Melnikov A.A., Schur P.A. Transparent conductive antireflective coatings based on ITO, SiO2, TiO2 // Proceedings of VIAM. 2019. No. 8 (80). Ст. 07. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2019-0-8-56-66.

Transparent conductive antireflective coatings based on ITO, SiO2, TiO2

Melnikov A.A., Schur P.A.
Abstract

Transparent conductive coatings are widely used nowadays. In this work simultaneously conductive and antireflective coatings produced within one stack of optical coating are proposed. Production method allows to receive the coatings with high uniformity on large size substrates (up to 350×500 mm). Transmittance T>93%, reflectance R<1% and surface resistance Rpov<20 Om/□ for silicate glasses with such coatings. Demonstration of electrical heating of the coatings is showed.

Keywords
optical coatings, antireflective coatings, conductive coatings, enlightening coatings, electrical heating.
Reference list
  1. Kablov E.N. Materialy novogo pokoleniya – osnova innovatsiy, tekhnologicheskogo liderstva i natsionalnoy bezopasnosti Rossii [Materials of a new generation – the basis of innovation, technological leadership and national security of Russia] // Intellekt i tekhnologii. 2016. №2 (14). S. 16–21.
  2. Kablov E.N. Iz chego sdelat budushcheye? Materialy novogo pokoleniya, tekhnologii ikh sozdaniya i pererabotki – osnova innovatsiy [What to make the future of? Materials of a new generation, technologies for their creation and processing – the basis of innovation ] // Krylya Rodiny. 2016. №5. S. 8–18.
  3. Kablov E.N. Nastoyashcheye i budushcheye additivnykh tekhnologiy [Present and future of additive technologies] // Metally Evrazii. 2017. №1. S. 2–6.
  4. Bogatov V.A., Krynin A.G., Shchur P.A. Vliyaniye velichiny natekaniya v vakuumnoy kamere na parametry reaktivnogo magnetronnogo raspyleniya i svoystva pokrytiya oksida titana [Influence of the leakage value in the vacuum chamber on the parameters of reactive magnetron discharge and properties of titanium oxide coatings] // Aviaсionnye materialy i tehnologii. 2019. №1 (54). S. 17–22. DOI: 10.18577/2071-9140-2019-0-1-17-22.
  5. Kuzmichev A.I. Magnetronnyye raspylitelnyye sistemy. Kn. 1. Vvedeniye v fiziku i tekhniku magnetronnogo raspyleniya [Magnetron Spray Systems. Book 1. Introduction to the physics and technology of magnetron sputtering]. Kiev: Avers, 2008. 244 s.
  6. Jeong S.H., Lee J.W., Lee S.B., Boo J.H. Deposition of aluminum-doped zincoxide films by RF magnetron sputtering and study of their structural, electrical and optical properties // Thin Solid Films. 2003. Vol. 435. P. 78–82.
  7. Iyevlev V.M., Kushchev S.B., Latyshev A.N. i dr. Spektry pogloshcheniya tonkikh plenok TiO2, sintezirovannykh reaktivnym vysokochastotnym magnetronnym raspyleniyem titana [Absorption spectra of thin TiO2 films synthesized by reactive high-frequency magnetron sputtering of titanium] // Fizika i tekhnika poluprovodnikov. 2014. T. 48. №7. S. 875–884.
  8. Ellmer K., Welzel T. Reactive magnetron sputtering of transparent conductive oxide thin films: Role of energetic particle (ion) bombardment // Journal of Materials Research. 2012. Vol. 27. No. 5. P. 765–779.
  9. Elinson V.M., Shchur P.A., Kirillov D.V. et al. Study of the Mechanical Characteristics of Single-Layer and Multilayer Nanostructures Based on Carbon and Fluorocarbon Coatings // Pleiades Publishing, Journal of Surface Investigation: X-ray, Synchrotron and Neutron Techniques. 2018. Vol. 12. No. 2. P. 342–345.
  10. Zhanga K., Wena M., Chengb G. et al. Reactive magnetron sputtering deposition and characterization of niobium carbide films // Vacuum. 2014. Vol. 99. P. 233–241.
  11. Komlev A.E., Shapovalov V.I., Shutova N.S. Magnetronnyy razryad v srede argona i kisloroda pri osazhdenii plenki oksida titana [Magnetron discharge in an argon and oxygen medium during deposition of a titanium oxide film] // Zhurnal tekhnicheskoy fiziki. 2012. T. 82. №7. S. 134–136.
  12. Navabpoura P., Ostovarpourb S., Hampshirea J. et al. The effect of process parameters on the structure, photocatalytic and self-cleaning properties of TiO2 and Ag-TiO2 coatings deposited using reactive magnetron sputtering // Thin Solid Films. 2014. Vol. 571. Part 1. P. 75–83.
  13. Leóna J.J.D., Garretta M.P., Zhanga J. et al. Aluminum titanium oxide alloys: Deposition of amorphous, transparent, corrosion-resistant films by pulsed DC reactive magnetron sputtering with RF substrate bias // Materials Science in Semiconductor Processing. 2015. Vol. 36. P. 96–102.
  14. Stana G.E., Boteaa M., Bonia G.A. et al. Electric and pyroelectric properties of AlN thin films deposited by reactive magnetron sputtering on Si substrate // Applied Surface Science. 2015. Vol. 353. P. 1195–1202.
  15. Fakhouri H., Pulpytel J., Smith W. et al. Control of the visible and UV light water splitting and photocatalysis of nitrogen doped TiO2 thin films deposited by reactive magnetron sputtering // Applied Catalysis B: Environmental. 2014. Vol. 144. P. 12–21.
  16. Juškevičius K., Audronis M., Subačius A. et al. High-rate reactive magnetron sputtering of zirconia films for laser optics applications // Applied Physics A. 2014. Vol. 116. No. 3. P. 1229–1240.
  17. Solovan M.N., Brus V.V., Maryanchuk P.D. i dr. Kineticheskiye svoystva tonkikh plenok TiN, poluchennykh metodom reaktivnogo magnetronnogo raspyleniya [Kinetic properties of thin TiN films obtained by reactive magnetron sputtering] // Fizika tverdogo tela. 2013. T. 55. №11. S. 2123–2127.
  18. Bogatov V.A., Krynin A.G., Popkov O.V., Khokhlov Yг.A. Vliyaniye dvukhosnoy deformatsii na svoystva prozrachnogo elektroprovodyashchego pokrytiya, osazhdennogo na PETF plenku metodom reaktivnogo magnetronnogo raspyleniya [Influence of biaxial strain on the properties of the transparent conductive coating deposited on PET film by reactive magnetron sputtering] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2016. №1 (37). St. 06. Available at: http://www.viam-works.ru (accessed: May 25, 2019). DOI: 10.18577/2307-6046-2016-0-1-42-49.
  19. Gorjanca T.C., Leonga D., Py C., Rotha D. Room temperature deposition of ITO using r.f. magnetron sputtering // Thin Solid Films. 2002. Vol. 413. P. 181–185.
  20. Khokhlov Yu.A., Bogatov V.A, Krynin A.G. Vliyanie raspredeleniya magnitnogo polya na svojstva ITO pokrytiya, poluchaemogo na polimernoj plenke metodom reaktivnogo magnetronnogo osazhdeniya [An influence of the magnetic field distribution on properties of ITO coating deposited on a polymer film by reactive magnetron sputtering method] // Trudy VIAM : electron. nauch.-tenhich. zhurn. 2014. №12. St. 11. Available at: http://viam-works.ru (accessed: May 25, 2019). DOI: 10.18577/2307-6046-2014-0-12-11-11.
  21. Khokhlov Yu.A., Bogatov V.A., Berezin N.M., Krynin A.G. Reaktivnoye magnetronnoye osazhdeniye ITO pokrytiya na polimernuyu plenku s primeneniyem sektsionirovannoy sistemy napuska gazov [Reactive magnetron deposition of ITO coating on the polymer film using a sectionalized gas feed system] // Trudy VIAM: elektron. nauch.-tekhnich. zhurn. 2015. №5. St. 07. Available at: http://www.viam-works.ru (accessed: May 25, 2019). DOI: 10.18577/2307-6046-2015-0-5-7-7.