Starostina I.V., Petrova A.P., Shevchenko Yu.N., Shishimirov M.V. Control thermoplastic binding for PCM (review) // Proceedings of VIAM. 2019. No. 4 (76). Ст. 11. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2019-0-4-99-107.

Control thermoplastic binding for PCM (review)

Starostina I.V., Petrova A.P., Shevchenko Yu.N., Shishimirov M.V.
Abstract

Тhe description of test methods thermoflexible binding, used as a part of polymeric composite materials, – density, flowability indicator melt, water absorptions, the adhesive durability, the impact strength, durability is provided at stretching, softening temperature, fire safety characteristics, including combustibility, a smoke education, an oxygen index, thermal emission is provided. Comparison of properties thermoflexible and thermosetting binding is given, advantages of refining technology thermoflexible binding before thermosetting binding are shown.

Keywords
thermoflexible binding, polysulphone, polyetheretherketon, melting temperature, flowability melt, molecular weight, density, softening temperature, fire safety, combustibility.
Reference list
  1. Bejder E.Ya., Petrova G.N. Termoplastichnye svyazuyushhie dlya polimernyh kompozicionnyh materialov [The thermoplastic binder for polymeric composite materials] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2015. №11. St. 05. Available at: http://viam-works.ru (accessed: December 17, 2018). DOI: 10.18577/2307-6046-2015-0-11-5-5.
  2. Petrova A.P., Mukhametov R.R., Shishimirov M.V., Pavlyuk B.Ph., Starostina I.V. Metody ispytaniy i issledovaniy termoreaktivnykh svyazuyushchikh dlya polimernykh kompozitsionnykh materialov (obzor) [Test methods and researches thermosetting binding for polymeric composite materials (review)] // Trudy VIAM: elektron. nauch.-tekhnich. zhurnal. 2018. №12 (72). St. 07. Available at: http://viam-works.ru (accessed: December 17, 2018). DOI: 10.18577/2307-6046-2018-0-12-62-70.
  3. Petrova G.N., Larionov S.A., Platonov M.M., Perfilova D.N. Termoplastichnye materialy novogo pokoleniya dlya aviacii [Thermoplastic materials of new generation for aviation] // Aviacionnye materialy i tehnologii 2017. №S. S. 420–436. DOI: 10.18577/2071-9140-2017-0-S-420-436.
  4. Kondrashov S.V., Shashkeev K.A., Petrova G.N., Mekalina I.V. Polimernye kompozicionnye materialy konstrukcionnogo naznacheniya s funkcionalnymi svojstvami [Constructional polymer composites with functional properties] // Aviacionnye materialy i tehnologii. 2017. №S. S. 405–419. DOI: 10.18577/2071-9140-2017-0-S-405-419.
  5. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  6. Kablov E.N. Materialy novogo pokoleniya [New generation materials] // Zashchita i bezopasnost. 2014. №4. S. 28–29.
  7. Kablov E.N. Iz chego sdelat budushcheye? Materialy novogo pokoleniya, tekhnologii ikh sozdaniya i pererabotki – osnova innovatsiy [What to make the future from? Materials of the new generation, technologies of their creation and processing – the basis of innovation] // Krylya Rodiny. 2016. №5. S. 8–18.
  8. Sorokin A.E., Petrova G.N., Beyder E.Ya., Perfilova D.N. Sloistyye ugleplastiki na termoplastichnoy matritse novogo pokoleniya [Layered carbon plastic on a thermoplastic matrix of a new generation] // Vse materialy. Entsiklopedicheskiy spravochnik. 2017. №9. S. 10–17.
  9. Babin A.N., Petrova A.P. Metody ispytaniy i issledovaniy osnovnykh svoystv polimernykh svyazuyushchikh dlya konstruktsionnykh PKM [Test methods and studies of the basic properties of polymeric binders for structural PCM] // Vse materialy. Entsiklopedicheskiy spravochnik. 2016. №3. S. 52–59.
  10. Grelmann V., Zaydler S. Ispytaniya plastmass [Tests of plastics]. SPb.: Professiya, 2010. 720 s.
  11. Nikolayev E.V., Lutsenko A.N., Barbotko S.L., Pavlov M.R., Abramov D.V. Kompleksnyy metodicheskiy podkhod k opredeleniyu sokhranyayemosti svoystv polimernogo svyazuyushchego i polimernykh kompozitsionnykh materialov na ego osnove pri vozdeystvii klimaticheskikh i ekspluatatsionnykh faktorov [Comprehensive methodical approach to determining the persistence properties of polymer binder and polymer composites based on it under the influence of climatic and operational factors] // Fundamentalnyye issledovaniya i posledniye dostizheniya v oblasti zashchity ot korrozii, stareniya i biopovrezhdeniy materialov i slozhnykh tekhnicheskikh sistem v razlichnykh klimaticheskikh usloviyakh. M.: VIAM, 2016. S. 13.
  12. Barbotko S.L. Razvitie metodov ocenki pozharobezopasnosti materialov aviacionnogo naznacheniya [Development of the fire safety test methods for aviation materials] // Aviacionnye materialy i tehnologii. 2017. №S. S. 516–526. DOI: 10.18577/2071-9140-2017-0-S-516-526.
  13. Petrova A.P., Donskoy A.A. Kleyashchiye materialy. Germetiki [Adhesive materials]. SPb.: Professional, 2008. 589 s.
  14. Deyev I.S., Kobets L.P. Issledovaniye mikrostruktury i osobennostey razrusheniya epoksidnykh matrits [Study of the microstructure and features of the destruction of epoxy matrices] // Klei. Germetiki. Tekhnologii. 2013. №5. S. 19–27.
  15. Barbotko S.L., Volnyy O.S., Kiriyenko O.A., Shurkova E.N. Osobennosti ispytaniy aviatsionnykh materialov na pozharoopasnost. Chast 1. Ispytaniye na goryuchest. Vliyaniye tolshchiny obraztsa na registriruyemyye kharakteristiki [Peculiarities of fire hazard testing of aviation materials. Part 1. Flammability test. The influence of the sample thickness on the recorded characteristics] // Pozharovzryvobezopasnost'. 2015. T. 24. №1. S. 40–48.
  16. Petrova G.N., Beyder E.Ya., Starostina I.V. Lityevyye termoplasty dlya izdeliy aviakosmicheskoy tekhniki [Molded thermoplastics for aerospace products] // Vse materialy. Entsiklopedicheskiy spravochnik. 2016. №7. S. 21–28.
  17. Kotomin S.V., Barankova T.I., Gorbunova I.Yu., Filippova T.N. Polucheniye i svoystva mikroplastikov s polisulfonom i montmorillonitom. II. Prochnost i adgeziya mikroplastikov s polisulfonovoy i kompozitnoy matritsey [Preparation and properties of microplastics with polysulfone and montmorillonite. II. Strength and adhesion of microplastics with polysulfone and composite matrix] // Vse materialy. Entsiklopedicheskiy spravochnik. 2016. №3. S. 6–12.