Klyukvina T.D., Vlasova K.A., Leonov A.A., Yashina S.A. Study of the mechanism of formation of strength in self-hardening mixtures with a phenolic binder (review) // Proceedings of VIAM. 2018. No. 3 (63). Ст. 03. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2018-0-3-18-27.

Study of the mechanism of formation of strength in self-hardening mixtures with a phenolic binder (review)

Klyukvina T.D., Vlasova K.A., Leonov A.A., Yashina S.A.
Abstract

The aim of the work is to study the technology of obtaining forms using self-hardening mixtures based on phenolic binders. The article gives statistical data about using different types of mixtures for the cores production. The classification of the most common resins used in molding using cold-hardening mixtures is given. The specific characteristics, advantages and disadvantages of cast alkaline phenolic resins are discussed. Time characteristics and strength parameters are analyzed on the basis of the curing curve of self-hardening mixtures. Examples of defects in forms, cores and castings associated with strength of the mixtures are given. The mechanism of strength formation of alkaline phenolic resins is considered (alpha-set process).

Keywords
self-hardening mixtures, phenolic binder, single contact strength, adhesion, cohesion, alpha-set process, green sand.
Reference list
  1. Ponomarenko O.I., Kolesnik E.V., Evtushenko N.S. Issledovanie prochnostnyh svojstv smolyanyh HTS na hromitovyh peskah [Research of strength properties of pitch HTS on hromitovy sand] // Litejnoe proizvodstvo. 2015. №3. S. 5–7.
  2. Duyunova V.A., Muhina I.Yu., Uridiya Z.P. Novye sostavy i tehnologiya polucheniya protivoprigarnyh prisadochnyh materialov [New compositions and technology of antiburning-on additive materials production] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2014. №11. St. 03. Available at: http://viam-works.ru (accessed: January 26, 2018). DOI: 10.18577/2307-6046-2014-0-11-3-3.
  3. Leonov A.A., Duyunova V.A., Stupak E.V., Trofimov N.V. Lite magnievyh splavov v razovye formy, poluchennye novymi metodami [Casting of magnesium alloys in disposable moulds produced by new methods] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2014. №12. St. 01. Available at: http://www.viam-works.ru (accessed: January 26, 2018). DOI: 10.18577/2307-6046-2014-0-12-1-1.
  4. Truhov A.P., Sorokin Yu.A., Ershov M.Yu. i dr. Tehnologiya litejnogo proizvodstva: Lite v peschanye formy: ucheb. [Technology of foundry production: Sand casting: textbook]. M.: Akademiya, 2005. 528 s.
  5. Zhukovskij S.S. Holodnotverdeyushhie svyazuyushhie i smesi dlya litejnyh sterzhnej i form: spravochnik [Coldhardening binding and mixes for foundry rods and forms: directory]. M.: Mashinostroenie, 2010. 256 s.
  6. Kablov E.N. Additivnye tehnologii – dominanta nacional'noj tehnologicheskoj iniciativy [The additive technologies – dominant of national technological initiative] // Intellekt i tehnologii. 2015. №2 (11). S. 52–55.
  7. Karataev A.M., Ponomarenko O.I., Evtushenko N.S. i dr. Formovochnye smesi s novym smolyanym svyazuyushhim [Forming mixes with the new pitch binding] // Litejnoe pro-izvodstvo. 2010. №1. S. 31–34.
  8. Foseco Non-Ferrous Foundryman`s Handbook. 11th ed. / ed. by John R. Brown. Butterworth
  9. Heinemann. Available at: http://alexandria-library.space/files/Ebooks/WorldTracker/Engineering/
  10. Metallurgy/Foseco%20Non-Ferrous%20Foundryman%27s%20Handbook%20(11th%20Edition).pdf (accessed: January 26, 2018).
  11. Duyunova V.A., Kozlov I.A. Holodnotverdeyushhie formovochnye smesi: perspektivy ispolzovaniya pri lite magnievyh splavov [Coldhardening forming mixes: use perspectives when molding magnesium alloys] // Vse materialy. Enciklopedicheskij spravochnik. 2011. №1. S. 41–43.
  12. Kablov E.N. Sovremennye materialy – osnova innovacionnoj modernizacii Rossii [Modern materials – basis of innovative modernization of Russia] // Metally Evrazii. 2012. №3. S. 10–15.
  13. Modern Casting breaks down the U.S. metalcasting industry by material, process and state: a modern casting staff report // Modern Casting Journal. January, 2015. P. 25–27. Available at: http://www.afsinc.org/multimedia/contentMC.cfm?ItemNumber=17657 (accessed: January 26, 2018).
  14. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  15. Galante G., Mikilli O., Maspero R. Formovka s primeneniem HTS. Nash vzglyad [Formovka using CHS. Our look]. Luino: IMF Luino, 1997. Ch. 2. 343 s.
  16. Duyunova V.A., Volkova E.F., Uridiya Z.P., Trapeznikov A.V. Dinamika razvitiya magnievyh i litejnyh alyuminievyh splavov [Dynamics of the development of magnesium and cast aluminum alloys] // Aviacionnye materialy i tehnologii. 2017. №S. S. 225–241. DOI: 10.18577/2071-9140-2017-0-S-225-241.
  17. Kaftannikov A.S., Nuraliev F.A., Stepashkin Yu.A. Svojstva zhidkostekolnyh HTS s ponizhennym soderzhaniem svyazuyushhego [Properties of liquidly glass CHS with the lowered maintenance of the binding] // Litejnoe proizvodstvo. 2015. №1. S. 31–33.
  18. Kablov E.N. Aviakosmicheskoe materialovedenie [Aerospace materials science] // Vse materialy. Enciklopedicheskij spravochnik. 2008. №3. S. 2–14.
  19. LaFay V. Application of No-Bake Sodium Silicate Binder Systems. American Foundry Society // International Journal of Metalcasting. 2012. Vol. 6. Is. 3. P. 19–26. Available at: https://link.springer.com/