Kashin D.S., Ivanov I.M., Doronin O.N. Research of erosion resistance of soldered joints with protective coatings // Proceedings of VIAM. 2021. No. 8 (102). Ст. 08. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2021-0-8-67-74.
Research of erosion resistance of soldered joints with protective coatings
Abstract
Presents results of studies of the erosion resistance of soldered joints with various types of coatings. It was established that a coating based on tungsten carbide, applied by the electrospark method, has the greatest positive influence on the erosion resistance of VPr4 solder. At the same time, preliminary machining of the solder surface also increases resistance to the effects of erosion flow. The possibility of using an electrospark coating as an erosion-resistant sublayer for composite protective coatings was shown.
Keywords
erosion-resistant coating, soldered joints, electrospark alloying, solder, erosion resistance.
Reference list
- Kablov E.N., Petrova A.P. History of Aviation Materials Science. VIAM – 75 years of search, creativity, discoveries. Moscow: Nauka, 2007, 343 p.
- Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
- Kablov E.N., Echin A.B., Bondarenko Yu.A. History of development of directional crys-tallization technology and equipment for casting blades of gas turbine engines. Trudy VIAM, 2020, no. 3 (87), paper no. 01. Available at: http://www.viam-works.ru (accessed: February 2, 2021). DOI: 10.18577/2307-6046-2020-0-3-3-12.
- Kablov E.N., Muboyadzhyan S.A., Budinovskiy S.A., Pomelov Ya.A. Ion-plasma protective coatings for blades of gas turbine engines. Konversiya v mashinostroyenii, 1999, no. 2, pp. 42–47.
- Kablov E.N., Startsev O.V., Medvedev I.M. Review of international experience on corrosion and corrosion protection. Aviacionnye materialy i tehnologii, 2015, no. 2 (35), pp. 76–87. DOI: 10.18577/2071-9140-2015-0-2-76-87.
- Karpinos B.S., Korovin A.V., Lobunko A.P., Vedishcheva M.Yu. Operational damage of turbojet engines with afterburner combustion chamber. Vestnik dvigatelestroyeniya, 2014, no. 1, pp. 18–24.
- Kablov E.N., Muboyadzhyan S.A. Erosion-resistant coatings for compressor blades of gas turbine engines. Elektrometallurgiya, 2016, no. 10, pp. 23–38.
- Muboyadzhyan S.A., Lutsenko A.N., Alexandrov D.A., Gorlov D.S., Zhuravleva P.L. Investigation of the properties of nanolayer erosion-resistant coatings based on metal carbides and nitrides. Metally, 2011, no. 4, pp. 3–20.
- Muboyadzhyan S.A., Alexandrov D.A., Gorlov D.S. Ion-plasma nanolayer erosion-resistant coatings based on metal carbides and nitrides. Metally, 2010, no. 5, pp. 3–20.
- Vinogradov A.S. The design of the TRDDF RD-33. Samara: Korolev Samara State Aerospace University, 2013, 99 p.
- Zrelov V.A. Domestic gas turbine engines. Basic parameters and design schemes (Part 2): textbook. allowance. Samara: Samara State Aerospace University, 2002, 250 p.
- Kashin D.S., Dergacheva P.E., Stekhov P.A. Heat resistant slurry coatings (review). Trudy VIAM, 2018, no. 5 (65), paper no. 08. Available at: http://www.viam-works.ru (accessed: February 3, 2021). DOI: 10.18577/2307-6046-2018-0-5-64-75.
- Vinogradov S.S., Nikiforov A.A., Demin S.A., Chesnokov D.V. Protection against corrosion of carbon steel. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 242–263. DOI: 10.18577/2071-9140-2017-0-S-242-263.
- Vinogradov S.S., Nikiforov A.A., Demin S.A. Ways of solving the problem of replacing the cadmium coating. Galvanotekhnika i obrabotka poverkhnosti, 2018, vol. 26, no. 2, pp. 13–25.
- Malikov A.A., Markova E.V., Chechuga O.V. Application of electric discharge methods of surface hardening for tool life durability. Aviacionnye materialy i tehnologii, 2018, no. 4 (53), pp. 19-25. DOI: 10.18577 / 2071-9140-2018-0-4-19-25.
- Aleksandrov D.A., Muboyadzhyan S.A., Zhuravleva P.L., Gorlov D.S. Investigation of the effect of surface preparation and ion-assisted deposition on the structure and properties of erosion-resistant ion-plasma coating. Trudy VIAM, 2018, no. 10 (70), paper no. 08. Available at: http://www.viam-works.ru (accessed: January 27, 2021). DOI: 10.18577/2307-6046-2018-0-10-62-73.