Ivanov M.S., Veshkin E.A, Satdinov R.A., Donskih I.N. New domestic coated textile material for flexible air conditioning ducts of flight vehicles // Proceedings of VIAM. 2019. No. 4 (76). Ст. 07. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2019-0-4-57-66.

New domestic coated textile material for flexible air conditioning ducts of flight vehicles

Ivanov M.S., Veshkin E.A, Satdinov R.A., Donskih I.N.
Abstract

The analysis of information sources in area of the materials applied to manufacturing of flexible air conditioning ducts of flight vehicles is carried out. Requirements are as a result formulated and the new domestic coated textile material is developed for manufacturing of flexible air conditioning ducts of flight vehicles of the VRT-12 brand on the basis of E1-100 fiber glass textile with bilateral fluoropolymer covering. Research of its properties is conducted. The material has the weight of 1 m2 no more than 275 g, meets the requirements AP-25 of flammability, maintains excess pressure of 0,01 MPa and can be maintained in the range of temperatures from -60 to +80°С.

Keywords
flexible air conditioning ducts, coated textile material, flammability, tightness, analogue.
Reference list
  1. Satdinov R.A., Veshkin E.A., Postnov V.I., Strelnikov S.V. Vozduhovody nizkogo davleniya iz PKM v letatelnyh apparatah [РСМ low-pressure air ducts in aircraft] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2016. №8. St. 08. Available at: http://www.viam-works.ru (accessed: February 15, 2019). DOI: 10.18577/2307-6046-2016-0-8-8-8.
  2. Kablov E.N. Materialy dlya izdeliya «Buran» – innovacionnye resheniya formirovaniya shestogo tehnologicheskogo uklada [Materials for «Buran» spaceship – innovative solutions of formation of the sixth technological mode] // Aviacionnye materialy i tehnologii. 2013. №S1. S. 3–9.
  3. Kablov E.N. Kompozity: segodnya i zavtra [Composites: today and tomorrow] // Metally Evrazii. 2015. №1. S. 36–39.
  4. Kablov E.N. Materialy i khimicheskiye tekhnologii dlya aviatsionnoy tekhniki [Materials and chemical technologies for aviation technology] // Vestnik Rossiyskoy akademii nauk. 2012. T. 82. №6. S. 520–530.
  5. Kablov E.N. Aviakosmicheskoye materialovedeniye [Aerospace Materials] // Vse materialy. Entsiklopedicheskiy spravochnik. 2008. №3. S. 2–14.
  6. Veshkin E.A., Satdinov R.A., Postnov V.I., Strelnikov S.V. Sovremennyye polimernyye materialy dlya izgotovleniya elementov sistemy konditsionirovaniya vozdukha v letatel'nykh apparatakh [Modern polymeric materials for the manufacture of elements of the air conditioning system in aircraft] // Polimernyye kompozitsionnyye materialy i proizvodstvennyye tekhnologii novogo pokoleniya: sb. dokl. konf. M.: VIAM, 2017. S. 16.
  7. Vetrova L.E., Ionova V.F., Taskayeva P.V., Titarenko A.T., Shpakov V.P. Tkani s elastomernym pokrytiyem dlya myagkikh obolochnykh konstruktsiy [Elastomeric coated fabrics for soft shell structures]. M.: Ves Sergiyev Posad, 2012. 304 s.
  8. Ultra-lightweight air distribution & insulation systems. Available at: http://www.senioraerospacebwt.co.uk (accessed: February 15, 2019).
  9. Aeroduct. Available at: http://www.hbdthermoid.com (accessed: February 15, 2019).
  10. Herber Aircraft – a Flexfab Distributor. Available at: http://www.herberaircraft.com (accessed: February 15, 2019).
  11. High performance foam solutions for specialist markets worldwide. Available at: http://www.zotefoams.com (accessed: February 15, 2019).
  12. Prorezinennyye tkani [Rubberized fabric]. Available at: http://www.niirp.com (accessed: February 15, 2019).
  13. Steklotkani s silikonovym pokrytiyem [Fiberglass fabrics with silicone coating]. Available at: http://www.chemproduct.ru (accessed: February 15, 2019).
  14. Nesterova T.A., Barbotko S.L., Nikolaeva M.F., Gerter Yu.A. Mnogoslojnyj zashhitno-dekorativnyj material dlya dekorirovaniya detalej v salonah samoletov i vertoletov [Multi-layer protective and decorative material for decorating details in the cabin of aircraft and helicopters] // Trudy VIAM: elektron. nauch.-tehni. zhurn. 2013. №8. St. 04. Available at: http://www.viam-works.ru (accessed: February 15, 2019).
  15. Barbotko S.L. Razvitie metodov ocenki pozharobezopasnosti materialov aviacionnogo naznacheniya [Development of the fire safety test methods for aviation materials] // Aviacionnye materialy i tehnologii. 2017. №S. S. 516–526. DOI: 10.18577/2071-9140-2017-0-S-516-526.
  16. Kablov E.N., Startsev V.O., Inozemtsev A.A. Vlagonasyshhenie konstruktivno-podobnyh elementov iz polimernyh kompozicionnyh materialov v otkrytyh klimaticheskih usloviyah s nalozheniem termociklov [The moisture absorption of structurally similar samples from polymer composite materials in open climatic conditions with application of thermal spikes] // Aviacionnye materialy i tehnologii. 2017. №2 (47). S. 56–68. DOI: 10.18577/2071-9140-2017-0-2-56-68.
  17. Ivanov M.S., Veshkin E.A., Satdinov R.A., Donskikh I.N. Tkaneplenochnyy material dlya izgotovleniya gibkikh elementov sistemy konditsionirovaniya vozdukha v letatel'nykh apparatakh [Tissue film material for the manufacture of flexible elements of the air conditioning system in aircraft] // Polimernyye kompozitsionnyye materialy i proizvodstvennyye tekhnologii novogo pokoleniya: sb. dokl. konf. VIAM: Moskva, 2018. S. 147.
  18. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  19. Platonov M.M., Nesterova T.A., Nazarov I.A., Bejder E.Ya. Pozharobezopasnyj material na tekstilnoj osnove s poliuretanovym pokrytiem dlya naduvnoj obolochki spasatelnogo trapa [Fabric-based fireproof material with polyurethane coating for inflatable shell of rescue ladder] // Aviacionnye materialy i tehnologii. 2013. №2. S. 50–54.
  20. Venediktova M.A., Naumov I.S., Chajkun A.M., Eliseev O.A. Sovremennye tendencii v oblasti ftorsiloksanovyh i siloksanovyh kauchukov i rezin na ih osnove (obzor) [Current trends in fluorosiloxane and siloxane rubbers and rubber compounds based thereon (rеview)] // Aviacionnye materialy i tehnologii. 2014. №S3. S. 17–24. DOI: 10.18577/2071-9140-2014-0-S3-17-24.
  21. Nesterova T.A., Platonov M.M., Nazarov I.A., Barbotko S.L. Issledovaniya po razrabotke novogo materiala dlya balloneta pnevmaticheskogo trapa dlya avariynogo pokidaniya kabiny vertoleta [Researches on development new material for ballonet of pneumatic emergency slide of helicopter] // Trudy VIAM: elektron. nauch.-tekhnich. zhurnal. 2016. №12 (48). St. 07. Available at: http://www.viam-works.ru (accessed: February 15, 2019) DOI: 10.18577/2307-6046-2016-0-12-7-7.