Morgunov R.B., Koplak O.V., Talantsev A.D., Korolev D.V., Piskorsky V.P., Valeev R.A. The phenomenology of the magnetic hysteresis loops in multilayer microwires α-Fe/DyPrFeCoB // Proceedings of VIAM. 2019. No. 7 (79). Ст. 08. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2019-0-7-67-75.

The phenomenology of the magnetic hysteresis loops in multilayer microwires α-Fe/DyPrFeCoB

Morgunov R.B., Koplak O.V., Talantsev A.D., Korolev D.V., Piskorsky V.P., Valeev R.A.
Abstract

The shapes of the magnetic hysteresis loops recorded with a Kerr microscope at different points of the α-Fe/DyPrFeCoB microwire were analyzed. Depending on the distance from the ends of the microwire, where the demagnetization field makes a significant contribution to the magnetization, hysteresis loops of various forms were obtained. The micro-wire fragments that are most significant for practical use demonstrate a rectangular hysteresis loop with exchange bias, as well as a hysteresis loop with 4 equilibrium levels of magnetization like a spin-valve device. These data indicate a high practical potential of the obtained microwires for the manufacture of magnetic field, mechanical stress and temperature sensors from them.

Keywords
multilayered microwires, ferromagnetic amorphous alloys, magnetostriction, exchange bias.
Reference list
  1. Kablov E.N., Piskorskiy V.P., Burkhanov G.S., Valeyev R.A. i dr. Termostabilnye koltsevye magnity s radialnoy teksturoy na osnove Nd(Pr)–Dy–Fe–Co–B [Thermally stable ring magnets with a radial texture based on Nd (Pr)–Dy–Fe–Co–B] // Fizika i khimiya obrabotki materialov. 2011. T. 3. C. 43–47.
  2. Kablov E.N., Ospennikova O.G., Rezchikova I.I., Piskorskij V.P., Valeev R.A., Korolev D.V. Zavisimost svojstv spechennyh materialov sistemy Nd–Dy–Fe–Co–B ot tehnologicheskih parametrov [Properties dependence of the Nd–Dy–Fe–Co–B sintered materials on technological parameters] // Aviacionnye materialy i tehnologii. 2015. №S2 (39). S. 24–29. DOI: 10.18577/2071-9140-2015-0-S2-24-29.
  3. Kablov E.N., Ospennikova O.G., Korolev D.V., Piskorskij V.P., Valeev R.A., Rezchikova I.I. Mehanizm vliyaniya soderzhaniya bora i termoobrabotki na svojstva magnitov sistemy Nd–Fe–Al–Ti–B [Influence mechanisms of boron content and heat treatment on the properties of Nd–Fe–Al–Ti–B magnets] // Aviacionnye materialy i tehnologii. 2015. №S2 (39). S. 30–34. DOI: 10.18577/2071-9140-2015-0-S2-30-34.
  4. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  5. Koplak O.V., Gornakov V.S., Kabanov Yu.P., Kunitsyna E.I., Shashkov I.V. Temperaturnaya zavisimost obmennoy anizotropii ferrimagnitnoy plenki GdFeCo, svyazannoy s antiferromagnetikom IrMn [Temperature dependence of the exchange anisotropy of the GdFeCo ferrimagnetic film associated with the antiferromagnet IrMn] // Pisma v zhurnal eksperimentalnoy i teoreticheskoy fiziki. 2019. T. 109. Vyp. 11. S. 753–760.
  6. Fache T., Tarazona H.S., Lu Y. et al. Nonmonotonic aftereffect measurements in perpendicular synthetic ferrimagnets // Physical Review B. 2018. Vol. 98. P. 064410–064418.
  7. Morgunov R., Lu Y., Lavanant M. et al. Magnetic aftereffects in CoFeB/Ta/CoFeB spin valves of large area // Physical Review B. 2017. Vol. 96 (5). P. 054421.
  8. Knobel M., Sampaio L.C., Sinnecker E.H.C.P. et al. Dipolar magnetic interactions among magnetic microwires // Journal of Magnetism and Magnetic Materials. 2002. Vol. 249. P. 60–72.
  9. Piskorskiy V.P., Korolev D.V., Valeyev R.A., Morgunov R.B., Kunitsyna E.I. Fizika i inzheneriya postoyannykh magnitov: ucheb. posobie / pod obshch. red. E.N. Kablova [Physics and engineering of permanent magnets: tutorial / gen. ed. E.N. Kablov]. M.: VIAM, 2018. 360 s.
  10. Peng H., Qin F., Phan M. Ferromagnetic Microwire Composites From Sensors to Microwave Applications // Engineering Materials and Processes. Springer, 2016. 240 p.
  11. Draganová K., Blažek J., Praslička D., Kmec F. Possible applications of magnetic microwires in aviation // Journal of Fatigue of Aircraft Structures. 2013. Vol. 1. P. 12–17.
  12. Panina L., Ipatov M., Zhukova V. et al. Tuneable Composites Containing Magnetic Microwires // Metal, Ceramic and Polymeric Composites for Various Uses. 2011. P. 431–461.
  13. Evstigneeva S., Morchenko A., Trukhanov A. Structural and magnetic anisotropy of directionally – crystallized ferromagnetic microwires // EPJ Web of Conferences. 2018. Vol. 185. P. 04022.
  14. Baranov S.A. Cast Amorphous Magnetic Microwires for Medical Applications // Advanced in Biotechnology and Microbiology. 2018. Vol. 8 (3). P. 555736.
  15. Szary P., Luciu I., Duday D. et al. Synthesis and magnetic properties of Ta/NdFeB-based composite microwires // Journal of Applied Physics. 2015. Vol. 117. P. 17D134.