Goundobin N.V., Titov V.I., Pilipenko L.V. Determination germanium in alloys of Ni–Ti–Fe–Co–Si–Ge system // Proceedings of VIAM. 2015. No. 9. Ст. 09. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2015-0-9-9-9.

Determination germanium in alloys of Ni–Ti–Fe–Co–Si–Ge system

Goundobin N.V., Titov V.I., Pilipenko L.V.
Abstract

The paper shows the possibility of the determination of germanium in alloys nitinol of the Ni–Ti–Fe–Co–Si–Ge using extraction-photometric method. For the separation of germanium from hindering its defining elements and from the alloy base and others used the extraction of germanium by tetrachlorides from the salt – acid solution. The extractant used carbon tetrachloride. After stripping water germanium determined phenylfluorone as a complex phenilfluoronatum of germanium yellow-orange color in a weakly acid medium (0,3 N on HCl). The technique determination of germanium in the concentration range 0,01–1% by weight. alloys of Ni–Ti–Fe–Co–Si–Ge.

Reference list
  1. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitija materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative development of VIAM Federal State Unitary Enterprise of GNTs Russian Federation on implementation «The strategic directions of development of materials and technologies of their processing for the period till 2030»] //Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33.
  2. Kablov E.N., Sidorov V.V., Kablov D.E., Rigin V.E., Gorjunov A.V. Sovremennye tehnologii poluchenija prutkovyh zagotovok iz litejnyh zharoprochnyh splavov novogo pokolenija [Modern technologies of receiving bar preparations from foundry hot strength alloys of new generation] //Aviacionnye materialy i tehnologii. 2012. №S. S. 97–105.
  3. Shmotin Ju.N., Starkov R.Ju., Danilov D.V., Ospennikova O.G., Lomberg B.S. Novye materialy dlja perspektivnogo dvigatelja OAO «NPO „Saturn”» [New materials for the perspective engine of JSC NPO Saturn] //Aviacionnye materialy i tehnologii. 2012. №2. S. 6–8.
  4. Kablov E.N., Ospennikova O.G., Bazyleva O.A. Materialy dlja vysokoteplonagruzhennyh detalej gazoturbinnyh dvigatelej [Materials for the high-heatloaded details of gas turbine engines] //Vestnik MGTU im. N.Je. Baumana. Ser. «Mashinostroenie». 2011. №SP4. C. 13–19.
  5. Kablov E.N., Ospennikova O.G., Sidorov V.V., Rigin V.E. Proizvodstvo lityh prutkovyh (shihtovyh zagotovok) iz sovremennyh litejnyh vysokozharoprochnyh splavov [Production cast bar (blend preparations) from modern foundry high-hot strength alloys] /V sb. trudov nauchn.-tehn. konf. «Problemy i perspektivy razvitija metallurgii i mashinostroenija s ispol'zovaniem zavershennyh fundamental'nyh issledovanij i NIOKR». Ekaterinburg: Nauka-servis. 2011. T. 1. S. 31–38.
  6. Kablov E.N., Bondarenko Ju.A., Echin A.B., Surova V.A. Razvitie processa napravlennoj kristallizacii lopatok GTD iz zharoprochnyh splavov s monokristallicheskoj i kompozicionnoj strukturoj [Development of process of the directed crystallization of blades of GTD from hot strength alloys with single-crystal and composition structure] //Aviacionnye materialy i tehnologii. 2012. №1. S. 3–8.
  7. Kablov E.N., Petrushin N.V., Svetlov I.L., Demonis I.M. Nikelevye litejnye zharoprochnye splavy novogo pokolenija [Nickel foundry hot strength alloys of new generation] //Aviacionnye materialy i tehnologii. 2012. №S. S. 36–52.
  8. Tarasov Ju.M., Antipov V.V. Novye materialy VIAM − dlja perspektivnoj aviacionnoj tehniki proizvodstva OAO «OAK» [The VIAM new materials − for perspective aviation engineering of production of JSC OAK] //Aviacionnye materialy i tehnologii. 2012. №2. S. 5–6.
  9. Sidorov V.V., Timofeeva O.B., Kalicev V.A., Gorjunov A.V. Vlijanie mikrolegirovanija RZM na svojstva i strukturno-fazovye prevrashhenija v intermetallidnom splave VKNA-25-VI [Influence of microalloying of RZM on properties and structural phase changes in intermetallidny alloy VKNA-25-VI] //Aviacionnye materialy i tehnologii. 2012. №4. S. 8–13.
  10. Kauffman G.B. The story of National: The Serendipitous Discovery of the Memory Metal and Its Applications. The Chemical Educator 2. 1997. P. 1021.
  11. Miyazaki S., Kim H.Y., Hosoda H. Development and characterization of Ni-free Ti – base shape memory and superelastic alloys //Mater. Sci. Eng. 2006. V. 18. P. 438–440.