Satdinov R.A., Veshkin E.A, Postnov V.I., Strelnikov S.V. РСМ low-pressure air ducts in aircraft // Proceedings of VIAM. 2016. No. 8 (44). Ст. 08. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2016-0-8-8-8.

РСМ low-pressure air ducts in aircraft

Satdinov R.A., Veshkin E.A, Postnov V.I., Strelnikov S.V.
Abstract

A review of the literature in the field of materials for low-pressure air ducts in the air-conditioning system is presented. A comparison of the major domestic and imported materials for the manufacture of air ducts is performed. The requirements for development of a competitive domestic material for manufacture of low-pressure air duct elements of PCM are determined.

Keywords
ACS, fiberglass, properties, low-pressure air ducts, fire-prevention requirements, middleware, analog, prepreg, PCM.
Reference list
  1. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  2. Kablov E.N. Rossii nuzhny materialy novogo pokoleniya [Materials of new generation are necessary to Russia] // Redkie zemli. 2014. №3. S. 8–13.
  3. Kablov E.N., Kirillov V.N., Zhirnov A.D., Startsev O.V., Vapirov Yu.M. Centry dlya klimaticheskikh ispytanijj aviacionnykh PKM [The centers for climatic tests of aviation PCM] // Aviacionnaya promyshlennost. 2009. №4. S. 36–46.
  4. Kablov E.N., Grashhenkov D.V., Erasov V.S., Anchevskijj I.Eh., Ilin V.V., Valter R.S. Stend dlya ispytaniya na klimaticheskojj stancii GCKI krupnogabaritnykh konstrukcijj iz PKM [The stand for testing for the GTsKI climatic stations of large-size designs from PCM] // Sb. dokl. IX Mezhdunarod. nauch. konf. po gidroaviacii «Gidroaviasalon–2012». 2012. S. 122–123.
  5. Barbotko S.L., Kirillov V.N., Shurkova E.N. Ocenka pozharnoj bezopasnosti polimernyh kompozicionnyh materialov aviacionnogo naznacheniya [Assessment of fire safety of polymeric composite materials of aviation assignment] // Aviacionnye materialy i tehnologii. 2012. №3. S. 56–63.
  6. Spravochnik po kompozicionnym materialam / pod red. Dzh. Lyubina [Directory on composite materials / ed. by Dzh. Lyubin]. M.: Mashinostroenie, 1988. 446 s.
  7. Polimernye kompozicionnye materialy: struktura, svojjstva, tekhnologiya / pod red. A.A. Berlina [Polymeric composite materials: structure, properties, technology / ed. by A.A. Berlin]. SPb.: Professiya, 2009. 556 s.
  8. Minakov V.T., Postnov V.I., Shvec N.I., Zastrogina O.B., Petukhov V.I., Makrushin K.V. Osobennosti izgotovleniya trekhslojjnykh sotovykh panelejj s polimernym zapolnitelem goryachego otverzhdeniya [Features of manufacturing of three-layered cellular panels with polymeric filler of hot curing] // Aviacionnye materialy i tehnologii. 2009. №3. S. 6–9.
  9. Kondrashov Eh.K., Postnov V.I., Petukhov V.I., Kavun N.S., Abramov P.A., Yudin A.A., Barbotko S.L. Issledovanie svojjstv trekhslojjnykh panelejj na modificirovannom svyazuyushhem FPR-520G [Research of properties of three-layered panels on modified binding FPR-520G] // Aviacionnye materialy i tehnologii. 2009. №3. S. 19–23.
  10. Postnova M.V., Postnov V.I. Opyt razvitiya bezavtoklavnyh metodov formovaniya PKM [Development experience out-of-autoclave methods of formation PCM]// Trudy VIAM: elektron. nauch.-tekhnich. zhurn. 2014. №4. St. 06. Available at: http://www.viam-works.ru (accessed: April 17, 2016). DOI 10.18577/2307-6046-2014-0-4-6-6.
  11. Veshkin E.A., Postnov V.I., Strelnikov S.V., Abramov P.A., Satdinov R.A. Opyt primeneniya tekhnologicheskogo kontrolya polufabrikatov PKM [Experience of application of technological control of semi-finished products of PCM] // Izvestiya Samarskogo nauchnogo centra RAN. 2014. T. 16. №6 (2). S. 393–398.
  12. Zastrogina O.B., Shvets N.I., Postnov V.I., Serkova E.A. Fenolformaldegidnye svjazuyushhie novogo pokoleniya dlya materialov interera [Phenolformaldehyde binding new generation for interior materials] // Aviacionnye materialy i tehnologii. 2012. №S. S. 265–272.
  13. Muhametov R.R., Ahmadieva K.R., Chursova L.V., Kogan D.I. Novye polimernye svyazujushhie dlya perspektivnyh metodov izgotovleniya konstrukcionnyh voloknistyh PKM [New polymeric binding for perspective methods of manufacturing of constructional fibrous PCM] //Aviacionnye materialy i tehnologii. 2011. №2. S. 38–42.
  14. Veshkin E.A. Osobennosti bezavtoklavnogo formovaniya nizkoporistykh PKM [Features of out-of-autoclave forming of poor-porous PCM] // Trudy VIAM elektron. nauch.-tekhnich. zhurn. 2016. №2. St. 07. Available at: http://www.viam-works.ru (accessed: April 20, 2016). DOI 10.1857/2307-6046-2016-0-2-7-7.
  15. Available at: http://www.mobile.gurit.com (accessed: May 25, 2016).