Budinovskiy S.A., Stekhov P.A., Doronin O.N., Artemenko N.I. Main mechanisms of destruction of the ceramic layer of thermal barrier coatings (review) // Proceedings of VIAM. 2019. No. 2 (74). Ст. 11. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2019-0-2-105-112.

Main mechanisms of destruction of the ceramic layer of thermal barrier coatings (review)

Budinovskiy S.A., Stekhov P.A., Doronin O.N., Artemenko N.I.
Abstract

The article discusses various mechanisms of destruction and methods for assessing the performance of the ceramic layer of heat-shielding coating for parts of gas-turbine engines (GTE). The analysis showed that the main cause of spallation of the ceramic layer of the heat-shielding coating, during normal use of the product, is the formation of a thermal growing oxide, which is formed during the operation of the product and grows throughout the life of the resource, and has a critical value at which the ceramic layer is cleaving.

Keywords
YSZ, nickel alloys, ceramic layer, thermal barrier coating (TBC), thermal growing oxide (TGO), thermal conductivity coefficient.
Reference list
  1. Lityye lopatki gazoturbinnykh dvigateley: splavy, tekhnologii, pokrytiya / pod obshch. red. E.N. Kablova. 2-ye izd. [Cast blades of gas turbine engines: alloys, technologies, coatings / gen. ed. by E.N. Kablov. 2nd ed.]. M.: Nauka, 2006. 632 s.
  2. Kablov E.N. Razrabotki VIAM dlya gazoturbinnykh dvigateley i ustanovok [Development of VIAM for gas turbine engines and installations] // Krylya Rodiny. 2010. №4. S. 31–33.
  3. Kablov E.N., Petrushin N.V., Svetlov I.L., Demonis I.M. Nikelevye litejnye zharoprochnye splavy novogo pokoleniya [Nickel foundry heat resisting alloys of new generation] // Aviacionnye materialy i tehnologii. 2012. №S. C. 36–52.
  4. Chubarov D.A., Matveev P.V. Novye keramicheskie materialy dlya teplozashhitnyh pokrytij rabochih lopatok GTD [New ceramic materials for thermal barrier coating using in GTE turbine blades] // Aviacionnye materialy i tehnologii. 2013. №4. S. 43–46.
  5. Kablov E.N., Muboyadzhyan S.A. Zharostojkie i teplozashhitnye pokrytiya dlya lopatok turbiny vysokogo davleniya perspektivnyh GTD [Heat resisting and heat-protective coverings for turbine blades of high pressure of perspective GTE] // Aviacionnye materialy i tehnologii. 2012. №S. S. 60–70.
  6. Budinovskij S.A., Smirnov A.A., Matveev P.V., Chubarov D.A. Razrabotka teplozashhitnyh pokrytij dlja rabochih i soplovyh lopatok turbiny iz zharoprochnyh i intermetallidnyh splavov [Development of thermal barrier coatings for rotor and nozzle turbine blades made of nickel-base super- and intermetallic alloys] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2015. №4. St. 05. Available at: http://www.viam-works.ru (accessed: December 11, 2018). DOI: 10.18577/2307-6046-2015-0-4-5-5.
  7. Muboyadzhyan S.A., Budinovskij S.A., Gayamov A.M., Matveev P.V. Vysokotemperaturnye zharostojkie pokrytiya i zharostojkie sloi dlya teplozashhitnyh pokrytij [High-temperature heat resisting coverings and heat resisting layers for heat-protective coverings] // Aviacionnye materialy i tehnologii. 2013. №1. S. 17–20.
  8. Terry S.G., Litty J.R., Levi C.G. Evolution of porosity and texture in thermal barrier coatings grown by EB-PVD // Elevated Temperature Coatings: Science and Technology III. The Minerals, Metals and Materials Society, 1999. P. 13–26.
  9. Kashin D.S., Stekhov P.A. Sovremennyye teplozashchitnyye pokrytiya poluchennyye metodom elektronno-luchevogo napyleniya (obzor) [Modern thermal barrier coatings obtained by electron-beam physical vapor deposition (review)] // Trudy VIAM: elektron. nauch.-tekhnich. zhurn. 2018. №2. St. 10. Available at: http://www.viam-works.ru (accessed: December 21, 2018). DOI: 10.18577/2307-6046-2018-0-2-10-10.
  10. Kablov E.N. Materialy novogo pokoleniya [New generation materials] // Zashchita i bezopasnost. 2014. №4. S. 28–29.
  11. Avduyevskiy V.S., Galitseyskiy B.M., Glebov G.A. i dr. Osnovy teploperedachi v aviatsionnoy i raketno-kosmicheskoy tekhnike: ucheb. 2-ye izd., pererab. i dop. [Fundamentals of heat transfer in aviation and rocket and space technology: textbook. 2nd ed., rev. and add.]. M.: Mashinostroyeniye, 1992. 528 s.
  12. Schlichting K.W., Padture N.P., Klemens P.G. Thermal conductivity of dense and porous yttria-stabilized zirconia // Journal of materials science. 2001. No. 36. P. 3003–3010.
  13. Bychkov N.G., Klimov D.A., Myktybekov B., Nizovtsev V.Ye. Otsenka optimalnoy tolshchiny teplozashchitnykh pokrytiy stolbchatoy struktury na rabochikh lopatkakh turbin s uchetom deystviya tsentrobezhnykh nagruzok [Estimation of the optimal thickness of heat-shielding coatings of the columnar structure on turbine blades taking into account the effect of centrifugal loads] // Trudy MAI: elektron. zhurn. 2011. №46. Available at: http://trudymai.ru/published.php?ID=26030 (accessed: December 11, 2018).
  14. Ilinkova T.A., Valiyev R.R., Tagirov A.T. Dolgovechnost plazmennykh teplozashchitnykh pokrytiy v usloviyakh termicheskogo nagruzheniya [Durability of plasma heat-shielding coatings under thermal loading] // Vestnik KGTU im. A.N. Tupoleva. 2010. №2. S. 24–29.
  15. Ilinkova T.A., Ilinkov A.V., Valiyev R.R., Shigapov A.I. Issledovaniye teplozashchitnykh pokrytiy v usloviyakh termicheskogo udara [Study of heat-shielding coatings under thermal shock] // Tr. 8-y Mezhdunar. konf. «Plenki i pokrytiya». 2007. SPb.: Izd-vo Politekh. un-ta, 2007. S. 231–233.
  16. Jung S.H., Jeon S.H., Park H. et al. Growth Behavior of Thermally Grown Oxide Layer with Bond Coat Species in Thermal Barrier Coatings // Journal of the Korean Ceramic Society. 2018. Vol. 55. No. 4. P. 344−351.
  17. Karaoglanli A.C., Doleker K.M., Demire B. et al. Effect of shot peening on the oxidation behavior of thermal barrier coatings // Applied Surface Science. 2015. No. 354. P. 314–322.
  18. Nirav V. Patel. Use of Thermally Grown Oxide Stress Measurements to Predict Remaining Life of Thermal Barrier Coatings under Realistic Turbine Engine Conditions: Master’s Theses. 2014. 700 p.
  19. Hille T.S., Turteltaub S., Suiker A.S.J. Oxide growth and damage evolution in thermal barrier coatings // Engineering Fracture Mechanics. 2011. No. 78. P. 2139–2152.
  20. Fahr A., Rogé B., Thornton J. Detection of Thermally Grown Oxides in Thermal Barrier Coatings by Nondestructive Evaluation // Journal of Thermal Spray Technology. 2006. Vol. 15. P. 46–52.
  21. Song P. Influence of Material and Testing Parameters on the Lifetime of TBC Systems with MCrAlY and NiPtAl Bondcoats. Publikationsserver der RWTH Aachen University, 2012. 126 p.