Serpova V.M., Grishina O.I. Study of formation of intermetallic matrix structure based on heat-resistant nickel alloys // Proceedings of VIAM. 2018. No. 6 (66). Ст. 06. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2018-0-6-48-58.

Study of formation of intermetallic matrix structure based on heat-resistant nickel alloys

Serpova V.M., Grishina O.I.
Abstract

The paper presents the results of a study of the structure formation of in-thermetallide-oxide high-temperature metal composite materials based on nickel alloys reinforced with monocrystalline aluminum oxide plastids. Samples for research were obtained by the method of reaction impregnation. nickel powder with a diameter of 5–10 µm and nanosized nickel alumina particles with a diameter of 1–10 nm were used as matrix-forming agents. The results of the study of the microstructure and phase composition of samples of metal composite materials with different NiAl particle content (10; 15 and 20%) are shown. In order to identify individual intermetallic phases, microhardness studies were conducted.

Keywords
metal-matrix composite, intermetallic composites, nickel intermetallic, x-ray diffractometry, scanning electron microscopy.
Reference list
  1. Bazyleva O.A., Ospennikova O.G., Arginbaeva E.G., Letnikova E.Yu., Shestakov A.V. Tendencii razvitiya intermetallidnyh splavov na osnove nikelya [Development trends of nickel-based intermetallic alloys] // Aviacionnye materialy i tehnologii. 2017. №S. S. 104–115. DOI: 10.18577/2071-9140-2017-0-S-104-115.
  2. Letnikov M.N., Lomberg B.S., Ovsepyan S.V. Issledovanie kompozicij sistemy Ni–Al–Co pri razrabotke novogo zharoprochnogo deformiruemogo intermetallidnogo splava [Investigation experimental alloys based on Ni–Al–Co ternary system for development a new high-temperature intermetallic alloy for disk application] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2013. № 10. St. 01. Available at: http://www.viam-works.ru (accessed: May 28, 2018).
  3. Kablov E.N., Lomberg B.S., Ospennikova O.G. Sozdanie sovremennykh zharoprochnykh materialov i tekhnologij ikh proizvodstva dlya aviatsionnogo dvigatelestroeniya [Creation of modern heat resisting materials and technologies of their production for aviation engine building] // Krylya Rodiny. 2012. №3–4. S. 34–38.
  4. Bazyleva O.A., Arginbaeva E.G., Turenko E.Yu. Zharoprochnye litejnye intermetallidnye splavy [Heat resisting cast intermetallic alloys] // Aviacionnye materialy i tehnologii. 2012. №S. S. 57–60.
  5. Buntushkin V.P., Kablov E.N., Bazyleva O.A., Morozova G.I. Splavy na osnove alyuminidov nikelya [Alloys on the basis of nickel aluminides] // Metallovedenie i termicheskaya obrabotka metallov. 1999. №1. S. 32–34.
  6. Kablov E.N., Petrushin N.V., Svetlov I.L., Demonis I.M. Nikelevye litejnye zharoprochnye splavy novogo pokoleniya [Nickel foundry heat resisting alloys of new generation] // Aviacionnye materialy i tehnologii. 2012. №S. C. 36–52.
  7. Intermetallic Alloy Development. Publ. NMAB-487-1. Washington: National Academy Press., 1997. 51 p.
  8. Kablov E.N., Buntushkin V.P., Bazyleva O.A. Litye lopatki iz intermetallida nikelya (Ni3Al) dlya vysokotemperaturnykh gazovykh turbin [Cast blades from intermetallic compound of nickel (Ni3Al) for high-temperature gas turbines] // Konversiya v mashinostroenii. 2004. №4. S. 57–59.
  9. Kablov E.N. Osnovnye itogi i napravleniya razvitiya materialov dlya perspektivnoj aviatsionnoj tekhniki [The main results and the directions of development of materials for perspective aviation engineering] // 75 let. Aviatsionnye materialy. Izbrannye trudy «VIAM» 1932–2007. M.: VIAM, 2007. S. 20–26.
  10. Goryunov A.V., Rigin V.E. Sovremennaya tehnologiya polucheniya litejnyh zharoprochnyh nikelevyh splavov [The modern technology of cast nickel base superalloys production] // Aviacionnye materialy i tehnologii. 2014. №2. S. 3–7. DOI: 10.18577/2071-9140-2014-0-2-3-7.
  11. Grashchenkov D.V. Strategiya razvitiya nemetallicheskih materialov, metallicheskih kompozicionnyh materialov i teplozashhity [Strategy of development of non-metallic materials, metal composite materials and heat-shielding] // Aviacionnye materialy i tehnologii. 2017. №S. S. 264–271. DOI: 10.18577/2071-9140-2017-0-S-264-271.
  12. Grashchenkov D.V., Efimochkin I.Yu., Bolshakova A.N. Vysokotemperaturnye metallomatrichnye kompozicionnye materialy, armirovannye chasticami i voloknami tugoplavkih soedinenij [High-temperature metal-matrix composite materials reinforced with particles and fibers of refractory compounds] // Aviacionnye materialy i tehnologii. 2017. №S. S. 318–328. DOI: 10.18577/2071-9140-2017-0-S-318-328.
  13. Bolshakova A.N., Najmushin A.I., Efimochkin I.Yu. Issledovanie struktury intermetallidno-oksidnykh vysokotemperaturnykh kompozitsionnykh materialov na osnove nikelya i titana, armirovannykh monokristallicheskimi plastinami oksida alyuminiya [Research of structure of intermetallic oxide high-temperature composite materials on the basis of nickel and the titanium reinforced by single-crystal plates of aluminum oxide] // Vse materialy. Entsiklopedicheskij spravochnik. 2015. №6. S. 8–12.
  14. Ospennikova O.G. Itogi realizacii strategicheskih napravlenij po sozdaniyu novogo pokoleniya zharoprochnyh litejnyh i deformiruemyh splavov i stalej za 2012–2016 gg. [Implementation results of the strategic directions on creation of new generation of heat-resisting cast and wrought alloys and steels for 2012–2016] // Aviacionnye materialy i tehnologii. 2017. №S. S. 17–23. DOI: 10.18577/2071-9140-2017-0-S-17-23.
  15. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  16. Bekkert M., Klemm Kh. Sposoby metallograficheskogo travleniya: spravochnik [Ways of metallographic etching: directory]. M.: Metallurgiya, 1988. 400 s.