46–54.
  15. Sibileva S.V., Knyazev A.V., Leshko S.S., Chesnokov D.V. Plazmennoye elektroliticheskoye oksidirovaniye titanovykh splavov s tselyu zashchity ot kontaktnoy korrozii sopryazhennykh elementov iz alyuminiyevykh splavov [Plasma electrolytic oxidation of titanium alloys to protect contact corrosion of conjugated elements from aluminum alloys] // Korroziya: materialy, zashchita. 2019. №6. S. 1–6. DOI: 10.31044/1813-7016-2019-0-6-1-6.
  16. Chechulin B.B., Khesin Yu.D. Tsiklicheskaya i korrozionnaya prochnost titanovykh splavov [Cyclic and corrosion resistance of titanium alloys]. M.: Metallurgiya, 1987. 208 s.
  17. Kolachev B.A., Livanov V.A., Bukhanova A.A. Mekhanicheskiye svoystva titana i yego splavov [Mechanical properties of titanium and its alloys]. M.: Metallurgiya, 1974. 544 s.
  18. Zakharova L.V. Vliyanie kisloroda vozdukha i tolshchiny solevykh otlozheniy na korrozionnoe rastreskivanie titanovykh splavov pri vysokikh temperaturakh v kontakte s NaCl [Influence of oxygen of air and thickness of salt deposits on corrosion cracking of titanium alloys at high temperatures in contact with NaCl] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2014. №10. St. 12. Available at: http://www.viam-works.ru (accessed: August 13, 2019). DOI: 10.18577/2307-6046-2014-0-10-12-12.
  19. Zakharova L.V. Vliyanie khimicheskogo sostava, termicheskoj obrabotki i struktury na stojkost' titanovykh splavov k rastreskivaniyu ot goryachesolevoj korrozii [Influence of chemical composition, thermal treatment and structure on cracking sensitivity of titanium alloys to hot-salt stress corrosion] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2016. №9 (45). St. 11. Available at: http://www.viam-works.ru (accessed: August 13, 2019). DOI: 10.18577/2307-6046-2016-0-9-11-11.
  20. Zakharova L.V. Anodno-oksidnoe pokrytie – zashhita titanovyh splavov ot goryachesolevoj korrozii [Anodic oxide coating – protection of titanium alloys against hot salt corrosion] //Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2015. №10. St. 02. Available at: http://www.viam-works.ru (accessed: August 13, 2019). DOI: 10.18577/2307-6046-2015-0-10-2-2.
  21. Moroz L.S., Chechulin B.B. Vodorodnaya khrupkost metallov [Hydrogen fragility of metals]. M.: Metallurgiya, 1967. 256 s.
  22. Kolachev B.A. Vodorodnaya khrupkost tsvetnykh metallov [Hydrogen fragility of non-ferrous metals]. M.: Metallurgiya, 1966. 256 s.
  23. Gordon P. Metal-induced embrittlement of metals – an evaluation of embrittler transport mechanisms // Metallurgical Transactions A. 1978. Vol. 9A. P. 267–273. DOI: 10.1007/BF02646710.
  24. Lynch S.P. Metal-induced embrittlement of materials // Materials Characterization. 1992. Vol. 28. No. 3. P. 279–289. DOI: 10.1016/1044-5803(92)90017-c.
  25. Fager D.N., Spurr W.F. Solid cadmium embrittlement: titanium alloys // Corrosion. 1970. Vol. 26. No. 10. P. 409–419.
  26. Stoltz R.E., Stulen R.H. Solid metal embrittlement of Ti–6Al–6V–2Sn by cadmium, silver and gold // Corrosion. 1979. Vol. 35. No. 4. P. 165–169. DOI: 10.5006/0010-9312-35.4.165.