Kulagina G.S., Zhelezina G.F., Levakova N.M. Antifriction organoplastics for high-loaded friction knots // Proceedings of VIAM. 2019. No. 2 (74). Ст. 09. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2019-0-2-89-96.
Antifriction organoplastics for high-loaded friction knots
Abstract
The work presents antifriction organoplastics Orgalon AF-1MR-260 and Orgalon AF-1MR-500 based on reinforcing fabric fillers containing antifriction polytetrafluoroethylene fibers and aramid power fibers. The materials are designed to reduce the cost and increase the load capacity compared to standard organoplastics Orgalon AF-1M-260 and Orgalon AF-1M-500.
The data on the friction coefficient, the load capacity of organoplastics were obtained. It is shown that the developed materials are highly effective antifriction materials for high-loaded self-lubricating friction knots and can be used in many areas of technics – for example, aircraft engineering, railway transport, mechanical engineering, building, re-construction of bridges and so on.
Keywords
antifriction organoplastic, high-loaded friction knot, self-lubricating material, reinforcing fabric filler, polytetrafluoroethylene fiber, aramid fiber, friction coefficient, load capacity.
Reference list
- Sovremennyye mashinostroitelnyye materialy. Nemetallicheskiye materialy: spravochnik / pod obshch. red. I.V. Gorynina, A.S. Oryshchenko [Modern engineering materials. Non-metallic materials: a handbook / gen. ed. by I.V. Gorynin, A.S. Oryshchenko]. SPb.: Professional, 2012. 916 s.
- Voronkov B.D. Podshipniki sukhogo treniya [Bearings dry friction]. L.: Mashinostroyeniye, 1979. 224 s.
- Adamenko N.A., Agafonova G.V. Tribotekhnicheskiye polimernyye materialy [Tribotechnical polymeric materials]. Volgograd: VolgGTU, 2013. 107 s.
- Referativnyy byulleten nauchno-tekhnicheskoy i patentnoy informatsii po uglerodnym materialam: M.: NIIgrafit, 2017. №9. 46 s.
- Yudin A.S. Razrabotka iznosostoykikh, antifriktsionnykh organotekstolitov na osnove polioksadiazolnykh tkaney i polimer-mineralnykh modifikatorov: avtoref. dis. ... kand. tekhn. nauk [Development of wear-resistant, antifriction organo-textolites based on polyoxadiazole fabrics and polymer-mineral modifiers: thesis abstract, Cand. Sc. (Tech.)]. M.: INEOS RAN, 2013. 20 s.
- Anisimov A.V., Bakhareva V.E., Balyshko I.V., Ginzburg B.M. i dr. Kharakteristiki organoplastikov na osnove fenolnoy matritsy i oksolanovogo volokna [Characteristics of organoplastics on the basis of the phenolic matrix and oxolane fiber] // Voprosy materialovedeniya. 2006. №2. S. 113–118.
- Kablov E.N. Materialy dlya aviakosmicheskoy tekhniki [Materials for aerospace] // Vse materialy. Entsiklopedicheskiy spravochnik. 2007. №5. S. 7–27.
- Kablov E.N. Materialy i khimicheskiye tekhnologii dlya aviatsionnoy tekhniki [Materials and chemical technologies for aviation technology] // Vestnik Rossiyskoy akademii nauk. 2012. T. 82. №6. S. 520–530.
- Kablov E.N. Aviakosmicheskoye materialovedeniye [Aerospace Materials] // Vse materialy. Entsiklopedicheskiy spravochnik. 2008. №3. S. 2–14.
- Organoplastiki [Organoplastics] // Konstruktsionnyye kompozitsionnyye materialy [Elektronnyy resurs]. Available at: https://www.viam.ru/organoplastics (accessed: December 20, 2018).
- Zhelezina G.F. Konstrukcionnye i funkcionalnye organoplastiki novogo pokoleniya [Constructional and functional organoplastics of new generation] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2013. №4. St. 06. Available at: http://www.viam-works.ru (accessed: December 17, 2018).
- Kulagina G.S., Korobova A.V., Zuev S.V., Zhelezina G.F. Issledovanie tribologicheskih svojstv organoplastikov na osnove tkanogo armiruyushhego napolnitelya [Study of tribological properties of organoplastics on the basis of reinforcing fabric filler] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2016. №11. St. 06. Available at: http://www.viam-works.ru (accessed: December 17, 2018). DOI: 10.18577/2307-6046-2016-0-11-6-6.
- Kulagina G.S., Korobova A.V., Ilichev A.V., Zhelezina G.F. Fizicheskiye i fiziko-mekhanicheskiye svoystva antifriktsionnogo organoplastika na osnove kombinirovannogo tkanogo napolnitelya i epoksidnogo svyazuyushchego [Physical and physico-mechanical properties of antifriction organoplastics based on combined fabric filler and epoxy binder] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2017. №10 (58). St. 08. Available at: http://www.viam-works.ru (accessed: December 18, 2018). DOI: 10.18577/2307-6046-2017-0-10-8-8.
- Prepreg antifriktsionnogo organoplastika i izdeliye, vypolnennoye iz nego: pat. 2404202 Ros. Federatsiya. №2009111566/05 [The prepreg antifriction organoplasty and the product made from it: pat. 2404202 Rus. Federation. No. 2009111566/05]; zayavl. 31.03.09; opubl. 20.11.10, Byul. №32.
- Solomentseva A.V., Fadeeva V.M., Zhelezina G.F. Antifriktsionnye organoplastiki dlya tyazhelonagruzhennykh uzlov treniya skolzheniya aviatsionnykh konstruktsij [Antifriction organoplastics for heavy loaded sliding friction units of aircraft structures] // Aviacionnye materialy i tehnologii. 2016. №2 (41). S. 30–34. DOI: 10.18577/2071-9140-2016-0-2-30-34.
- Kablov E.N. Strategicheskie napravleniya razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda [The strategic directions of development of materials and technologies of their processing for the period to 2030] // Aviacionnye materialy i tehnologii. 2012. №S. S. 7–17.
- Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
- Kirillov V.N., Efimov V.A., Shvedkova A.K., Nikolaev E.V. Issledovanie vliyaniya klimaticheskih faktorov i mehanicheskogo nagruzheniya na strukturu i mehanicheskie svojstva PKM [Research of influence of climatic factors and mechanical loading on structure and the PCM mechanical properties] // Aviacionnye materialy i tehnologii. 2011. №4. S. 41–45.