Development of melting technology of high pure REM–Fe–Co–B alloys for temperature-stable magnets
The influence of the ceramic crucible on chemical composition stability and purity of the REM–Fe–Co–B alloy during melting in a vacuum induction furnace is studied. It is shown that using MgO and Y2O3 as a working layer of the crucible allows to increase REM content stability in REM–Fe–Co–B system alloys and ensure high purity from aluminum and oxygen impurities. Usage of cobalt «K0» grade instead of «K1Au» grade as charge material leads to a significant reduction of nickel content in the melted alloy. For the first time the technology of melting of REM–Fe–Co–B alloys for temperature-stable magnets is designed. providing stability of chemical composition (REM ±1% by mass. from goal value, Co and B ±0,5% mass. from goal value) and high purity (aluminum and nickel impurities ≤0,1% mass. of each, oxygen impurity ≤0,05% by mass).
- Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33.
- Kablov E.N., Petrakov A.F., Piskorskij V.P., Valeev R.A., Nazarova N.V. Vliyanie disproziya i kobalta na temperaturnuyu zavisimost namagnichennosti i fazovyj sostav materiala sistemy Nd–Dy–Fe–Co–B [Influence disprosium and cobalt on temperature dependence of magnetization and phase structure of material of Nd-Dy-Fe-Co-B system] // MiTOM. 2007. №4. S. 3–10.
- Piskorskij V.P., Valeev R.A., Buzenkov A.V., Davydova E.A., Zolotareva M.V. Vliyanie vysokih koncentracij kobalta na svojstva magnitov Pr–Dy–Fe–Co–B [Influence of high concentration of cobalt on properties of magnets of Pr-Dy-Fe-Co-B] // Perspektivnye materialy. Specialnyj vypusk. 2008. S. 268–271.
- Piskorskij V.P., Valeev R.A., Tereshina I.S., Bronfin M.B., Chabina E.B., Davydova E.A., Buzenkov A.V. Magnitnye svojstva i fazovyj sostav materialov sistemy Pr–Dy–Fe–Co–B [Magnetic properties and phase structure of materials of Pr-Dy-Fe-Co-B system] // Perspektivnye materialy. 2007. №3. S. 16–19.
- Kablov E.N., Ospennikova O.G., Min P.G., Piskorskij V.P., Rezchikova I.I., Davydova E.A., Korolev D.V. Effekt vliyaniya splavov-dobavok na svojstva spechennyh magnitov (Pr, Dy)–(Fe, Co)–B s vysokim soderzhaniem kobalta [Effect of influence of alloys additives on properties of the sintered magnets (Pr, Dy)–(Fe, Co)–B with the high content of cobalt] // Metally. 2014. №6. S. 54–58.
- Kablov E.N., Petrakov A.F., Piskorskij V.P., Valeev R.A., Chabina E.B. Vliyanie ceriya i ittriya na magnitnye svojstva i fazovyj sostav materiala sistemy Nd–Dy–Fe–Co–B [Influence of cerium and yttrium on magnetic properties and phase structure of material of Nd-Dy-Fe-Co-B system] // MiTOM. 2005. №10. S. 25–29.
- Kablov E.N., Petrakov A.F., Piskorskij V.P., Valeev R.A., Chabina E.B. Vliyanie prazeodima na magnitnye svojstva i fazovyj sostav materiala sistemy Nd–Pr–Dy–Fe–Co–B [Influence praseodium on magnetic properties and phase structure of material of Nd–Pr–Dy–Fe–Co–B system] //MiTOM. 2005. №6 (600). S. 12–16.
- Min P.G., Sidorov V.V. Opyt pererabotki litejnyh othodov splava ZhS32-VI na nauchno-proizvodstvennom komplekse VIAM po izgotovleniyu lityh prutkovyh (shihtovyh) zagotovok [The experience of GS32-VI alloy scrap recycling at the VIAM scientific and production complex for cast bars production] // Aviacionnye materialy i tehnologii. 2013. №4. S. 20–25.
- Kablov E.N., Sidorov V.V., Kablov D.E., Rigin V.E., Goryunov A.V. Sovremennye tehnologii polucheniya prutkovyh zagotovok iz litejnyh zharoprochnyh splavov novogo pokoleniya [Modern technologies of receiving the bar stock preparations from foundry heat resisting alloys of new generation] // Aviacionnye materialy i tehnologii. 2012. №S. S. 97–105.
- Min P.G., Sidorov V.V. Resursosberegayushhaja tehnologiya pererabotki othodov litejnyh zharoprochnyh nikelevyh splavov [Resource-saving refining technology of waste of cast heat resisting nickel alloys] / V sb. tr. XXII Mezhdunar. nauch.-tehnich. konf. «Litejnoe proizvodstvo i metallurgiya». Minsk, 2014. S. 118–123.
- Min P.G., Goryunov A.V., Vadeev V.E. Sovremennye zharoprochnye nikelevye splavy i effektivnye resursosberegayushhie tehnologii ih izgotovleniya [Modern heat resisting nickel alloys and effective resource-saving technologies of their manufacturing] // Tehnologiya metallov. 2014. №8. S. 12–23.
- Min P.G., Vadeev V.E., Kalitsev V.A., Kramer V.V. Rafinirovanie nekondicionnyh othodov deformiruemyh nikelevyh splavov v vakuumnoj indukcionnoj pechi [Refinement of unconditioned waste of deformable nickel alloys in the vacuum induction furnace] // Tehnologiya metallov. 2015. №4. S. 8–13.
- Min P.G., Sidorov V.V., Rigin V.E., Gorjunov A.V. Resursosberegajushhaja tehnologiya pererabotki nekondicionnyh othodov Re–Ru soderzhashhih zharoprochnyh nikelevyh splavov [Resource-saving refining technology of unconditioned waste of Re-Ru of containing heat resisting nickel alloys] / V sb. tez. dokl. VI Mezhdunar. nauch.-tehnich. konf. «Molodezh v aviacii: novye resheniya i perspektivnye tehnologii». Zaporozhie: Motor Sich, 2012. S. 205–206.
- Piskorskij V.P. Termostabilnye magnitotverdye materialy na osnove redkozemelnyh intermetallidov s tetragonalnoj strukturoj [Thermostable magnitotverdy materials on the basis of rare-earth intermetallic compound with tetragonal structure]: avtoref. dis. … d-r tehn. nauk. M., 2013. 36 s.
- Burzo E., Plugaru N. Magnetic properties of R2–Fe14-x–Cux B compounds with R=Nd or Er // J. of Magn. and Magn. Mater. 1990. V. 86. P. 97–101.
- Hirosawa S., Hanaki A., Tomizawa H., Hamamura A. Current status of Nd–Fe–B permanent magnet materials // Physica B. 1990. V. 164. P. 117–123.
- Yakimovich P.V., Alekseev A.V., Min P.G. Opredelenie nizkih soderzhanij fosfora v zharoprochnyh nikelevyh splavah metodom ISP-MS [Determination of low phosphorus content in heat-resistant nickel alloys by ICP-MS method] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2014. №10. St. 02. Available at: http://www.viam-works.ru (accessed: June 06, 2015). DOI: 10.18577/2307-6046-2014-0-10-2-2.
- Dvoretskov R.M., Karachevtsev F.N., Isachenko Ya.A., Zagvozdkina T.N. Opredelenie osnovnyh i legiruyushhih elementov v termostabilnyh magnitnyh materialah sistemy RZM–Fe–Co–B metodom AES-ISP [ICP-AES determination of basic and alloying elements in thermostable magnetic materials of REM–Fe–Co–B system] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2014. №11. St. 10. Available at: http://www.viam-works.ru (accessed: June 06, 2015). DOI: 10.18577/2307-6046-2014-0-11-10-10.
- Sidorov V.V., Min P.G. Rafinirovanie slozhnolegirovannogo nikelevogo rasplava ot primesi sery pri plavke v vakuumnoj indukcionnoj pechi (chast 2) [Refinement complex-alloyed nickel rasplava from sulfur impurity when melting in the vacuum induction furnace (part 2)] // Elektrometallurgiya. 2014. №5. S. 26–30.
- Sidorov V.V., Min P.G. Refining a Complex Nickel Alloy to Remove a Sulfur Impurity during Vacuum Induction Melting: Part 2 // Russian Metallurgy (Metally). 2014. V. №12. P. 987–991.
- Min P.G., Sidorov V.V. Rafinirovanie othodov zharoprochnogo nikelevogo splava ZhS32-VI ot primesi kremniya v usloviyah vakuumnoj indukcionnoj plavki [Refining of scraps of Ni-base superalloy ZhS32-VI to eliminate silicon impurity under conditions of vacuum induction melting] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2014. №9. St. 01. Available at: http://www.viam-works.ru (accessed: June 06, 2015). DOI: 10.18577/2307-6046-2014-0-9-1-1.
- Sidorov V.V., Rigin V.E., Min P.G., Folomejkin Yu.I., Timofeeva O.B., Filonova E.V., Ishodzhanova I.V. Vliyanie primesej na strukturu i svojstva vysokozharoprochnyh litejnyh splavov i razrabotka effektivnyh metodov ustraneniya ih otricatelnogo vliyaniya [Influence of impurity on structure and property of high-heat resisting cast alloys and development of effective methods of elimination of their negative influence] // Novosti materialovedenija. Nauka i tehnika: elektron. nauch.-tehnich. zhurn. 2014. №2. St. 3. Available at: http://www.materialsnews.ru (accessed: June 06, 2015).
- Sidorov V.V., Rigin V.E., Timofeeva O.B., Min P.G. Vliyanie kremniya i fosfora na zharoprochnye svojstva i strukturno-fazovye prevrashheniya v monokristallah iz vysokozharoprochnogo splava VZhM4-VI [An effect of silicon and phosphorus on high temperature properties and structure-phase transformations of single crystals of VGM4-VI superalloy] // Aviacionnye materialy i tehnologii. 2013. №3. S. 32–38.
- Sidorov V.V., Min P.G., Folomejkin Yu.I., Vadeev V.E. Vliyanie skorosti filtracii slozhnolegirovannogo nikelevogo rasplava cherez penokeramicheskij filtr na soderzhanie primesi sery v metalle [Influence of speed of filtering complex-alloyed nickel rasplava via the penokeramichesky filter on the content of impurity of sulfur in metal] // Elektrometallurgiya. 2015. №5. S. 12–15.
- Sidorov V.V., Podkopaeva L.A., Min P.G. Use of rhenium – containing master alloy in melting single-crystal nickel superalloys // Metallurgist. 2013. V. 57. P. 543–547.
- Sidorov V.V., Podkopaeva L.A., Min P.G. Primenenie renijsoderzhashhej ligatury pri vyplavke monokristallicheskih vysokozharoprochnyh nikelevyh splavov [Application of reniysoderzhashchy ligature when smelting single-crystal high-heat resisting nickel alloys] // Metallurg. 2013. №6. S. 77–81.
- Spedding F.H., Daane A.H.J. Metals. 1954. V. 6. 504 p.