Sidorov V.V., Petrov D.N., Kosenkov O.M., Gorunov A.V. Testing express-methods for determining the oxygen content in the complexly alloyed nickel melts under vacuum induction melting process with the use of oxygen probes // Proceedings of VIAM. 2018. No. 2 (62). Ст. 02. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2018-0-2-2-2.

Testing express-methods for determining the oxygen content in the complexly alloyed nickel melts under vacuum induction melting process with the use of oxygen probes

Sidorov V.V., Petrov D.N., Kosenkov O.M., Gorunov A.V.
Abstract

The technique provides ultra-low oxygen content in the process of smelting complex alloyed heat-resistant nickel alloys with special oxygen probes. This technique allows rapid and efficiently manage the processes of regulating the concentration of oxygen in the melt. Tested the developed method for installing in the melting of nickel-based superalloys. The technique of determining the oxygen content in the melt at can also be used for other, including newly developed alloys.

Keywords
vacuum melting, heat-resistant nickel alloys, method of express control, oxidation of the melt, measurement EDF, oxygen probes, oxygen content.
Reference list
  1. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  2. Kablov E.N., Sidorov V.V., Rigin V.E. Metallurgiya litejnyh zharoprochnyh splavov [Metallurgy of cast heat-resistant alloys] // 75 let. Aviacionnye materialy. Izbrannye trudy «VIAM» 1932–2007: yubil. nauch.-tehnich. sb. M.: VIAM, 2007. S. 125–132.
  3. Petrushin N.V., Ospennikova O.G., Svetlov I.L. Monokristallicheskie zharoprochnye nikelevye splavy dlya turbinnyh lopatok perspektivnyh GTD [Single-crystal Ni-based superalloys for turbine blades of advanced gas turbine engines] // Aviacionnye materialy i tehnologii. 2017. №S. S. 72−103. DOI: 10.18577/2071-9140-2017-0-S-72-103.
  4. Bazyleva O.A., Arginbaeva E.G., Turenko E.Yu. Vysokotemperaturnye intermetallidnye splavy dlya detaley GTD [The high-temperature intermetallic alloys for parts of gas-turbine engines] // Aviacionnye materialy i tehnologii. 2013. №3. S. 26–31.
  5. Petrushin N.V., Ospennikova O.G., Visik E.M., Rassohina L.I., Timofeeva O.B. Zharoprochnye nikelevye splavy nizkoj plotnosti [High-temperature nickel alloys of low density] // Litejnoe proizvodstvo. 2012. №6. S. 5-11.
  6. Kablov E.N., Petrushin N.V., Svetlov I.L., Demonis I.M. Litejnye zharoprochnye splavy novogo pokoleniya [Foundry hot strength alloys of new generation] // 75 let. Aviacionnye materialy. Izbrannye trudy «VIAM» 1932–2007: yubil. nauch.-tehnich. sb. M.: VIAM, 2007. S. 27–44.
  7. Orehov N.G., Starostina I.V. Analiz kachestva litoj prutkovoj (shihtovoj) zagotovki iz zharoprochnyh splavov proizvodstva FGUP «VIAM» [Quality analysis of the charge bar castings made from superalloys by FSUE «VIAM»] // Aviacionnye materialy i tehnologii. 2014. №S5. S. 23–30. DOI: 10.18577/2071-9140-2014-0-s5-23-30.
  8. Litye lopatki gazoturbinnyh dvigatelej: splavy, tehnologii, pokrytiya / pod obshh. red. E.N. Kablova. 2-e izd. [The analysis of quality of cast bar (blend) preparation from hot strength alloys of production of VIAM Federal State Unitary Enterprise]. M.: Nauka, 2006. 632 s.
  9. Luzgin V.P., Yavojskij V.I. Gazy v stali i kachestvo metalla [Gases in steel and quality of metal]. M.: Metallurgiya, 1983. 232 s.
  10. Grigoryan V.A., Belyanchikov L.N., Stomahin A.Ya. Teoreticheskie osnovy staleplavilnyh processov [Theoretical bases of steel-smelting processes]. M.: Metallurgiya, 1987. 272 s.
  11. Paderin S.N., Serov G.V., Shilnikov E.V., Alpatov A.V. Elektrohimicheskij kontrol i raschjoty staleplavilnyh processov [Electrochemical control and calculations of steel-smelting processes]. M.: Izd. Dom MISiS, 2011. 284 s.
  12. Zhuhovickij A.A., Shvarcman L.A. Fizicheskaya himiya [Physical chemistry]. M.: Gos. nauch.-tehn. izd-vo lit-ry po chern. i cvetn. metallurgii, 1963. 676 s.
  13. Luzgin V.P., Zinkovskij I.V., Pokidyshev V.V., Ivanov A.A. Kislorodnye zondy v staleplavilnom proizvodstve [Oxygen probes in steel-smelting production]. M.: Metallurgiya, 1989. 144 s.
  14. Rigin V.E., Sidorov V.V., Burcev V.T. Issledovanie aktivnosti kisloroda v rasplavah nikelya, soderzhashhih renij, pri vakuumnoj indukcionnoj plavke [Research of activity of oxygen in melt the nickel, containing rhenium, at vacuum induction melting] // Elektrometallurgiya. 2012. №11. S. 21–26.
  15. Zubarev K.A. Issledovanie processov rafinirovaniya splavov na osnove zheleza i nikelya v vakuume s celyu sovershenstvovaniya tehnologii plavki v vakuumnoj indukcionnoj pechi: dis. … kand. tehn. nauk [Research of refining processes of ferrous alloys and nickel in vacuum for the purpose of improvement of technology of melting in the vacuum induction furnace: thesis, Cand. Sci. (Tech.)]. M.: MISiS, 2016. 166 s.