Isaev A.Yu., Smirnov O.I., Rubtsova E.V., Petrova A.P. Properties and applications areas of the adhesive VKR-85 // Proceedings of VIAM. 2021. No. 5 (99). Ст. 05. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2021-0-5-48-55.
Properties and applications areas of the adhesive VKR-85
Abstract
The properties of the adhesive VKR-85 recommended for gluing rubbers, rubber fabric materials bands together and gluing them to metals during the vulcanization process are given. It is shown for which types of rubbers the adhesive can be used, performance of adhesive joints under the influence of various factors. A comparison of the properties of the adhesive joints based on adhesive VKR-85 with adhesives of a similar purpose – Leuconate and Desmodur RE is given. Adhesive joints strength made with adhesive VKR-85 is higher than strength of the bonded rubber.
Keywords
adhesive, rubber, vulcanization, bonding technology, strength of adhesive joints, climate resistance.
Reference list
- Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
- Kablov E.N. Russia in the market of intellectual resources. Ekspert, 2015, no. 28 (951), pp. 48-51.
- Kablov E.N. What to make the future of? New generation materials, technologies for their creation and processing - the basis of innovations. Krylya Rodiny, 2016, no. 5, pp. 8–18.
- Kablov E.N. Aviation materials science. Vse materialy. Entsiklopedicheskiy spravochnik, 2008, no. 3, pp. 2–14.
- Aviation materials: reference book: in 13 vols. Ed. E.N. Kablova. 7th ed., add. and rev. Moscow: VIAM, 2019, vol. 10: Adhesives, sealants, rubbers, hydraulic fluids, part 1. Adhesives, adhesive prepregs. 276 p.
- Petrova A.P., Donskoy A.A. Adhesive materials. Sealants. Saint Petersburg: Professional, 2008. 589 p.
- Large reference book of the rubber worker: in 2 parts. Ed. S.V. Reznichenko, Yu.L. Morozov. Moscow: Tekhinform, 2012, part 2: Rubber and mechanical rubber goods, 641 p.
- Khorova E.A., Myshlyavtsev A.V., Strizhak E.A., Tretyakova N.A. Examination of hydrogenated butadiene-nitrile rubbers by methods of differential scanning calori-metry and dynamic mechanical analysis. Aviacionnye materialy i tehnologii, 2019, no. 1 (54), pp. 11–16. DOI: 10.18577/2071-9140-2019-0-1-11-16.
- Naumova Yu.A. Synergistic effects in elastomeric adhesive compositions. III Intern. scientific and technical conf. «Modern achievements in the field of adhesives and sealants: materials, raw materials, technologies». N. Novgorod, 2019, pp. 60–62.
- Isaev A.Yu., Rubtsova E.V., Kotova E.V., Sutyagin M.N. Research of properties of glues and glue binding, made with use of modern domestic component base. Trudy VIAM, 2021, no. 3 (97), paper no. 05. Available at: http://www.viam-works.ru (accessed: March 22, 2021). DOI: 10.18577/2307-6046-2021-0-3-58-67.
- Kuznetsova V.А. Influence of the elastomeric modifier on mechanical and viscoelastic properties of epoxy and rubber compositions for erosion resistant coatings. Aviacionnye materialy i tehnologii, 2020, no. 2 (59), pp. 56–62. DOI: 10.18577/2071-9140-2020-0-2-56-62.
- Laptev A.B., Barbotko S.L., Nikolaev E.V. The main research areas of the persistence properties of materials under the influence of climatic and operational factors. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 547–561. DOI: 10.18577/2071-9140-2017-0-S-547-561.
- Tyumeneva T.Yu., Lukina N.F. Development in the field of elastomeric adhesives for aviation. Trudy VIAM, 2016, no. 8, paper no. 9. Available at: http://viam-works.ru (accessed: April 20, 2021). DOI: 10.18577/2307-6046-2016-0-8-9-9.
- Tyumeneva T.Yu., Lukina N.F., Zhuravleva P.L., Gulyaev A.I. Influence of nanomodifiers on the properties of elastomeric adhesive systems. Klei. Germetiki. Tekhologii, 2015, no. 3, pp. 11–16.
- Sagomonova V.A., Kislyakova V.I., Tyumeneva T.Yu., Bolshakov V.A. Influence of the adhesive layer on the damping properties of a vibration-absorbing material based on thermoplastic polyurethane. Klei. Germetiki. Tekhologii, 2015, no. 2, pp. 8–11.
- Petrova A.P., Malysheva G.V. Adhesives, adhesive binders and adhesive prepregs: textbook. Ed. E.N. Kablov. Moscow: VIAM, 2017, 472 p.
- Logacheva E.P., Bokov S.V., Polsman G.S. Adhesives for attaching rubbers to each other and to other substrates. Klei. Germetiki. Tekhologii, 2007, no. 9, pp. 26–30.
- Kopylov V.M., Ivanov V.V., Kovyazin V.A. Organosilicon dressings. Klei. Germetiki. Tekhologii, 2004, no. 6, pp. 2–12.
- Kotova S.V., Lyusova L.R., Popov A.A. Adhesive compositions of cold curing based on butadiene-nitrile rubber and chloroprenes. Kauchuk i rezina, 2009, no. 4, pp. 29–33.
- Lyusova L.R. Development of the direction «elastomeric adhesives» at the Department of Chemistry and Technology of Elastomer Processing. F.F. Koshelev ITHT them. M.V. Lomonosov RTU-MIREA. III Intern. scientific and technical conf. «Modern achievements in the field of adhesives and sealants: materials, raw materials, technologies». N. Novgorod, 2019, pp. 59–60.